# US 2025/0385387 A1 · Composite separator, preparation method therefor, and lithium-sulfur battery containing composite separator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0385387 A1
- Document ID: US20250385387A1
- Status: Published application
- Kind: A1
- Application number: 18/879,516
- Filed: 2022-09-28
- Published: 2025-12-18
- Earliest claimed: 2022-06-28
- Assignees: China Petroleum & Chemical Corporation; Shanghai Research Institute of Petrochemical Technology, Sinopec
- Applicants: China Petroleum & Chemical Corporation; Shanghai Research Institute of Petrochemical Technology, Sinopec
- Inventors: Weimin YANG; Xiaofei WANG; Dawei LAN; Jun LI; Zhendong WANG; Haoliang XUE; Daoming ZHANG; Sifei ZHOU
- Web page: https://patentgrep.com/patent/US20250385387A1

## CPC

- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 4/38: of elements or alloys
- H01M 10/052: Li-accumulators
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/417: Polyolefins
- H01M 50/426: Fluorocarbon polymers
- H01M 50/431: Inorganic material
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A composite separator and a preparation method therefor, as well as a lithium-sulfur battery containing the composite separator are provided. The composite separator has a polymer substrate film and a composite layer disposed on the surface of the polymer substrate film. The composite layer includes a molecular sieve and a conductive carbon material. The molecular sieve contains cobalt and optionally lithium.

## Claims

### Claim 1

A composite separator, characterized by comprising a polymer substrate film and a composite layer disposed on the surface of the polymer substrate film, wherein the composite layer comprises a molecular sieve and a conductive carbon material, wherein the molecular sieve contains cobalt.

### Claim 2 (depends on 1)

The composite separator of claim 1, wherein
the composite layer has a thickness of 5-50 μm, preferably 10-40 μm; and/or
the conductive carbon material and the molecular sieve in the composite layer are in a mass ratio of 1(1-9), preferably 1:(2-9).

### Claim 3 (depends on 1)

The composite separator of claim 1, wherein the molecular sieve further contains lithium;
preferably, lithium is present in the molecular sieve in an amount of 0.1-5 wt %, preferably 0.2-3 wt %, more preferably 0.5-2.5 wt %, on lithium ion basis;
preferably, cobalt is present in the molecular sieve in an amount of 1-30 wt %, preferably 1-15 wt %, more preferably 2-7 wt %, on element cobalt basis.

### Claim 4 (depends on 3)

The composite separator of claim 3, wherein the molecular sieve has at least one topological structure selected from the group consisting of MFI, MWW, GIS, BEC, FAU and MOR, preferably at least one topological structure selected from the group consisting of MFI, MWW and GIS.

### Claim 5 (depends on 1)

The composite separator of claim 1, wherein
the material of the polymer substrate film is at least one of polyethylene, polypropylene, polyimide, polyacrylonitrile, polyethylene terephthalate, polytetrafluoroethylene and polyvinylidene fluoride, preferably polyethylene and/or polypropylene; and/or
the conductive carbon material is at least one of graphene, graphene oxide, reduced graphene oxide, carbon nanotubes, carbon nanofibers, acetylene black, Super P and Ketjen black, preferably at least one of graphene, graphene oxide and reduced graphene oxide.

### Claim 6 (depends on 1)

A method for preparing the composite separator of claim 1, characterized by comprising the steps of:
(1) mixing a molecular sieve and a conductive carbon material to obtain a mixture, wherein the molecular sieve contains cobalt;
(2) dispersing the mixture and a binder in a solvent to obtain a coating slurry;
(3) coating the coating slurry on the surface of a polymer substrate film, and then removing the solvent, to obtain the composite separator.

### Claim 7 (depends on 6)

The method of claim 6, wherein the method further comprises: obtaining the molecular sieve by: mixing a cobalt ion solution with a raw molecular sieve, and subjecting to drying and reducing, to obtain a cobalt containing molecular sieve.

### Claim 8 (depends on 6)

The method of claim 6, wherein the molecular sieve further contains lithium, and wherein the method further comprises: obtaining the molecular sieve by:
S1, exchanging a raw molecular sieve with a lithium ion solution, and subjecting to washing and drying, to obtain a precursor I; and
S2, mixing a cobalt ion solution with the precursor I, and subjecting to drying and reducing, to obtain the molecular sieve which contains cobalt and lithium.

### Claim 9 (depends on 7)

The method of claim 7, wherein
the lithium ion solution is at least one selected from the group consisting of a lithium chloride solution, a lithium sulfate solution, and a lithium nitrate solution; and/or
the exchanging is operated at conditions including: a temperature of 40-100° C., and a liquid-to-solid ratio of 10-50; preferably, the exchanging is operated 1-3 times; and/or
the cobalt ion solution is at least one selected from the group consisting of cobalt chloride solution, cobalt nitrate solution, cobalt sulfate solution and cobalt acetate solution; and/or
the reducing is operated under a hydrogen atmosphere at a temperature of 600-750° C. for 1-4h; and/or
the raw molecular sieve has a chemical composition of xM2O·ySiO2·zAl2O3, wherein 0.01≤x/y≤0.2, 10≤y/z≤50; and M is one or two selected from the group consisting of Na and K, preferably Na; and/or
the raw molecular sieve is at least one selected from the group consisting of MFI, MWW, GIS, BEC, FAU and MOR, preferably at least one of MFI, MWW and GIS.

### Claim 10 (depends on 7)

The method of claim 7, wherein the molecular sieve has at least one topological structure selected from the group consisting of MFI, MWW, GIS, BEC, FAU and MOR; preferably at least one topological structure selected from the group consisting of MFI, MWW and GIS;
preferably, lithium is present in the molecular sieve in an amount of 0.1-5 wt %, preferably 0.2-3 wt %, more preferably 0.5-2.5 wt %, on lithium ion basis;
preferably, cobalt is present in the molecular sieve in an amount of 1-30 wt %, preferably 1-15 wt %, more preferably 2-7 wt %, on element cobalt basis.

### Claim 11 (depends on 6)

The method of claim 6, wherein
the solvent in step (2) is at least one selected from the group consisting of deionized water, anhydrous ethanol, N,N-dimethylacetamide, N,N-dimethylformamide, dimethyl sulfoxide and N-methylpyrrolidone, preferably N-methylpyrrolidone; and/or
the binder in step (2) is at least one of polyvinyl alcohol, carboxymethyl cellulose, polyvinylidene fluoride, polytetrafluoroethylene, polyvinyl pyrrolidone, styrene-butadiene rubber and polyacrylate, preferably polyvinylidene fluoride; and/or
the coating in step (3) is at least one of casting, blade coating, spray coating and spin coating, preferably blade coating

### Claim 12 (depends on 1)

A lithium-sulfur battery, characterized by comprising a cathode, an anode and the composite separator of claim 1 between the cathode and the anode.