# US 2025/0378318 A1 · Memristor structures with analog switching characteristics and method for fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0378318 A1
- Document ID: US20250378318A1
- Status: Published application
- Kind: A1
- Application number: 18/736,611
- Filed: 2024-06-07
- Published: 2025-12-11
- Earliest claimed: 2024-06-07
- Assignees: VNU-HCM University of Science
- Inventors: NGOC KIM PHAM; QUAN PHU PHAM; THANG BACH PHAN; THUAT TRAN NGUYEN
- Web page: https://patentgrep.com/patent/US20250378318A1

## CPC

- G06N 3/065: Analogue means
- G06N 3/049: Temporal neural networks, e.g. delay elements, oscillating neurons or pulsed inputs
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- G06N: COMPUTING ARRANGEMENTS BASED ON SPECIFIC COMPUTATIONAL MODELS
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method for fabricating a memristor and a memristor device are disclosed which comprises: depositing a first metal electrode on a substrate; depositing a Chromium oxide (CrOx) layer directly on top of a first metal electrode; depositing a Titanium oxide (TiOy) layer directly on top of the CrOx layer; and depositing a second metal electrode on the TiOy layer.

## Claims

### Claim 1

A method for fabricating a memristor device, comprising:
(a) depositing a first metal electrode on a substrate using a physical vapor deposit (PVD) method, wherein said first metal electrode has a dog bone shape and a first terminal and a second terminal;
(b) depositing a Chromium oxide (CrOx) layer directly on top and on a middle section of said first metal electrode using said physical vapor deposit (PVD) method with Chromium (Cr) having a purity of 99.95%;
(c) depositing a Titanium oxide (TiOy) layer directly on top of said CrOx layer using said physical vapor deposit (PVD) method with Titanium (Ti) vapor having a purity of 99.2%-99.7%; and
(d) depositing a second metal electrode directly on said TiOy layer using said physical vapor deposit (PVD) method; wherein said second metal electrode has a dog bone shape and a third terminal and a fourth terminal, said second metal electrode is deposited perpendicular to said first metal electrode; and said first terminal, said second terminal, said third terminal, and said fourth terminal are extended beyond the edges of said Chromium oxide (CrOx) layer and said Titanium oxide (TiOy) layer; wherein when a varying voltage potential is applied between said first metal electrode and said second metal electrode, respective switching resistances of said TiOy layer and said CrOx layer are gradually modulated so that an analog memory is resulted within said memristor.

### Claim 2 (depends on 1)

The method of claim 1 wherein said dog bone shape of said first metal electrode comprises a connective strip with a width of 500 μm and said first terminal and said second terminal have a 1.5 mm×1.5 mm square shape.

### Claim 3 (depends on 1)

The method of claim 1 wherein said first metal electrode comprises Titanium (Ti), wherein a first Schottky barrier diode is formed between said first metal electrode and said CrOx layer.

### Claim 4 (depends on 3)

The method of claim 3 wherein said first metal electrode has a thickness of 50 nm to 150 nm, preferably 70 nm.

### Claim 5 (depends on 4)

The method of claim 4 wherein said second metal electrode comprises Chromium (Cr), wherein a second Schottky barrier diode is formed between said second metal electrode and said TiOy layer.

### Claim 6 (depends on 5)

The method of claim 5 wherein said second metal electrode has a thickness of 50 nm to 150 nm, preferably 70 nm.

### Claim 7 (depends on 1)

The method of claim 1 wherein said substrate is a glass substrate.

### Claim 8 (depends on 1)

The method of claim 1 wherein said step (a) of depositing a first metal electrode on a substrate comprises said physical vapor deposit (PVD) method that uses a DC sputtering of Argon (Ar) gas in a vacuum chamber set at a working pressure of 3×10−3 Torr with a base vacuum pressure of 7.5×10−6 Torr.

### Claim 9 (depends on 8)

The method of claim 8 wherein electrodes of said vacuum chamber is applied a power of 100 W for 5 minutes.

### Claim 10 (depends on 9)

The method of claim 9 wherein said physical vapor deposit (PVD) method comprises a reactive sputtering deposition that uses Argon (Ar) and Oxygen (O2) gases in a vacuum chamber set at a pressure of 7×10−3 Torr with a base vacuum pressure of 7.5×10−6 Torr.

