# US 2025/0375825 A1 · Golf Club Head With Miter Joint For Brazing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0375825 A1
- Document ID: US20250375825A1
- Status: Published application
- Kind: A1
- Application number: 18/913,774
- Filed: 2024-10-11
- Published: 2025-12-11
- Earliest claimed: 2022-07-19
- Assignees: Topgolf Callaway Brands Corp.
- Applicants: Topgolf Callaway Brands Corp.
- Inventors: Eric Itokazu; Alex Power; Patrick Davis; Matthew Myers
- Web page: https://patentgrep.com/patent/US20250375825A1

## CPC

- A63B 53/042: {the face insert consisting of a material different from that of the head}
- A63B 53/047: {iron-type}
- B23K 1/0008: {specially adapted for particular articles or work}
- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- A63B 2209/00: Characteristics of used materials
- B23K 35/302: {Cu as the principal constituent}
- B23K 35/3033: {Ni as the principal constituent}
- B23K 2103/24: Ferrous alloys and titanium or alloys thereof
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A golf club head with a mitered joint for joining components of dissimilar materials is disclosed herein. The golf club head has a body with an internal edge defining a recess, and a face component having an internal edge. The face component is disposed over the recess. The internal edge of the body and the internal edge of the face have an angle ranging from about 10 degrees to about 80 degrees.

## Claims

### Claim 1

A method for joining iron-type golf club head components, the method comprising:
applying a copper-based filler material to a first attachment surface of an iron-type body to create a copper-based filler material attachment surface of the iron-type body, the iron-type body having an internal edge defining a recess, the first attachment surface formed continuously around an entire perimeter portion of the iron-type body, wherein the iron-type body is consisting essentially of a steel material;
positioning a second attachment surface of a single material face component over the copper-based filler material attachment surface of the iron-type body, the face component disposed over the recess, wherein the face component is consisting essentially of a titanium alloy material; and
performing at least one brazing cycle within a vacuum brazing furnace to braze the face component to the iron-type body, wherein the at least one brazing cycle comprises reaching a maximum vacuum level within the vacuum brazing furnace, increasing a temperature within the vacuum brazing furnace to a maximum temperature while at the maximum vacuum level, dropping the temperature to a minimum temperature while reducing the vacuum level;
wherein a miter joint is formed between the second attachment surface of the face component and the first attachment surface of the iron-type body and has an angle ranging from 10 degrees to 80 degrees relative to a plane of a rear surface of the face component, wherein the second attachment surface of the face component is formed continuously around an entire circumference of the rear surface of the face component, and wherein the second attachment surface of the face component has a width ranging from 0.04 inch to 0.5 inch and wherein the first attachment surface of the iron-type body has a width substantially matching the width of the second attachment surface of the face component.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the copper-based filler is selected from the group consisting of copper and a copper alloy consisting essentially of copper, manganese and nickel.

### Claim 3 (depends on 1)

The method according to claim 1 wherein the maximum vacuum level ranges from 10−2 Torr to 10−7 Torr, and the maximum temperature ranges from 1400° F. to 1800° F.

### Claim 4 (depends on 1)

The method according to claim 1 wherein the at least one brazing cycle has a time period ranging from 200 to 300 minutes.

### Claim 5 (depends on 1)

The method according to claim 1 wherein the at least one brazing cycle comprises creating a reducing environment within the vacuum brazing furnace.

### Claim 6 (depends on 1)

The method according to claim 1 wherein the steel material is selected from the group consisting of C300 maraging steel, 1020 steel, 1025 steel, 1045 steel, 4130 steel, 4140 steel, and 4340 steel, 17-4 stainless steel, 304 stainless steel, 304L stainless steel, 321 stainless steel, 303 stainless steel, 316 stainless steel, 316L stainless steel, 420 stainless steel, 425 stainless steel, 425M stainless steel, 450 stainless steel, 455 stainless steel, 475 stainless steel, and HSR300 stainless steel.

### Claim 7 (depends on 1)

The method according to claim 1 wherein the titanium alloy material is selected from the group consisting of 6-4 titanium, 811 titanium, FS2S titanium, FS2S+ titanium, SP700 titanium, Ti 17, Ti 21, and 15-3-3-3 titanium.

