# US 2025/0385155 A1 · Package structure and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0385155 A1
- Document ID: US20250385155A1
- Status: Published application
- Kind: A1
- Application number: 18/949,083
- Filed: 2024-11-15
- Published: 2025-12-18
- Earliest claimed: 2024-06-13
- Assignees: Sureway Technology Co.,Ltd.
- Applicants: Sureway Technology Co.,Ltd.
- Inventors: Hsing-Hua TSAI; Song-Huan SUN; Ming-Chih HSU; Tung-Han CHUANG; Chih-Hsin TSAI
- Web page: https://patentgrep.com/patent/US20250385155A1

## CPC

- H10W 40/228: {the projecting parts being wire-shaped or pin-shaped}
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A package structure includes a substrate; a chip disposed on the substrate and having a backside surface away from the substrate; a fin heat sink having a surface facing the chip disposed above the substrate; a thermal interface material disposed between the chip and the fin heat sink; and a twinned layer disposed on at least one side of the thermal interface material and in direct contact with the thermal interface material. A method for forming the package structure is also provided.

## Claims

### Claim 1

A package structure, comprising:
a substrate;
a chip disposed on the substrate and having a backside surface away from the substrate;
a heat sink disposed over the substrate, wherein the heat sink has a surface facing the chip;
a thermal interface material (TIM) disposed between the chip and the heat sink; and
a twinned layer disposed on at least one side of the TIM and in direct contact with the TIM.

### Claim 2 (depends on 1)

The package structure of claim 1, wherein the twinned layer is disposed between the TIM and the heat sink, and the twinned layer comprises a plurality of discrete segments spaced apart from each other on a same level.

### Claim 3 (depends on 1)

The package structure of claim 1, wherein the twinned layer comprises gold, silver, copper, or silver-copper alloy, and has at least 1% twinned structures in its crystal structure.

### Claim 4 (depends on 1)

The package structure of claim 1, wherein the twinned layer has a thickness of 0.1 to 100 μm.

### Claim 5 (depends on 1)

The package structure of claim 1, wherein the chip comprises a metal layer on the backside surface, wherein the metal layer comprises at least one of Al/Ti/NiV/Au, Al/Cr/NiV/Au, Al/NiV/Au, Al/W/Au, Ti/NiV/Au, TiW/Au, Cr/NiV/Au, Cr/Au, W/Au, WTi/Au, WTi/Ti/Au, Al/Ti/Ni/Au, Ti/Ni/Ag, Ti/Ag, Al/Ti/NiV/Ag, Al/Cr/NiV/Ag, Al/NiV/Ag, Al/W/Ag, Ti/NiV/Ag, TiW/Ag, Cr/NiV/Ag, Cr/Ag, W/Ag, WTi/Ag, WTi/Ti/Ag, Al/Ti/Ni/Ag, Rh, Ir, Pd, and Pt, and the metal layer has a thickness of 0.001 to 10 μm.

### Claim 6 (depends on 1)

The package structure of claim 1, wherein the heat sink is a heat-dissipating metal lid and/or a cooling fin.

### Claim 7 (depends on 1)

The package structure of claim 1, wherein the heat sink comprises copper (Cu), aluminum (Al), cobalt (Co), nickel (Ni), nickel plated copper, silicon carbide (SiC), nitrogen aluminum (AIN), graphite, or a combination thereof.

### Claim 8 (depends on 1)

The package structure of claim 1, wherein the heat sink comprises a metal layer on the surface, wherein the metal layer comprises at least one of Au, Ag, Cu, Ni, Ti/Ag, Ti/Ni/Ag, Ti/Cu, Ti/Ni/Cu, Ni/Ag, Ni/Au, Ni/Cu, Rh, Ir, Pd, and Pt, and the metal layer has a thickness of 0.001 to 10 μm.

### Claim 9 (depends on 8)

The package structure of claim 8, wherein the metal layer comprises a plurality of discrete portions spaced apart from each other on a same level.

### Claim 10 (depends on 1)

The package structure of claim 1, wherein the TIM comprises an indium-based alloy or a tin-based alloy.

### Claim 11 (depends on 10)

The package structure of claim 10, wherein the indium-based alloy comprises at least one of:
30 to 35 wt % of bismuth, 15 to 18 wt % of tin, and a balance of indium, with a melting point of 55 to 65° C.;
30 to 35 wt % of bismuth and a balance of indium, with a melting point of 70 to 75° C.;
52 to 60 wt % of bismuth, 15 to 18 wt % of tin, and a balance of indium, with a melting point of 80 to 85° C.;
48 to 50 wt % of tin and a balance of indium, with a melting point of 110 to 120° C.;
0.1 to 15 wt % of silver and a balance of indium, with a melting point of 140 to 280° C.; and
100 wt % of indium with a melting point of 150 to 160° C.

### Claim 12 (depends on 10)

The package structure of claim 10, wherein the tin-based alloy comprises tin, tin-silver, tin-silver-copper, or tin-silver-copper-nickel-germanium.

### Claim 13 (depends on 1)

The package structure of claim 1, wherein the chip has an orthogonal projection area on the surface of the heat sink, and a coverage of the TIM on the backside surface of the chip or the orthogonal projection area is greater than 90%.

### Claim 14 (depends on 1)

The package structure of claim 1, wherein the twinned layer is configured to at least partially fuse into the TIM.

### Claim 15

A method for forming a package structure, comprising:
disposing a chip on a substrate, wherein the chip has a backside surface away from the substrate;
providing a heat sink, wherein the heat sink has a surface corresponding to the backside surface of the chip, and the chip has an orthogonal projection area on the surface of the heat sink;
forming a twinned layer on the backside surface of the chip and/or the surface of the heat sink;
disposing a thermal interface material (TIM) on the twinned layer; and
bonding the surface of the heat sink toward the backside surface of the chip so that the twinned layer is positioned on at least one side of the TIM.

### Claim 16 (depends on 15)

The method of claim 15, wherein disposing the TIM on the twinned layer comprises applying pressure at a single point or multiple points to the TIM towards the surface of the twinned layer to affix the TIM on the twinned layer.

### Claim 17 (depends on 15)

The method of claim 15, wherein bonding the surface of the heat sink toward the backside surface of the chip comprises:
performing a hot press process to make a coverage of the TIM melted on the backside surface of the chip or the orthogonal projection area greater than 90%.

### Claim 18 (depends on 17)

The method of claim 17, wherein the hot press process comprises applying a force greater than 1 gf/cm2 to the heat sink for a duration of 2 seconds to 10 minutes at a temperature greater than 50° C. in a process chamber under pressure or vacuum.

### Claim 19 (depends on 15)

The method of claim 15, wherein the heat sink is a heat-dissipating metal lid, and after bonding the heat sink to the chip, the method further comprises disposing a cooling fin over the heat-dissipating metal lid.

### Claim 20 (depends on 15)

The method of claim 15, wherein, prior to forming the twinned layer, the method further comprises forming a metal layer on the backside surface of the chip and/or the surface of the heat sink.

### Claim 21 (depends on 20)

The method of claim 20, wherein the metal layer and/or the twinned layer is at least partially fused into the TIM.