# US 2026/0002089 A1 · Lubricant compositions including a polymerizable-acid graft polymer as a corrosion inhibitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0002089 A1
- Document ID: US20260002089A1
- Status: Published application
- Kind: A1
- Application number: 18/881,059
- Filed: 2023-07-07
- Published: 2026-01-01
- Earliest claimed: 2022-07-08
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Puspendu Deo; Sean Ewart; Cathi Evans-Beatty
- Web page: https://patentgrep.com/patent/US20260002089A1

## CPC

- C10M 145/00: Lubricating compositions characterised by the additive being a macromolecular compound containing oxygen (oxidised hydrocarbons C10M143/18)
- C10M 169/041: {the additives being macromolecular compounds only}
- C10M 2203/1006: used as base material
- C10M 2209/02: Macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C10M 2209/084: Acrylate; Methacrylate
- C10M 2209/103: Polyethers, i.e. containing di- or higher polyoxyalkylene groups
- C10M 2209/104: of alkylene oxides containing two carbon atoms only
- C10N 2030/12: Inhibition of corrosion, e.g. anti-rust agents or anti-corrosives
- C10N 2040/30: Refrigerators lubricants {or compressors lubricants}
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

Embodiments of lubricant compositions that may comprise a lubricant oil and a corrosion inhibitor, wherein the corrosion inhibitor may comprise a polymerizable-acid graft polymer that may comprise from about 3.0% to about 35% by weight of an unsaturated grafting acid and an alkylene oxide polymer backbone, the alkylene oxide polymer backbone having the formula: R″—[(OCnH2n)z—OR′]a wherein each R′ in the formula may be independently selected from the group consisting of a hydrogen atom, hydrogen radicals, and acyl radicals, wherein each R″ in the formula may be independently selected from the group consisting of a hydrogen atom, hydrogen radicals, amine-containing radicals, and acyl radicals, wherein each “n” in the formula may independently have a value of from 2 to 4, wherein each “Z” in the formula may independently have a value of from 4 to about 1800, and wherein “a” may have a value of from 1 to 4.

## Claims

### Claim 1

A lubricant composition comprising:
an oil lubricant and
a corrosion inhibitor comprising a polymerizable-acid graft polymer comprising from about 3.0% to about 35% by weight of an unsaturated grafting acid and an alkylene oxide polymer backbone, the alkylene oxide polymer backbone having the following formula:
wherein each R′ is independently selected from the group consisting of a hydrogen atom, hydrogen radicals, and acyl radicals;
wherein R″ is independently selected from the group consisting of a hydrogen atom, hydrogen radicals, amine-containing radicals, and acyl radicals;
wherein each “n” has, independently, a value of from 2 to 4;
wherein each “Z” has, independently, a value of from 4 to about 1800; and
wherein “a” has a value of from 1 to 4.

### Claim 2 (depends on 1)

The lubricant composition of claim 1, wherein R′ and R″ are not both a hydrogen atom.

### Claim 3 (depends on 1)

The lubricant composition of claim 1, wherein the grafting acid is selected from the group consisting of acrylic acid, methacrylic acid, itaconic acid, maleic acid, 2-acrylamido-2-methylpropylsulfonic acid (AMPS), 2-methacrylamido-2-methylpropylsulfonic acid, styrene sulfonic acid, vinylsulfonic acid, ethylene glycol methacrylate phosphate, vinyl phosphonic acid and mixtures thereof.

### Claim 4 (depends on 1)

The lubricant composition of claim 1, wherein “n”=2 or 3;
wherein “a” has a value of 1;
wherein each R′ or R″ independently selected from the group consisting of a hydrogen atom, hydrogen radicals, and acyl radicals; and
wherein the alkylene oxide polymer backbone is either an ethylene oxide (“EO”) or propylene oxide (“PO”) polymer.

### Claim 5 (depends on 1)

The lubricant composition of claim 1, wherein the alkylene oxide polymer backbone is selected from the group consisting of oxyethylene (“EO”) and oxypropylene (“PO”).

### Claim 6 (depends on 1)

The lubricant composition of claim 1, wherein the alkylene oxide polymer backbone is a copolymer of EO and PO polymers having a weight ratio of from about 0:100 to about 100:0 of EO:PO, or from about 90:10 to about 10:90 of EO:PO, or from about 75:25 to about 25:75 of EO:PO.

### Claim 7 (depends on 1)

The lubricant composition of claim 1, wherein the polymer has an average molecular weight between approximately 1500 Daltons and approximately 80000 Daltons.

### Claim 8 (depends on 1)

The lubricant composition of claim 1, wherein the grafting acid is acrylic acid (10 wt. %), and the alkylene oxide polymer backbone is poly(oxyethylene-oxypropylene) having a weight ratio of oxyethylene (“EO”) to oxypropylene (“PO”) of 50:50.

### Claim 9 (depends on 1)

The lubricant composition of claim 1, wherein the oil lubricant comprises mineral oil.

### Claim 10 (depends on 1)

The lubricant composition of claim 1, wherein the lubricant composition comprises from 0.5 wt. % to 20 wt. % corrosion inhibitor, or from 2.5 wt. % to 10 wt % corrosion inhibitor.

### Claim 11 (depends on 1)

A method for reducing corrosion comprising:
exposing a metal component to a solution comprising the lubricant composition of claim 1 and (meth)acrylic acid, wherein the lubricant composition reduces metal corrosion.

### Claim 12 (depends on 11)

The method of claim 11, wherein the solution may comprise co-solvent.

### Claim 13 (depends on 12)

The method of claim 12, wherein the co-solvent comprises carboxylic acid, alcohol, or combinations thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the alcohol comprises methanol.

### Claim 15 (depends on 12)

The method of claim 12, wherein the metal component comprises bronze packing rings.

### Claim 16 (depends on 15)

The method of claim 15, wherein the bronze packing rings are part of a compressor.

### Claim 17 (depends on 16)

The method of claim 16, wherein the bronze packing rings are part of a compressor unit utilized in a high pressure polyethylene reactor.

### Claim 18 (depends on 1)

A free-radical polymerization process comprising:
polymerizing ethylene monomer and optionally (meth)acrylic acid comonomer in the presence of the lubricant composition of claim 1 via free radical polymerization in a high pressure polyethylene reactor having a compressor with bronze packing rings.