# US 2026/0002236 A1 · SYSTEMS AND PROCESSES FOR THE RECOVERY OF 226Ra FROM PHOSPHOGYPSUM

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0002236 A1
- Document ID: US20260002236A1
- Status: Published application
- Kind: A1
- Application number: 18/948,314
- Filed: 2024-11-14
- Published: 2026-01-01
- Earliest claimed: 2024-06-26
- Assignees: Village Enterprises, Inc.; DMT Co., Ltd.
- Applicants: SpectronRx; DMT GmbH & Co KG
- Inventors: John A. Zehner; Peter Webner; David Trump; Michael Haschke; Marie Charlotte Bornhoft
- Web page: https://patentgrep.com/patent/US20260002236A1

## CPC

- C05D 3/02: from limestone, calcium carbonate, calcium hydrate, slaked lime, calcium oxide, waste calcium products
- C22B 60/00: Obtaining metals of atomic number 87 or higher, i.e. radioactive metals
- C01F 13/00: Compounds of radium
- C05B 11/02: Pretreatment
- C22B 3/065: {Nitric acids or salts thereof}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/14: containing ammonia or ammonium salts
- C22B 3/165: {with organic acids}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 26/20: Obtaining alkaline earth metals or magnesium
- G21G 1/10: by bombardment with electrically charged particles (irradiation devices G21K5/00)
- G21G 1/12: by electromagnetic irradiation, e.g. with gamma or X-rays (applications of radiation G21H5/00; irradiation devices G21K5/00)
- G21G 2001/0094: {Other isotopes not provided for in the groups listed above}
- Y02P 10/20: Recycling
- C05D: INORGANIC FERTILISERS NOT COVERED BY SUBCLASSES C05B, C05C; FERTILISERS PRODUCING CARBON DIOXIDE
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C05B: PHOSPHATIC FERTILISERS
- G21G: CONVERSION OF CHEMICAL ELEMENTS; RADIOACTIVE SOURCES (applications of radiation in general G21H5/00; handling particles, e.g. neutrons, or electromagnetic radiation not otherwise provided for G21K)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods of processing phosphogypsum (PG) to recover Radium (e.g., 226Ra), and/or other constituents from PG, are described. PG (stockpiled PG, fresh PG or a combination) is combined with a leach solution, allowed to react for 2-6 hours (e.g., a single leaching step), at a temperature in the range of about 40-70° C. to obtain leachate and leach residue. Further processing by subjecting the leachate and/or the leach residue to one or more separation techniques, such as ion exchange, enables the recovery of one or more constituents of interest. By separating 226Ra, rare earth elements (REE) and/or other constituents from this secondary resource (e.g., waste PG), gypsum can be purified for use in the construction industry, the recovery of 226Ra can be used to produce dedicated isotopes like 223Ra and/or 225Ac for life-saving cancer medication, and raw materials can be provided for the high-tech industry, agriculture and the building industry.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim 20

A method of preparing a radionuclide, the method comprising:
subjecting PG to one or more lixiviant;
separating 226Ra from the PG;
isolating 226Ra by one or more separations method, optionally ion exchange; and
converting the 226Ra into 223Ra or converting the 226Ra into 225Ac, optionally by irradiation.

### Claim 21 (depends on 20)

The method of claim 20, comprising:
converting the 226Ra into 225Ac by irradiation;
wherein the irradiation comprises accelerator irradiation where electrons are accelerated to generate an electron beam at 40 MeV to reach the 226Ra target, then the 226Ra in the target is irradiated creating the 226Ra(g,n)225Ra by photoreaction, then allowing the 225Ra to then naturally decay into 225Ac.

### Claim 22

A method of processing phosphogypsum (PG), the method comprising:
combining phosphogypsum (PG) with a leach solution comprising Na(NO3)2 and/or Ca(NO3)2;
reacting the leach solution with the PG for a time and temperature sufficient to obtain i) leachate comprising an amount of radium and/or 226Ra extracted from the PG and ii) solids;
and separating the leachate from the solids.

### Claim 23

(canceled)

### Claim 24 (depends on 22)

The method of claim 22, comprising not repeating the reacting step, thereby performing only a single leaching step.

