# US 2025/0376385 A1 · Perovskite powder, light emitting layer for light emitting device and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0376385 A1
- Document ID: US20250376385A1
- Status: Published application
- Kind: A1
- Application number: 19/228,648
- Filed: 2025-06-04
- Published: 2025-12-11
- Earliest claimed: 2024-06-05
- Assignees: Seoul National University R&Db Foundation
- Applicants: Seoul National University R&DB Foundation
- Inventors: Tae-Woo Lee; Jung-Min Heo; Chan-Yul Park; Joo Sung Kim
- Web page: https://patentgrep.com/patent/US20250376385A1

## CPC

- C01D 17/003: {Compounds of alkali metals}
- C09K 11/06: containing organic luminescent materials
- C09K 11/613: {with alkali or alkakine earth metals}
- C01P 2002/34: perovskite-type (ABO3)
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A perovskite powder, a light emitting layer for a light emitting device, a perovskite layered structure, an optoelectronic device including the same, and a method for manufacturing the same are provided. The perovskite powder is easy to control the crystal phase ratio in the light emitting layer and is not pyrolyzed during deposition. In addition, the light emitting layer for the light emitting device has an enhanced exciton confinement effect to have excellent light emission efficiency and the like. In addition, the method for manufacturing the light emitting layer for the light emitting device may control the ratio of crystal phases in the light emitting layer and is advantageous for large-area manufacturing. In addition, the perovskite layered structure maintains very high phase uniformity. Further, the optoelectronic device has excellent performance. Furthermore, the method for manufacturing the perovskite layered structure may manufacture a large-area and uniform perovskite thin film.

## Claims

### Claim 1

A perovskite powder having a CsBX3 structure with a crystallite size of 110 nm or less, wherein the powder has peaks at 14˜16°, 20˜22°, 30˜31°, 33˜35°, and 37˜38° without peaks at 11˜14° as 20 values in a XRD graph,
the B is a metal ion,
the X is F−, Cl−, Br−, I−, SCN−, OCN−, SeCN−, HCO2−, CH3COO−, CF3COO− or a combination thereof,
the crystallite size of the powder is measured by X-ray diffraction and then obtained using Scherrer equation (D=λ/β cos θ), and
in the Scherrer equation, D denotes a crystallite size, K denotes a shape coefficient, λ denotes an X-ray wavelength, β denotes a full width at half maximum (FWHM) of a maximum intensity peak, and θ denotes an X-ray incident angle.

### Claim 2 (depends on 1)

The perovskite powder of claim 1, wherein in the perovskite powder, perovskites having a CsBX3 structure are manufactured into powder by adding and reacting an aqueous solution of HX (H is hydrogen) in a solution dissolved with CsX and BX2 precursors.

### Claim 3 (depends on 1)

The perovskite powder of claim 1, wherein the B is a divalent transition metal ion, a rare earth metal ion, an alkaline earth metal ion, a monovalent metal ion, a trivalent metal ion, or a combination thereof.

### Claim 4 (depends on 2)

The perovskite powder of claim 2, wherein the molar ratio of the CsX and BX2 is 1.15:1 to 1.95:1.

### Claim 5 (depends on 2)

The perovskite powder of claim 2, wherein A′X is added and reacted in the solution,
wherein the A′ is a monovalent organic cation, a monovalent inorganic cation without Cs+ or a combination thereof, and
the X is F−, Cl−, Br−, I−, SCN−, OCN−, SeCN−, HCO2−, CH3COO−, CF3COO− or a combination thereof.

### Claim 6 (depends on 5)

The perovskite powder of claim 5, wherein the perovskite powder includes Cs1−aA′aBX3 crystals,
wherein the A′ is a monovalent organic cation, a monovalent inorganic cation without Cs+ or a combination thereof, and
the a is more than 0 and 0.9 or less.

### Claim 7 (depends on 1)

The perovskite powder of claim 1, wherein the powder has peaks at binding energy of 138 to 140 eV and 143 to 145 eV, without peaks at binding energy of 136 to 138 eV and 141 to 142 eV in the XPS graph.

### Claim 8

A method for manufacturing a light emitting layer for a light emitting device, the method comprising: manufacturing a light emitting layer for a light emitting device by using a perovskite powder containing Cs1−aA′aBX3 crystals as a single-source deposition source, performing vapor deposition by applying heat in a high vacuum state of 10-5 torr or less, and forming a thin film through the vapor deposition,
wherein the A′ is a monovalent organic cation, a monovalent inorganic cation without Cs+ or a combination thereof,
the B is a metal ion,
the X is F−, Cl−, Br−, I−, SCN−, OCN−, SeCN−, HCO2−, CH3COO−, CF3COO− or a combination thereof, and
the a is 0 to 0.9.

### Claim 9 (depends on 8)

The method of claim 8, wherein the deposition rate of single-source deposition source is 0.7 to 1.2 Å/s.

### Claim 10 (depends on 8)

The method of claim 8, wherein the deposition is co-depositing a compound containing cations having an ionic radius larger than the ionic radius of Cs in order to substitute part or all of the Cs.

### Claim 11 (depends on 10)

The method of claim 10, wherein the compound containing cations having the ionic radius larger than the ionic radius of Cs is an aromatic ammonium halide compound.

### Claim 12 (depends on 10)

The method of claim 10, wherein a deposition rate ratio of the single-source deposition source and the deposition source containing the compound in the co-deposition is 1:0.65 to 1:0.85.

### Claim 13

A light emitting layer for a light emitting device comprising:
Cs1−aA′aBX3 crystals and/or A″2(Cs1−aA′a)m−1BmX3m+1 crystals inside the light emitting layer,
wherein the A′ is a monovalent organic cation, a monovalent inorganic cation without Cs+ or a combination thereof,
the A″ is a cation having an ionic radius greater than the ionic radius of Cs for partially or fully substituting Cs,
the B is a metal ion,
the X is F−, Cl−, Br−, I−, SCN−, OCN−, SeCN−, HCO2−, CH3COO−, CF3COO− or a combination thereof,
the a is 0 to 0.9,
the m is an integer of 2 to 6, and
in an XPS graph of the light emitting layer, peaks are not shown at binding energy of 136 to 138 eV and 141 to 142 eV and peaks are shown at binding energy of 138 to 140 eV and 143 to 145 eV.

### Claim 14 (depends on 13)

The light emitting layer for the light emitting device of claim 13, wherein the Cs1-aA′aBX3 crystal is a 3D perovskite crystal, and the A″2(Cs1−aA′a)m−1BmX3m+1 crystal is a quasi-2D perovskite crystal.

### Claim 15 (depends on 13)

The light emitting layer for the light emitting device of claim 13, wherein a mean grain size of the Cs1−aA′aBX3 crystal and/or A″2(Cs1−aA′a)n−1BnX3n+1 crystal is 50 nm or less.