# US 2025/0386643 A1 · Display device, electronic apparatus and method of manufacturing display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0386643 A1
- Document ID: US20250386643A1
- Status: Published application
- Kind: A1
- Application number: 19/079,134
- Filed: 2025-03-13
- Published: 2025-12-18
- Earliest claimed: 2024-06-17
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., LTD.
- Inventors: In Tae SON; Won Seok KIM; Jue Youn PARK; Kang Woo LEE; Da Song LEE; Hyun Jung LEE; Jin Yeong HEO
- Web page: https://patentgrep.com/patent/US20250386643A1

## CPC

- H10H 29/8506: {Containers}
- H10H 29/012: {of active-matrix LED displays}
- H10H 29/036: {of packages}
- H10H 29/0362: {of encapsulations}
- H10H 29/39: Connection of the pixel electrodes to the driving transistors
- H10H 29/49: Interconnections, e.g. wiring lines or terminals (connection of the pixel electrodes to the driving transistors H10H29/39)
- H10H 29/854: characterised by their material, e.g. epoxy or silicone resins
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

In a method of manufacturing a display device, the method may include: selecting a pre-adhesive layer by measuring a free volume of the pre-adhesive layer; and forming an adhesive layer and a cover window on a display panel. In the selecting of the pre-adhesive layer, the pre-adhesive layer selected may form the adhesive layer.

## Claims

### Claim at position 1

1 what is claimed is:

### Claim 1

A method of manufacturing a display device, the method comprising:
selecting a pre-adhesive layer by measuring a free volume of the pre-adhesive layer; and
forming an adhesive layer and a cover window on a display panel,
wherein, in the selecting of the pre-adhesive layer, the pre-adhesive layer selected forms the adhesive layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein a free volume of the pre-adhesive layer selected is less than 0.035 times of a volume of the pre-adhesive layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the selecting of the pre-adhesive layer comprises not selecting the pre-adhesive layer when the free volume of the pre-adhesive layer is 0.035 times or more of the volume of the pre-adhesive layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein, in the selecting of the pre-adhesive layer, the free volume is measured using a positive electron extinction method.

### Claim 5 (depends on 4)

The method of claim 4, wherein the free volume is derived by substituting a value R calculated from Expression 1 in
4
⁢
π
?
?
:
?
indicates text missing or illegible when filed
τ
⁢
3
=
0.5
×
[
1
-
R
R
+
Δ
⁢
R
+
1
2
⁢
π
⁢
sin
⁡
(
2
⁢
π
⁢
R
R
+
Δ
⁢
R
)
]
-
1
,
Expression
⁢
1
wherein, in Expression 1, τ3 is a lifetime of orthopositronium (o-PS), which is measured using the positive electron extinction method, R is an average radius of the free volume when the pre-adhesive layer is assumed to be a sphere, and AR is 0.1656 nm.

### Claim 6 (depends on 5)

The method of claim 5, wherein the forming of the adhesive layer and the cover window on the display panel comprises:
laminating the pre-adhesive layer selected on the display panel;
forming the cover window on the pre-adhesive layer; and
performing an autoclave process.

### Claim 7 (depends on 6)

The method of claim 6, wherein the laminating comprises laminating the pre-adhesive layer using a roller, or laminating the pre-adhesive layer by inputting the pre-adhesive layer to a vacuum chamber.

### Claim 8 (depends on 1)

The method of claim 1, wherein, in the selecting of the pre-adhesive layer, the free volume is derived by substituting a value R calculated from Expression 1 in
4
⁢
π
?
?
,
?
indicates text missing or illegible when filed
and in the selecting of the pre-adhesive layer, the selected pre-adhesive layer satisfies Expression 2:
τ
⁢
3
=
0.5
×
[
1
-
R
R
+
Δ
⁢
R
+
1
2
⁢
π
⁢
sin
⁡
(
2
⁢
π
⁢
R
R
+
Δ
⁢
R
)
]
-
1
,
Expression
⁢
1
wherein, in Expression 1, τ3 is a lifetime of orthopositronium (o-PS), which is measured using a positive electron extinction method, R is an average radius of the free volume when the pre-adhesive layer is assumed to be a sphere, and AR is 0.1656 nm, and
Free
⁢
Volume
⁢
of
⁢
Pre
-
adhesive
⁢
⁠
Layer
/
Volume
⁢
of
⁢
Pre
-
adhesive
⁢
Layer
<
0.035
.
Expression
⁢
2

### Claim 9 (depends on 8)

The method of claim 8, wherein the adhesive layer is between the display panel and the cover window.

### Claim 10

A display device comprising:
a display panel;
an adhesive layer on the display panel; and
a cover window on the adhesive layer,
wherein a free volume of the adhesive layer is less than 0.035 times of a volume of the adhesive layer.

### Claim 11 (depends on 10)

The display device of claim 10, wherein the free volume is derived by substituting a value R calculated from Expression 1 in
4
⁢
π
?
?
:
?
indicates text missing or illegible when filed
τ
⁢
3
=
0.5
×
[
1
-
R
R
+
Δ
⁢
R
+
1
2
⁢
π
⁢
sin
⁡
(
2
⁢
π
⁢
R
R
+
Δ
⁢
R
)
]
-
1
,
Expression
⁢
1
wherein, in Expression 1, τ3 is a lifetime of orthopositronium (o-PS), which is measured using a positive electron extinction method, R is an average radius of the free volume when the adhesive layer is assumed to be a sphere, and AR is 0.1656 nm.

### Claim 12 (depends on 11)

The display device of claim 11, wherein a bottom surface of the adhesive layer is in contact with the display panel, and a top surface of the adhesive layer is in contact with the cover window.

### Claim 13

An electronic apparatus comprising:
a display device; and
a housing accommodating the display device,
wherein the display device comprises:
a display panel;
an adhesive layer on the display panel; and
a cover window on the adhesive layer,
wherein a free volume of the adhesive layer is less than 0.035 times of a volume of the adhesive layer.