### Claim 25 (depends on 24)

The method of claim 24, wherein:
the leachate comprises at least 70% of the radium and/or 226Ra from the PG; or
the solids comprise a non-detectable amount of radium and/or 226Ra, or a concentration of no more than about 10 picocuries per gram (pCi/g) of radium and/or 226Ra.

### Claim 26 (depends on 22)

The method of claim 22, further comprising:
separating an amount of radium and/or 226Ra from the leachate by ion exchange.

### Claim 27 (depends on 26)

The method of claim 26, wherein the separating by ion exchange is performed by contacting at least a portion of the leachate with an ion exchange resin.

### Claim 28 (depends on 22)

The method of claim 22, further comprising:
prior to the reacting, separating a fine fraction from the PG and performing the reacting with the fine fraction to obtain the leachate and the solids;
wherein at least 75% of particles of the fine fraction are less than 25 μm in diameter.

### Claim 29 (depends on 28)

The method of claim 28, further comprising:
separating an amount of radium and/or 226Ra from the leachate by way of ion exchange.

### Claim 30 (depends on 29)

The method of claim 29, wherein the separating by ion exchange is performed by contacting at least a portion of the leachate with an ion exchange resin.

### Claim 31 (depends on 28)

The method of claim 28, further comprising:
grinding particles of the fine fraction prior to or during the reacting and/or the separating.

### Claim 32 (depends on 31)

The method of claim 31, further comprising subjecting at least a portion of the leachate and/or at least a portion of the solids to one or more separation techniques.

### Claim 33 (depends on 32)

The method of claim 32, wherein one or more of the separation techniques is chosen from separation by precipitation, ion exchange, solvent extraction, or membrane technologies.

### Claim 34 (depends on 32)

The method of claim 32, wherein:
one or more of the separation techniques is capable of separating one or more of the following constituents from the leachate and/or the solids:
one or more alkaline earth metals;
technologically enhanced naturally occurring radioactive material (TENORM);
gypsum; and/or
heavy metals.

### Claim 35 (depends on 32)

The method of claim 32, wherein one or more of the separation techniques comprises:
precipitation and/or
ion exchange; and/or
precipitation with hydroxide; and/or
precipitation of Ca(OH)2; and/or
precipitation with sulfate; and/or
precipitation of (Ba,Ra)SO4.

### Claim 36 (depends on 35)

The method of claim 35, wherein one or more of the separation techniques comprises:
reducing Ca content of the leachate to provide a Ca-reduced leachate; and
separating an amount of radium and/or 226Ra from the Ca-reduced leachate by way of selective precipitation, ion exchange, solvent extraction, and/or membrane technologies.

### Claim 37 (depends on 32)

The method of claim 32, wherein one or more of the separation techniques comprises:
ion exchange with acidic gel type cation exchange resin; or
ion exchange with one or more cation exchange resin;
wherein the cation is H+; and/or
wherein the cation exchange resin comprises sulfonic acid functional groups.

### Claim 38 (depends on 32)

The method of claim 32, further comprising:
subjecting the leachate to ion exchange by contacting at least a portion of the leachate with an ion exchange resin and separating an amount of radium and/or 226Ra from the leachate to provide a recyclable leach solution;
recycling and combining the recyclable leach solution with a second batch of PG comprising radium and/or 226Ra;
allowing the recycled leach solution to react with the second batch of PG to obtain a second batch of leachate and a second batch of solids;
separating the second batch of leachate from the second batch of solids;
subjecting the second batch of leachate to ion exchange by contacting at least a portion of the second batch of leachate with an ion exchange resin; and
separating an amount of radium and/or 226Ra from the second batch of leachate.

### Claim 39 (depends on 32)

The method of claim 32, further comprising:
processing at least a portion of the solids into NORM-free gypsum having a non-detectable amount, or a concentration of no more than about 10 picocuries per gram (pCi/g) of radium and/or 226Ra.

### Claim 40 (depends on 22)

The method of claim 22, wherein the leach solution comprises Na(NO3)2.

### Claim 41 (depends on 22)

The method of claim 22, wherein the leach solution comprises Ca(NO3)2.

### Claim 42 (depends on 41)

The method of claim 41, wherein:
the time the leach solution is reacted with the PG is for about 2-6 hours; and
the temperature is in the range of about 40-70° C.

### Claim 43 (depends on 22)

The method of claim 22, wherein the leach solution comprises about 10-30% Ca(NO3)2.