# US 2026/0001159 A1 · Method for friction stir welding or processing high strength steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0001159 A1
- Document ID: US20260001159A1
- Status: Published application
- Kind: A1
- Application number: 19/322,873
- Filed: 2025-09-09
- Published: 2026-01-01
- Earliest claimed: 2023-09-26
- Assignees: Fca US LLC
- Applicants: Fca US LLC
- Inventors: Bryan Macek
- Web page: https://patentgrep.com/patent/US20260001159A1

## CPC

- B23K 20/1235: {with temperature control during joining}
- B23K 20/24: Preliminary treatment
- B23K 20/26: Auxiliary equipment
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method of processing high-strength steel includes providing a first piece of high-strength steel. Friction stir processing the first piece of high strength steel is performed by pre-heating an area in advance of a friction stir welding tool and moving the friction stir welding tool between 500 mm and 300 mm per minute to attain a mixed zone having a mixed zone temperature at the mixed zone between a eutectoid temperature and a forge welding temperature from a combination of the friction from the friction welding tool and the step of pre-heating.

## Claims

### Claim 1

A method of processing high-strength steel comprising:
providing a first piece of steel;
providing a second piece of high-strength steel having a tensile strength between 590 MPa and 2000 MPa and abutting the first piece of steel;
friction stir welding the first piece of steel and the second piece of high strength steel by:
pre-heating a preheating zone in a joint area in advance of a friction stir welding tool; and
moving the friction stir welding tool between 500 mm and 3000 mm per minute to attain a mixed zone between the first piece and the second piece having a mixed zone temperature at the mixed zone between a eutectoid temperature of 727 C and a forge welding temperature of the second piece of high-strength steel of 1500 C from a combination of the friction from the friction welding tool and the step of pre-heating, wherein the step of pre-heating provides more than half of a heat at the mixed zone and moving the friction stir welding tool provides less than half of the heat at the mixed zone.

### Claim 2 (depends on 1)

The method of claim 1 wherein preheating the joint area comprises preheating by laser ablating a coating from a surface.

### Claim 3 (depends on 1)

The method of claim 1 wherein preheating the joint area comprises pre-heating by laser, induction heating or plasma heating.

### Claim 4 (depends on 1)

The method of claim 1 further comprising post heating the mixed zone to reduce hardness.

### Claim 5 (depends on 1)

The method of claim 1 further comprising post heating the mixed zone to relieve stress.

### Claim 6 (depends on 1)

The method of claim 1 further comprising post-heating the mixed zone to a temperature between 180 C and 500 C.

### Claim 7 (depends on 1)

The method of claim 1 further comprising post-heating the mixed zone to a temperature between 300 C and 400 C.

### Claim 8 (depends on 1)

The method of claim 1 further comprising post-heating the mixed zone comprises pre-heating by laser, induction or plasma pre-heating.

### Claim 9 (depends on 1)

The method of claim 1 wherein the first piece steel has a different strength than the second piece of high-strength steel.

### Claim 10 (depends on 1)

The method of claim 1 wherein the first piece of steel comprises advanced high strength steel.

### Claim 11 (depends on 1)

The method of claim 1 wherein the first piece of steel is composed of ultra-high strength steel.

### Claim 12 (depends on 1)

The method of claim 1 wherein the first piece has a first thickness, and the second piece has a second thickness greater than the first thickness.

### Claim 13 (depends on 12)

The method of claim 12 wherein the mixed zone comprises an angular transition from the first thickness to the second thickness.

### Claim 14 (depends on 1)

The method of claim 1 wherein the first piece has a first thickness and a first strength, and the second piece has a second thickness and a second strength, said second thickness greater than the first thickness, said first strength greater than the second strength.

### Claim 15 (depends on 1)

The method of claim 1 wherein the first piece has a first thickness and a first strength, and the second piece has a second thickness and a second strength, said second thickness greater than the first thickness, said first strength less than the second strength.

### Claim 16 (depends on 1)

The method of claim 1 wherein the first piece has a first thickness and a first strength, and the second piece has a second thickness and a second strength, said second thickness greater than the first thickness, said first strength the same as the second strength.

### Claim 17 (depends on 1)

The method of claim 1 wherein the mixed zone is non-linear.

### Claim 18 (depends on 1)

The method of claim 1 wherein the first piece of steel is high-strength steel has a tensile strength between 590 MPa and 2000 MPa.