# US 2025/0376374 A1 · Method for producing lithium hydroxide, method for producing lithium- containing sulfide solid electrolyte raw material, and method for producing sulfide solid electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0376374 A1
- Document ID: US20250376374A1
- Status: Published application
- Kind: A1
- Application number: 19/311,117
- Filed: 2025-08-27
- Published: 2025-12-11
- Earliest claimed: 2023-03-01
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Ryota ANDO
- Web page: https://patentgrep.com/patent/US20250376374A1

## CPC

- C01B 17/22: Alkali metal sulfides or polysulfides
- C01B 17/28: with reducing gases
- C01D 15/02: Oxides; Hydroxides
- C01D 15/04: Halides
- H01B 1/10: sulfides
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- C01P 2006/40: Electric properties
- H01M 2300/0068: inorganic
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing lithium hydroxide includes: reacting lithium carbonate with calcium hydroxide in a liquid to obtain a solution containing lithium hydroxide; subjecting the solution to solid-liquid separation into a liquid component containing the lithium hydroxide and a solid component comprising lithium derived from the lithium carbonate; and recovering the lithium hydroxide from the liquid component.

## Claims

### Claim 1

A method for producing lithium hydroxide, comprising:
reacting lithium carbonate with calcium hydroxide in a liquid to obtain a solution comprising lithium hydroxide;
subjecting the solution to solid-liquid separation into a liquid component comprising the lithium hydroxide and a solid component comprising lithium derived from the lithium carbonate; and
recovering the lithium hydroxide from the liquid component.

### Claim 2 (depends on 1)

The method for producing lithium hydroxide according to claim 1, wherein an amount of water with respect to a total liquid in which the lithium carbonate and the calcium hydroxide are reacted is 70 mass % to 96 mass %.

### Claim 3 (depends on 1)

The method for producing lithium hydroxide according to claim 1, wherein a blending ratio of the calcium hydroxide to the lithium carbonate (calcium hydroxide/lithium carbonate) is 0.2 to 1.1 on a molar basis.

### Claim 4 (depends on 1)

The method for producing lithium hydroxide according to claim 1, wherein a temperature of the liquid when the lithium carbonate and the calcium hydroxide are reacted is 10° C. to 95° C.

### Claim 5 (depends on 1)

A method for producing lithium sulfide, comprising reacting the lithium hydroxide obtained by the production method according to claim 1 with hydrogen sulfide to produce lithium sulfide.

### Claim 6 (depends on 5)

A method for producing a sulfide solid electrolyte, wherein the lithium sulfide obtained by the production method according to claim 5 is used as a raw material.

### Claim 7

A method for producing a sulfide solid electrolyte raw material comprising lithium, comprising:
reacting lithium carbonate with calcium hydroxide in a liquid to obtain a solution comprising lithium hydroxide;
subjecting the solution to solid-liquid separation into a liquid component comprising the lithium hydroxide and a solid component comprising lithium derived from the lithium carbonate; and
removing calcium in the solid component to obtain a sulfide solid electrolyte raw material comprising lithium from the solid component.

### Claim 8 (depends on 7)

The method for producing a sulfide solid electrolyte raw material comprising lithium according to claim 7, wherein the calcium in the solid component is removed by adding sulfate ions to the solid component.

### Claim 9 (depends on 7)

The method for producing a sulfide solid electrolyte raw material comprising lithium according to claim 7, wherein the sulfide solid electrolyte raw material comprising lithium is a lithium halide or lithium sulfate.

### Claim 10 (depends on 7)

A method for producing a sulfide solid electrolyte, comprising using the sulfide solid electrolyte raw material comprising lithium obtained by the production method according to claim 7.

### Claim 11

A method for producing lithium hydroxide and a sulfide solid electrolyte raw material comprising lithium, comprising:
reacting lithium carbonate with calcium hydroxide in a liquid to obtain a solution comprising lithium hydroxide;
subjecting the solution to solid-liquid separation into a liquid component comprising the lithium hydroxide and a solid component comprising lithium derived from the lithium carbonate;
recovering the lithium hydroxide from the liquid component; and
removing calcium in the solid component to obtain a sulfide solid electrolyte raw material comprising lithium from the solid component.

### Claim 12 (depends on 11)

A method for producing a sulfide solid electrolyte, wherein lithium sulfide obtained by reacting the lithium hydroxide obtained by the production method according to claim 11 with hydrogen sulfide and the sulfide solid electrolyte raw material comprising lithium obtained by the production method according to claim 11 are used as raw materials.

### Claim 13

A lithium hydroxide-containing composition for synthesizing a sulfide solid electrolyte, comprising lithium hydroxide and zinc.

### Claim 14 (depends on 13)

The lithium hydroxide-containing composition for synthesizing a sulfide solid electrolyte according to claim 13, further comprising aluminum.

### Claim 15 (depends on 14)

The lithium hydroxide-containing composition for synthesizing a sulfide solid electrolyte according to claim 14, wherein a sum of a zinc concentration and an aluminum concentration is 10 ppm by mass or more.

### Claim 16 (depends on 13)

The lithium hydroxide-containing composition for synthesizing a sulfide solid electrolyte according to claim 13, further comprising 10 ppm by mass or more of calcium.

### Claim 17

A lithium sulfide-containing composition for synthesizing a sulfide solid electrolyte, comprising lithium sulfide and zinc.

### Claim 18 (depends on 17)

The lithium sulfide-containing composition for synthesizing a sulfide solid electrolyte according to claim 17, further comprising aluminum.

### Claim 19 (depends on 18)

The lithium sulfide-containing composition for synthesizing a sulfide solid electrolyte according to claim 18, wherein a sum of a zinc concentration and an aluminum concentration is 10 ppm by mass or more.

### Claim 20 (depends on 17)

The lithium sulfide-containing composition for synthesizing a sulfide solid electrolyte according to claim 17, further comprising 10 ppm by mass or more of calcium.

### Claim 21

A lithium halide-containing composition for synthesizing a sulfide solid electrolyte, comprising a lithium halide and at least one of sulfate ions, phosphate ions, and fluorine ions, wherein a concentration of the ions is 10 mass % or less.