# US 2025/0376404 A1 · Methods and apparatus for manufacturing a glass ribbon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0376404 A1
- Document ID: US20250376404A1
- Status: Published application
- Kind: A1
- Application number: 19/311,593
- Filed: 2025-08-27
- Published: 2025-12-11
- Earliest claimed: 2019-06-20
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Bethany Jon Alderman; Naigeng Chen; Claire Renata Coble; Peter Joseph Lezzi; Yousef Kayed Qaroush; Elizabeth Mary Sturdevant
- Web page: https://patentgrep.com/patent/US20250376404A1

## CPC

- C03B 18/12: Making multilayer, coloured or armoured glass (chemical aspects C03C)
- C03B 18/14: Changing the surface of the glass ribbon, e.g. roughening (by chemical methods C03C)
- C03C 3/091: containing aluminium
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/0025: {by a laser beam}
- C03C 2218/34: Masking
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass ribbon includes a first major surface extending along a first plane. The glass ribbon includes a second major surface extending along a second plane substantially parallel to the first plane. A first thickness is defined between the first major surface and the second major surface along a thickness direction perpendicular to the first major surface. The first thickness is within a range from about 25 μm to about 125 μm. An edge surface extends between the first plane and the second plane. The edge surface comprises a height in the thickness direction that is less than the first thickness. Methods of manufacturing a glass ribbon are also provided.

## Claims

### Claim 1

A method of manufacturing a glass ribbon comprising:
masking a first region and a second region of a first major surface of the glass ribbon, such that the first major surface comprises a first exposed region between the first region and the second region;
masking a third region and a fourth region of a second major surface of the glass ribbon, such that the second major surface comprises a second exposed region between the third region and the fourth region; and
etching the first exposed region and the second exposed region to separate a first ribbon portion, comprising the first region and the third region, from a second ribbon portion, comprising the second region and the fourth region, and form a first tapered edge at the first ribbon portion and a second tapered edge at the second ribbon portion.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming, prior to etching, an initial groove at the first exposed region.

### Claim 3 (depends on 2)

The method of claim 2, wherein the forming the initial groove comprises one of: perforating the first exposed region at a plurality of locations; or scoring the first exposed region.

### Claim 4 (depends on 3)

The method of claim 3, wherein the etching the first exposed region and the second exposed region comprises exposing the first exposed region and the second exposed region to an etchant and concluding an exposure of the first exposed region and the second exposed region to the etchant prior to the first ribbon portion separating from the second ribbon portion.

### Claim 5 (depends on 4)

The method of claim 4, further comprising applying a mechanical force to the glass ribbon to separate the first ribbon portion from the second ribbon portion after concluding the exposure of the first exposed region and the second exposed region to the etchant, wherein the etching the first exposed region and the second exposed region comprises, following a separation of the first ribbon portion from the second ribbon portion, exposing the first tapered edge and the second tapered edge to a second etchant.

### Claim 6

A method of manufacturing a glass ribbon comprising:
forming an initial groove at one or more of a first major surface of the glass ribbon or a second major surface of the glass ribbon, the initial groove formed between a first ribbon portion of the glass ribbon and a second ribbon portion of the glass ribbon; and
etching the glass ribbon to reduce a thickness of the glass ribbon and separate the first ribbon portion from the second ribbon portion along the initial groove such that a first tapered edge is formed at the first ribbon portion and a second tapered edge is formed at the second ribbon portion.

### Claim 7 (depends on 6)

The method of claim 6, wherein the forming the initial groove comprises one of: perforating the first major surface at a plurality of locations between the first ribbon portion and the second ribbon portion; or scoring the first major surface between the first ribbon portion and the second ribbon portion.

### Claim 8 (depends on 6)

The method of claim 6, wherein the etching the glass ribbon comprises exposing the first major surface and the second major surface to an etchant and concluding an exposure of the first major surface and the second major surface to the etchant prior to the first ribbon portion separating from the second ribbon portion, and further comprising applying a mechanical force to the glass ribbon to separate the first ribbon portion from the second ribbon portion after concluding the exposure of the first major surface and the second major surface to the etchant.

### Claim 9

A method of manufacturing a glass ribbon comprising:
masking a first major surface of the glass ribbon so that at least a central portion of the first major surface is covered with a first mask;
exposing the first mask to a laser beam to ablate the first mask along a boundary separating a first ribbon portion from a second ribbon portion that is initially covered by the first mask to form a first exposed region of the glass ribbon that is not covered by the first mask;
separating the first ribbon portion from the second ribbon portion so that the first ribbon portion comprises a section of the first major surface extending along a first plane and a section of the second major surface extending along a second plane; and
etching the first exposed region to form a first tapered edge at the first ribbon portion.

### Claim 10 (depends on 9)

The method of claim 9, wherein the exposing the first mask to the laser beam removes material from the glass ribbon.

### Claim 11 (depends on 10)

The method of claim 10, wherein exposure of the first mask to the laser beam results in an initial groove being formed in the first major surface of the ribbon.

### Claim 12 (depends on 11)

The method of claim 11, wherein the initial groove comprises a plurality of perforations that are separated from one another and extend at least partially through the glass ribbon.

### Claim 13 (depends on 12)

The method of claim 12, wherein the plurality of perforations are disposed at a plurality of locations along the boundary.

### Claim 14 (depends on 13)

The method of claim 13, wherein the plurality of perforations extend completely through the glass ribbon.

### Claim 15 (depends on 9)

The method of claim 9, further comprising:
masking a second major surface of the glass ribbon so that at least a central portion of the second major surface is covered with the second mask; and
exposing the second mask to the laser beam to ablate the second mask along the boundary.

### Claim 16 (depends on 15)

The method of claim 15, wherein the etching of the first exposed region comprises exposing the first exposed region to an etchant after the separating.

### Claim 17 (depends on 16)

The method of claim 16, further comprising maintaining an initial thickness of the glass ribbon such that the initial thickness of the glass ribbon, defined between the first major surface and the second major surface at a first location spaced a distance apart from the first exposed region and the second exposed region, prior to the etching is substantially equal to a final thickness of the first ribbon portion, defined between the first major surface and the second major surface at the first location, after the etching, wherein the maintaining the initial thickness of the glass ribbon comprises maintaining the initial thickness within a range from about 20 μm to about 200 μm.

### Claim 18 (depends on 17)

The method of claim 17, wherein the maintaining the initial thickness of the glass ribbon comprises maintaining the initial thickness within a range from about 20 μm to about 100 μm.

### Claim 19 (depends on 9)

The method according to claim 9, wherein, after the etching and separating, the first tapered edge comprises:
an edge surface extending between the first plane and the second plane;
a first intermediate surface extending between a first outer edge of the section of the first major surface and a first outer edge of the edge surface;
a second intermediate surface extending between a first outer edge of the section of the second major surface and a second outer edge of the edge surface, wherein a first separating length between the first outer edge of the section first major surface and the edge plane in a direction parallel to the first major surface is within a range from about 5 μm to about 85 μm and a first separating thickness between the first outer edge of the edge surface and the first plane along a direction parallel to the edge plane is within a range from about 25 μm to about 100 μm.

### Claim 20 (depends on 19)

The method according to claim 19, wherein:
the first ribbon portion comprises a first thickness that is within a range from about 25 μm to about 125 μm,
the edge surface extends along an edge plane that is substantially perpendicular to the first plane, and
the edge surface comprises a height along the edge plane that is less than the first thickness.