# US 2025/0385240 A1 · Method for manufacturing electrode for all-solid state battery, electrode free standing membrane, electrode, and all-solid state battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0385240 A1
- Document ID: US20250385240A1
- Status: Published application
- Kind: A1
- Application number: 18/939,151
- Filed: 2024-11-06
- Published: 2025-12-18
- Earliest claimed: 2024-06-18
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Ju Yeon Lee; Gyeong Jun Chung; Min Sun Kim; So Ri Lee; Seung Hwan Moon; Seul Gi Choi; Young Jin Nam; Jong Jung Kim
- Web page: https://patentgrep.com/patent/US20250385240A1

## CPC

- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/623: {fluorinated polymers}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are a method for dry-manufacturing an electrode for an all-solid state battery, an electrode free standing membrane prepared through the manufacturing method, an electrode, and an all-solid state battery including the same. This dry process eliminates solvents, making it environmentally friendly and efficient. The method involves forming an electrode active material complex by mixing the active material with a solid electrolyte, combining it with a conductive material and binder, and then rolling the mixture into an electrode film. The film is bonded to a current collector, ensuring strong adhesion and mechanical stability. The free-standing membrane enhances ion and electron conductivity, improving overall battery performance. The resulting all-solid-state battery offers higher energy density, longer cycle life, and increased safety, making it well-suited for electric vehicles, portable electronics, and advanced energy storage applications.

## Claims

### Claim 1

A method for manufacturing an electrode for an all-solid state battery, the method comprising:
mixing an electrode active material with a solid electrolyte to prepare an electrode active material complex (S1);
mixing the electrode active material complex, a conductive material, and a binder to prepare a mixture (S2);
rolling the mixture in a clay status to form an electrode film (S3); and
binding a current collector with the electrode film (S4),
wherein a ratio (D2/D1) between an average particle size (D2) of the binder and an average particle size (D1) of the electrode active material complex is at most about 20.

### Claim 2 (depends on 1)

The method of claim 1, wherein the electrode active material complex is prepared by coating a solid electrolyte shell on an electrode active material core, and
wherein a ratio (b/a) between a diameter (a) of the electrode active material core and a thickness (b) of the solid electrolyte shell ranges from about 0.05 to 0.5.

### Claim 3 (depends on 1)

The method of claim 1, wherein an average particle size of the electrode active material ranges from about 1 μm to 50 μm.

### Claim 4 (depends on 1)

The method of claim 1, wherein an average particle size of the solid electrolyte ranges from about 0.01 μm to 20 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein an average particle size of the binder is at most about 500 μm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the binder comprises polytetrafluoroethylene (PTFE) or polyvinylidene fluoride-hexapropylene (PVDF-HFP) copolymer.

### Claim 7 (depends on 1)

The method of claim 1, wherein a content of the binder in the electrode is at most about 5 wt %.

### Claim 8 (depends on 1)

The method of claim 1, wherein the S1 and the S2 are performed in absence of a solvent.

### Claim 9 (depends on 1)

The method of claim 1, wherein the S2 further comprises:
performing a needing process to change the mixture to be in the clay status.

### Claim 10 (depends on 1)

The method of claim 1, wherein the rolling process is performed using a primary roller and a secondary roller.

### Claim 11 (depends on 10)

The method of claim 10, wherein a roll speed ratio of the primary roller ranges from about 1:0.05 to 1:5.

### Claim 12 (depends on 10)

The method of claim 10, wherein a roll speed ratio of the secondary roller ranges from about 1:5 to 1:15.

### Claim 13 (depends on 1)

The method of claim 1, wherein a stretching speed in the S3 is at most about 20 mm/min.

### Claim 14 (depends on 1)

The method of claim 1, wherein the S3 is performed at a temperature ranging from about 50° C. to 90° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the electrode is a positive electrode.

### Claim 16

An electrode free standing membrane comprising:
an electrode active material complex comprising:
an electrode active material core and
a solid electrolyte on the electrode active material core;
a binder, and
a conductive material,
wherein a ratio (b/a) between a diameter (a) of the electrode active material core and a thickness (b) of the solid electrolyte shell ranges from about 0.05 to 0.5.

### Claim 17

An electrode free standing membrane comprising:
an electrode active material complex comprising an electrode active material and a solid electrolyte;
a binder, and
a conductive material,
wherein a ratio (D2/D1) between an average particle size (D1) of the electrode active material complex and an average particle size (D2) of the binder is at most about 20.

### Claim 18 (depends on 17)

The electrode free standing membrane of claim 17, wherein the electrode active material complex is prepared by coating a solid electrolyte shell on an electrode active material core, and
wherein a ratio (b/a) between a diameter (a) of the electrode active material core and a thickness (b) of the solid electrolyte shell ranges from about 0.05 to 0.5.

### Claim 19 (depends on 16)

An electrode comprising:
the electrode free standing membrane according to claim 16; and
a current collector.

### Claim 20 (depends on 19)

An all-solid state battery comprising:
the electrode according to claim 19;
an opposite electrode; and
a solid electrolyte layer interposed between the electrode and the opposite electrode.