### Claim 8 (depends on 1)

The method according to claim 1 wherein the angle of the miter joint ranges from 25 degrees to 65 degrees relative to a plane of a rear surface of the face component.

### Claim 9 (depends on 1)

The method according to claim 1 wherein the angle of the miter joint ranges from 30 degrees to 60 degrees relative to a plane of a rear surface of the face component.

### Claim 10 (depends on 1)

The method according to claim 1 wherein an iron-type golf club head formed from the iron-type golf club head components has a loft angle ranging from 15 degrees to 34 degrees.

### Claim 11 (depends on 1)

The method according to claim 1 wherein the face component comprises a return portion.

### Claim 12

A method for joining iron-type golf club head components, the method comprising:
applying a copper-based filler material to a first attachment surface of an iron-type body to create a copper-based filler material attachment surface of the iron-type body, the iron-type body having an internal edge defining a recess, the first attachment surface formed continuously around an entire perimeter portion of the iron-type body, wherein the iron-type body is consisting essentially of a steel material, wherein the first attachment surface comprises a first section, a second section and at least one transition section;
positioning a second attachment surface of a single material face component over the copper-based filler material attachment surface of the iron-type body, the face component disposed over the recess, wherein the face component is consisting essentially of a titanium alloy material, wherein the second attachment surface comprises a first section, a second section and at least one transition section corresponding to the first section, the second section and the at least one transition section of the first attachment surface; and
performing at least one brazing cycle within a vacuum brazing furnace to braze the face component to the iron-type body, wherein the at least one brazing cycle comprises reaching a maximum vacuum level within the vacuum brazing furnace, increasing a temperature within the vacuum brazing furnace to a maximum temperature while at the maximum vacuum level, dropping the temperature to a minimum temperature while reducing the vacuum level;
wherein a miter joint is formed between the second attachment surface of the face insert and the first attachment surface of the iron-type body and has a first angle ranging from 10 degrees to 80 degrees relative to a plane of a rear surface of the face insert, wherein the first angle of the first section of the first attachment surface and the first section of the second attachment surface is greater than a second angle of the second section of the first attachment surface and the second section of the second attachment surface, and wherein the at least one transition section has a third angle with a value between the first angle and the second angle.

### Claim 13 (depends on 12)

The method according to claim 12 wherein the copper-based filler is selected from the group consisting of copper and a copper alloy consisting essentially of copper, manganese and nickel.

### Claim 14 (depends on 12)

The method according to claim 12 wherein the maximum vacuum level ranges from 10−2 Torr to 10−7 Torr, and the maximum temperature ranges from 1400° F. to 1800° F.

### Claim 15 (depends on 12)

The method according to claim 12 wherein the at least one brazing cycle has a time period ranging from 200 to 300 minutes.

### Claim 16 (depends on 12)

The method according to claim 12 wherein the at least one brazing cycle comprises creating a reducing environment within the vacuum brazing furnace.

### Claim 17 (depends on 12)

The method according to claim 12 wherein the steel material is selected from the group consisting of C300 maraging steel, 1020 steel, 1025 steel, 1045 steel, 4130 steel, 4140 steel, and 4340 steel, 17-4 stainless steel, 304 stainless steel, 304L stainless steel, 321 stainless steel, 303 stainless steel, 316 stainless steel, 316L stainless steel, 420 stainless steel, 425 stainless steel, 425M stainless steel, 450 stainless steel, 455 stainless steel, 475 stainless steel, and HSR300 stainless steel.

### Claim 18 (depends on 12)

The method according to claim 12 wherein the titanium alloy material is selected from the group consisting of 6-4 titanium, 811 titanium, FS2S titanium, FS2S+ titanium, SP700 titanium, Ti 17, Ti 21, and 15-3-3-3 titanium.

### Claim 19 (depends on 12)

The method according to claim 12 wherein the angle of the miter joint ranges from 25 degrees to 65 degrees relative to a plane of a rear surface of the face component.

### Claim 20 (depends on 12)

The method according to claim 12 wherein an iron-type golf club head formed from the iron-type golf club head components has a loft angle ranging from 15 degrees to 34 degrees.