### Claim 11 (depends on 10)

The method of claim 10 wherein said dog bone shape of said second metal electrode comprises a connective strip with a width of 500 μm and said third terminal and said fourth terminal have a 1.5 mm×1.5 mm square shape.

### Claim 12 (depends on 1)

The method of claim 1 wherein said CrOx layer has a thickness of 130 nm.

### Claim 13 (depends on 1)

The method of claim 1 wherein said TiOy layer has a thickness of 160 nm.

### Claim 14

A memristor device, comprising:
a first metal electrode deposited on a glass substrate, wherein said first metal electrode has a dog bone shape and a first terminal and a second terminal;
a 99.95% Chromium (Cr) in a Chromium oxide (CrOx) layer deposited directly on top of and on a middle of said first metal electrode;
a 99.2%-99.7% Titanium in a Titanium oxide (TiOy) layer deposited directly on top of said CrOx layer; and
a second metal electrode formed directly on said TiOy layer; wherein said second metal electrode has a dog bone shape and a third terminal and a fourth terminal; said second metal electrode is deposited perpendicular to said first metal electrode; and said first terminal, said second terminal, said third terminal, and said terminal are extended beyond the edges of said Chromium oxide (CrOx) layer and said Titanium oxide (TiOy) layer; wherein when a varying voltage potential is applied between said first electrode and said second electrode, respective switching resistances of said TiOy layer and said CrOx layer are gradually modulated so that an analog memory is formed within said memristor.

### Claim 15 (depends on 14)

The memristor device of claim 14 wherein said first metal electrode comprises Titanium (Ti), wherein a first Schottky barrier diode is formed between said first metal electrode and said CrOx layer.

### Claim 16

The memristor device 15 wherein said Ti layer has a thickness between 50 nm to 150 nm, preferably 70 nm.

### Claim 17 (depends on 15)

The method of claim 15 wherein said second metal electrode comprises Chromium (Cr), wherein a second Schottky barrier diode is formed between said second metal electrode and said TiOy layer.

### Claim 18 (depends on 17)

The memristor device of claim 17 wherein said Cr layer has a thickness between 50 nm to 150 nm, preferably 70 nm.

### Claim 19

A neural network, comprising:
an input layer comprising a plurality of input neurons;
a plurality of hidden layers comprising a second plurality of processing neurons; and
an output layer comprising a plurality of output neurons, wherein said input layer, said plurality of hidden layers, and said output layers are connected together by a plurality of memristors, wherein each of said memristors further comprises:
a Titanium (Ti) electrode deposited on a glass substrate, wherein said Ti electrode has a dog bone shape and a first terminal and a second terminal;
a 99.95% Chromium (Cr) in a Chromium oxide (CrOx) layer directly on top of and on a middle of said Ti electrode;
a 99.2%-99.7% Titanium in a Titanium oxide (TiOy) layer directly on top of said CrOx layer; and
a Chromium (Cr) electrode formed directly on said TiOy layer; wherein said Cr electrode has a dog bone shape and a third terminal and a fourth terminal; said Cr electrode is deposited perpendicular to said Ti electrode; and said first terminal, said second terminal, said third terminal, and said fourth terminal are extended beyond the edges of said Chromium oxide (CrOx) and said Titanium oxide (TiOy); wherein when a varying voltage potential is applied between said first metal electrode and said second metal electrode, respective switching resistances of said TiOy layer and said CrOx layer are gradually modulated so that an analog memory is formed within said plurality of memristors.

### Claim 20 (depends on 19)

The neural network of claim 19 wherein said CrOx layer has a thickness of 130 nm, said TiOy layer has a thickness of 160 nm, said first Ti electrode has a thickness of 50 nm to 100 nm, preferably 70 nm; and said second Cr electrode has a thickness of 50 nm to 150 nm, preferably 70 nm, wherein a first Schottsky barrier diode is formed between said first metal electrode and said TiOy layer and wherein a second Schottky barrier diode is formed between said second metal electrode and said CrOx layer.