# US 2025/0385103 A1 · Semiconductor Device and Method of Making Using Microwave Soldering

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0385103 A1
- Document ID: US20250385103A1
- Status: Published application
- Kind: A1
- Application number: 18/740,525
- Filed: 2024-06-12
- Published: 2025-12-18
- Earliest claimed: 2024-06-12
- Assignees: JCET STATS ChipPAC Korea Limited
- Applicants: JCET STATS ChipPAC Korea Limited
- Inventors: Yeojun Yun; SeungHyun Lee; HeeSoo Lee
- Web page: https://patentgrep.com/patent/US20250385103A1

## CPC

- H10W 70/099: {Connecting interconnections to insulating or insulated package substrates, interposers or redistribution layers}
- B23K 1/0016: {Soldering of electronic components}
- B23K 1/005: Soldering by means of radiant energy
- B23K 1/203: {Fluxing, i.e. applying flux onto surfaces}
- H10W 74/117: {the substrate having spherical bumps for external connection}
- H10W 90/701: {characterised by the relative positions of pads or connectors relative to package parts}
- B23K 2101/40: Semiconductor devices
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A semiconductor device has a semiconductor package and a flux disposed on the semiconductor package. A solder ball is disposed on the flux. The solder ball is reflowed using microwave energy. The microwave energy is applied until a temperature of the flux reaches between 200 and 220° C. The flux and solder ball both include polarized molecules. The substrate is devoid of polarized molecules.

## Claims

### Claim 1

A method of making a semiconductor device, comprising:
providing a semiconductor package;
disposing a flux on the semiconductor package;
disposing a solder ball on the flux; and
reflowing the solder ball using microwave energy.

### Claim 2 (depends on 1)

The method of claim 1, further including applying the microwave energy until a temperature of the flux reaches between 200 and 220° C.

### Claim 3 (depends on 2)

The method of claim 2, further including maintaining approximately the maximum temperature reached for 30 seconds.

### Claim 4 (depends on 1)

The method of claim 1, further including forming the semiconductor package prior to reflowing the solder ball by,
providing a substrate;
disposing an electrical component over the substrate; and
depositing an encapsulant over the electrical component.

### Claim 5 (depends on 4)

The method of claim 4, wherein the substrate is devoid of polarized molecules.

### Claim 6 (depends on 5)

The method of claim 5, wherein the flux and solder ball both include polarized molecules.

### Claim 7

A method of making a semiconductor device, comprising:
providing a substrate;
disposing a flux on the substrate;
disposing a solder ball on the flux; and
reflowing the solder ball using microwave energy.

### Claim 8 (depends on 7)

The method of claim 7, further including applying the microwave energy until a temperature of the flux reaches between 200 and 220° C.

### Claim 9 (depends on 8)

The method of claim 8, further including maintaining approximately the maximum temperature reached for 30 seconds.

### Claim 10 (depends on 7)

The method of claim 7, further including,
disposing an electrical component over the substrate;
depositing an encapsulant over the electrical component; and
disposing the flux and solder ball over the substrate opposite the encapsulant.

### Claim 11 (depends on 7)

The method of claim 7, wherein the substrate is devoid of polarized molecules.

### Claim 12 (depends on 11)

The method of claim 11, wherein the flux and solder ball include polarized molecules.

### Claim 13 (depends on 7)

The method of claim 7, wherein the substrate includes an insulating material and a conductive layer formed over the insulating material.

### Claim 14

A method of making a semiconductor device, comprising:
providing a substrate;
disposing a solder ball over the substrate; and
reflowing the solder ball using microwave energy.

### Claim 15 (depends on 14)

The method of claim 14, further including applying the microwave energy until a temperature of the solder ball reaches between 200 and 220° C.

### Claim 16 (depends on 15)

The method of claim 15, further including maintaining approximately the maximum temperature reached for 30 seconds.

### Claim 17 (depends on 14)

The method of claim 14, further including,
disposing an electrical component over the substrate;
depositing an encapsulant over the electrical component; and
disposing the solder ball over the substrate opposite the encapsulant.

### Claim 18 (depends on 14)

The method of claim 14, wherein the substrate is devoid of polarized molecules.

### Claim 19 (depends on 18)

The method of claim 18, wherein the solder ball includes polarized molecules.

### Claim 20 (depends on 14)

The method of claim 14, wherein the solder ball includes polarized molecules.

### Claim 21

A semiconductor device, comprising:
a substrate;
a solder ball disposed over the substrate; and
a microwave emitter disposed over the substrate.

### Claim 22 (depends on 21)

The semiconductor device of claim 21, further including:
an electrical component disposed over the substrate opposite the solder ball; and
an encapsulant deposited over the electrical component and substrate.

### Claim 23 (depends on 21)

The semiconductor device of claim 21, further including a flux disposed between the substrate and solder ball.

### Claim 24 (depends on 21)

The semiconductor device of claim 21, wherein the substrate is devoid of polarized molecules.

### Claim 25 (depends on 24)

The semiconductor device of claim 24, wherein the solder ball includes polarized molecules.