# US 2025/0376402 A1 · Long Term Immobilization of Cesium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0376402 A1
- Document ID: US20250376402A1
- Status: Published application
- Kind: A1
- Application number: 19/210,336
- Filed: 2025-05-16
- Published: 2025-12-11
- Earliest claimed: 2024-05-17
- Applicants: University of Manitoba
- Inventors: Scott Kroeker; Arun Krishnamurthy
- Web page: https://patentgrep.com/patent/US20250376402A1

## CPC

- C03B 5/005: {of glass-forming waste materials (disposal or transformation of solid waste in general B09B; treatment of radioactive waste G21F9/00)}
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

Described herein is a method for combining waste-loaded zeolites and geopolymers with glass-forming components to produce materials with improved chemical durability and stability.

## Claims

### Claim 1

A method for preparing a waste-loaded vitrified zeolite composition comprising:
providing waste-loaded variants comprising waste-loaded CPT in dehydrated or non-dehydrated forms, either as CPT alone (CPT-Cs) or waste-loaded CPT as a geopolymer (CPT-Cs-GP), and at different stages of maturation;
adding suitable glass-forming chemicals to the waste-loaded variants, thereby forming a mixture;
grinding the mixture;
forming a melt from the mixture by heating; and
allowing the melt to cool, thereby forming a waste-loaded zeolite glass composition (CPT-Cs-GG and CPT-Cs-GP-GG).

### Claim 2 (depends on 1)

The method according to claim 1, wherein the waste-loaded zeolite is cesium-loaded zeolite, for example, CPT.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the waste-loaded zeolite is dehydrated at about 50-300° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the suitable glass-forming chemicals are added in appropriate amounts to achieve the target final glass composition.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the suitable glass-forming chemicals include or comprise about 15 parts (Na2O), about 5 parts (Al2O3), about 25 parts (B2O3) and about 55 (SiO2).

### Claim 6 (depends on 1)

The method according to claim 1 wherein the suitable glass forming chemicals include or comprise about 5-30 parts (Na2O), about 5-30 parts (Al2O3), about 15-40 parts (B2O3) and about 40-60 (SiO2) or 5-30 (Na2O)-5-30 (Al2O3)-15-40 (B2O3)-40-60 (SiO2).

### Claim 7 (depends on 1)

The method according to claim 1 wherein the suitable glass-forming chemicals include or comprise about 5-30 parts (Na2O), about 5-30 parts (Al2O3), about 15-40 parts (B2O3), about 1-10 parts of (P2O5) and about 40-60 (SiO2) or 5-30 (Na2O)-5-30 (Al2O3)-15-40 (B2O3)-40-60 (SiO2)-1-10 (P2O5).

### Claim 8 (depends on 1)

The method according to claim 1 wherein the waste-loaded zeolite glass is used as a starting material for the vitrification of intermediate- and high-level waste.