# US 2026/0001808 A1 · Micromechanical comb structure made of glass, and associated method of use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0001808 A1
- Document ID: US20260001808A1
- Status: Published application
- Kind: A1
- Application number: 18/880,621
- Filed: 2023-07-05
- Published: 2026-01-01
- Earliest claimed: 2022-07-05
- Assignees: Lpkf Laser & Electronics AG
- Applicants: LPKF Laser & Electronics SE
- Inventors: Roman Ostholt; Norbert AMBROSIUS; Maik BERTKE; Svenja SCHUDAK; Michael LOOTZE; Julia VOSS
- Web page: https://patentgrep.com/patent/US20260001808A1

## CPC

- B81C 1/00619: {Forming high aspect ratio structures having deep steep walls}
- C03C 23/0025: {by a laser beam}
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- B81B 2201/033: Comb drives
- B81B 2203/055: Translation in a plane parallel to the substrate, i.e. enabling movement along any direction in the plane
- B81C 2201/0133: Wet etching
- B81C 2201/0143: Focussed beam, i.e. laser, ion or e-beam
- G02B 26/085: {the reflecting means being moved or deformed by electromagnetic means}
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

In order to extend the possible applications of the already known LIDE (laser-induced deep etching) method, this invention provides for producing a micromechanical comb structure (25) by placing a plurality of laser pulses (4) on a glass substrate (3) with a subsequent wet-chemical etching step for exposing the comb structure (25), and to precisely control the position of those laser pulses (4) that define the outer contour (6) of respective fingers (24) of the comb structure (25). This makes it possible to form very narrow fingers (24) that have uniform sidewalls (13), whereby very small gap dimensions (35) and uniform electrostatic actuation of the comb structure (25) are rendered possible. By controlling the phase angle φ and/or the extent of the sidewall scalloping of the fingers (24), it is also possible to favorably influence or set, in a targeted manner, the mechanical properties of the comb structure (25).

## Claims

### Claim 1

A micromechanical comb structure (25) made of glass, comprising:
a glass substrate having a plurality of micromechanical fingers (24), the comb structure (25) being deflectable in a substrate plane (28) defined by the glass substrate (3), and
the fingers (24) made of the glass substrate (3) being exposed by laser-induced modification of the glass substrate (3) and subsequent wet-chemical anisotropic etching,
in which laser pulses (4) that define an outer contour (6) of the fingers (24) are placed on respective continuous tool trajectories (5a, 5b) that are opposite each other and
each of the tool trajectories (5a, 5b) has a maximum distance r from the contour (6), the distance corresponding precisely to an etching radius (27) of a wet-chemical etching step used to expose the fingers (24).

### Claim 2 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein at least one flexure (17) is exposed by the laser-induced modification of the glass substrate (3) and the subsequent wet-chemical anisotropic etching, said flexure being used to monolithically connect the comb structure (25) to the glass substrate (3) in order to provide a deflection capability.

### Claim 3 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein the fingers (24) each have two sidewalls (13a, 13b) that are opposite each other and exhibit concave indentations (8),
said concave indentations (8) each exhibit a curvature defined by the etching radius r and are delimited by respective convex ribs (9), and
the indentations (8) exhibit a constant mean spacing Lx, at least in sections of a length of the respective finger (24).

### Claim 4 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein opposing ribs (9), which are formed in opposing sidewalls (13a, 13b/13c, 13) of a respective one of the fingers (24) exhibit an offset Δx along a direction of extent (2) of the finger (24), to which the following applies: Lx/4≤Δx≤Lx/2, where Lx is the mean spacing between two directly adjacent ones of the ribs (9) that are formed in a same one of the sidewalls (13a/13b).

### Claim 5 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein in order to obtain weakly pronounced sidewall scalloping, the laser pulses (4) are placed in such a way and the fingers (24) are etched free in such a way that: p<r, where p=a ratio of a mean pulse spacing between adjacent laser pulses (4) on one of the two tool trajectories (5a or 5b) and r=the etching radius (27).

### Claim 6 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein; ty/r<0.1, where r=the local etching radius (27) and ty=a lateral depth (14) of the respective indentations (8), and ty/B<0.1, where B=
maximal width (15) of the respective finger (24) transversely to a direction of extent (2) thereof.

### Claim 7 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein the fingers (24) exhibit a rhombic cross section that results from wet-chemical etching of the glass substrate (3) on both sides.

### Claim 8 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein side faces (13) of the fingers (24) form a respective taper angle ϕ (22) of less than 6°.

### Claim 9 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein p/B<0.5, where p=a pulse spacing between two adjacent laser pulses (4) on a tool trajectory (5) extending parallel to the respective contour (6) of the respective finger (24) and B=a maximum width (15) of the respective finger (24) transversely to a direction of extent (2) thereof, and
the maximum width B (15) of the respective finger (24) is less than 100 μm.

### Claim 10 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein sidewalls (13) of the fingers (24) have a metallization (30) that serves for the formation of electrodes of the fingers (24).

### Claim 11 (depends on 1)

The micromechanical comb structure (25) made of glass as claimed in claim 1, wherein a respective spatial phase angle φ(x) of respective laser pulse pairs (18) of thee laser pulses or opposing ribs (9) in sidewalls (13a, 13b) of one of the fingers (24b) along a respective direction of extent (2) of the finger (24b) is chosen such that
in a specific actuation position of the comb structure (25), the ribs (9) formed in sidewalls (13a, 13b) of the finger (24b)
are formed flush with corresponding ones of the ribs (9) of a first directly adjacent one of the fingers (24a) on one side and
are formed offset to corresponding ones of the ribs (9) of a second directly adjacent one of the fingers (24c) on an opposite side, and
opposing ribs (9) of the finger (24b) located between the first and second directly adjacent fingers (24a, 24c) exhibit an offset Δx<Lx/4, where Lx is a mean spacing between two directly adjacent ones of the ribs.

### Claim 12 (depends on 1)

A micromechanical actuator comprising the micromechanical comb structure (25) as claimed in claim 1,
wherein the fingers (24) of the comb structure (25) comprise sidewall electrodes for electrostatic actuation of the comb structure (25).

### Claim 13 (depends on 1)

A micromechanical stepper actuator comprising the micromechanical comb structure (25) made of glass as claimed in claim 1, wherein
a step size (G) of the stepper actuator corresponds to a spacing (Lx) of convex ribs (9) (Lx=G) which delimit lateral concave indentations (8) that are formed in sidewalls (13) of the fingers (24) and exhibit a curvature defined by the etching radius (27), and t/r>0.1, where r=the etching radius (27) and ty=a lateral depth (14) of the respective indentations (8).

### Claim 14 (depends on 13)

The stepper actuator as claimed in claim 13,
wherein a respective spatial phase angle φ(x) of respective laser point pairs (18) or lateral indentations (8) along a respective direction of extent (2) of directly adjacent ones of the fingers (24) of the comb structure (25) is φ=0°+/−60°,
such that ribs (9) formed in opposing sidewalls (13) of in each case two directly adjacent ones of the fingers (24) are at least approximately flush with each other in a specific actuation position of the comb structure (25).

### Claim 15

A method for producing a micromechanical comb structure (25) made of glass, wherein the comb structure (25) comprises a glass substrate (3) with a plurality of micromechanical fingers (24), and the comb structure (25) is deflectable in a substrate plane (28) defined by the glass substrate (3), the method comprising:
placing laser pulses (4) that are intended to define an outer contour (6) of the fingers (24) on respective continuous tool trajectories (5a, 5b) that are opposite each other in order to expose the fingers, and
wet-chemical etching all of the fingers (24) of the comb structure (25) in a common wet-chemical etching step such that a respective outer contour (6) of the fingers (24) is exposed that has a maximum distance (r) from the associated tool trajectory (5a, 5b) that corresponds to an etching radius (27) of the etching step.

### Claim 16 (depends on 15)

The method as claimed in claim 15,
wherein an anisotropy of the etching step is chosen such that the fingers (24) are formed with a taper angle ϕ (22) of no more than 6° with respect to a surface normal (26) of the substrate plane (28), and
choosing a ratio of a first etching rate of regions (11) of the glass substrate (3) modified by laser radiation and a second etching rate of unmodified regions of the glass substrate (3) is chosen to be greater than 15:1.

### Claim 17 (depends on 15)

The method as claimed in claim 15, further comprising forming the fingers (24) with a rhombic cross-sectional shape by a wet-chemical etching solution being used to perform the etching from two sides of the glass substrate (3), and
wherein the anisotropy of the etching step is set such that following the etching, the fingers (24) form an interior angle (34) with a respective sidewall (13) of at least 170°.

### Claim 18 (depends on 15)

The method as claimed in claim 15, further comprising,
in order to obtain weakly pronounced sidewall scalloping, placing the laser pulses (4) such and the fingers (24) are etched free in such a way that the following applies: p<r, where p=a mean pulse spacing between adjacently placed ones of the laser pulses (4) and r=the etching radius r.

### Claim 19 (depends on 15)

The method as claimed in claim 15, wherein a respective contour (6) of the fingers (24) exhibits lateral concave indentations (8) that each exhibit a curvature defined by the etching radius (r) at a surface of the glass substrate (3) and that are delimited by respective convex ribs (9), and ty/r<0.1, where
r=the local etching radius (27) and ty=a lateral depth (14) of the respective indentations (8), and
ty/B<0.1, where B=a maximal width (15) of the respective finger (24) transversely to a direction of extent (2) thereof.

### Claim 20 (depends on 15)

The method as claimed in claim 15, further comprising applying a metallization (30) serving to form electrodes of the fingers (24) using
a shadow mask or
a spray photoresist or
a dry photoresist laminated
as a masking layer on sidewalls (13) of the fingers (24).

### Claim 21 (depends on 1)

A portable electronic device, comprising the micromechanical comb structure (25) made of glass as claimed in claim 1,
wherein the fingers (24) of the comb structure (25) have a respective length of >100 μm.