# US 2025/0375757 A1 · Superabsorbent polymer and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0375757 A1
- Document ID: US20250375757A1
- Status: Published application
- Kind: A1
- Application number: 18/798,330
- Filed: 2024-08-08
- Published: 2025-12-11
- Earliest claimed: 2024-06-07
- Assignees: Formosa Plastics Corporation
- Applicants: Formosa Plastics Corporation
- Inventors: Yan-Syun CIOU; Feng-Yi CHEN; Zhong-Yi CHEN
- Web page: https://patentgrep.com/patent/US20250375757A1

## CPC

- B01J 20/28016: {Particle form}
- C08J 3/245: {Differential crosslinking of one polymer with one crosslinking type, e.g. surface crosslinking}
- A61L 15/60: Liquid-swellable gel-forming materials, e.g. super-absorbents
- B01J 20/24: Naturally occurring macromolecular compounds, e.g. humic acids or their derivatives
- B01J 20/261: {obtained by reactions only involving carbon to carbon unsaturated bonds (macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds per se C08F)}
- B01J 20/267: {Cross-linked polymers}
- B01J 20/28011: {Other properties, e.g. density, crush strength}
- B01J 20/3021: {Milling, crushing or grinding}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3208: {Polymeric carriers, supports or substrates}
- B01J 20/3274: {Proteins, nucleic acids, polysaccharides, antibodies or antigens}
- B01J 20/3295: {Coatings made of particles, nanoparticles, fibers, nanofibers}
- C08J 3/126: {Polymer particles coated by polymer, e.g. core shell structures}
- B01J 2220/4825: Polysaccharides or cellulose materials, e.g. starch, chitin, sawdust, wood, straw, cotton
- B01J 2220/68: Superabsorbents
- C08J 2301/02: Cellulose; Modified cellulose
- C08J 2333/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

The present invention relates to a superabsorbent polymer and a method of making the same. The superabsorbent polymer includes a cross-linking core structure and a shell layer. The shell layer encloses the cross-linking core structure completely, and the shell layer includes microcrystalline cellulose. The superabsorbent polymer has not only good absorption properties but also excellent absorption rate as well as permeability, and can be applied to thinner hygiene products.

## Claims

### Claim 1

A superabsorbent polymer, comprising:
a cross-linking core structure, obtained by subjecting an aqueous solution of acid group-containing monomers, a crosslinking agent, and a polymerization initiator to a free radical polymerization step; and
a shell layer, enclosing the cross-linking core structure, wherein the shell layer is formed by performing a surface-treating step on the cross-linking core structure with a surface-treating agent, the surface-treating agent comprising microcrystalline cellulose, and based on the cross-linking core structure as 100 weight percent, a usage amount of the microcrystalline cellulose is 0.1 weight percent to 5.0 weight percent.

### Claim 2 (depends on 1)

The superabsorbent polymer according to claim 1, wherein based on a total solid content of the superabsorbent polymer as 100 weight percent, a usage amount of the crosslinking agent is 0.001 weight percent to 5 weight percent.

### Claim 3 (depends on 1)

The superabsorbent polymer according to claim 1, wherein the polymerization initiator comprises a thermal decomposition initiator and/or a redox initiator.

### Claim 4 (depends on 1)

The superabsorbent polymer according to claim 1, wherein based on a total solid content of the superabsorbent polymer as 100 weight percent, a usage amount of the surface-treating agent is 0.001 weight percent to 10 weight percent.

### Claim 5 (depends on 1)

The superabsorbent polymer according to claim 1, wherein a particle size of the microcrystalline cellulose is 20 μm to 100 μm.

### Claim 6 (depends on 1)

The superabsorbent polymer according to claim 1, wherein a bulk density of the microcrystalline cellulose is 0.25 to 0.35.

### Claim 7 (depends on 1)

The superabsorbent polymer according to claim 1, wherein a moisture content of the microcrystalline cellulose is smaller than or equal to 7%.

### Claim 8 (depends on 1)

The superabsorbent polymer according to claim 1, wherein a degree of polymerization of the microcrystalline cellulose is smaller than or equal to 350.

### Claim 9

A method of making a superabsorbent polymer, comprising:
performing a free radical polymerization step on a superabsorbent polymer composition, so as to form a cross-linking core structure, wherein the superabsorbent polymer composition comprises:
a aqueous solution of acid group-containing monomers;
a crosslinking agent; and
a polymerization initiator, comprising a thermal decomposition initiator and/or a redox initiator; and
performing a surface-treating step on the cross-linking core structure with a surface-treating agent, so as to form a shell layer on the cross-linking core structure, wherein the shell layer encloses the cross-linking core structure completely, the surface-treating agent comprises microcrystalline cellulose, and based on the cross-linking core structure of the superabsorbent polymer is 100 weight percent, an usage amount of the microcrystalline cellulose is 0.1 weight percent to 5.0 weight percent, thereby obtaining the superabsorbent polymer.

### Claim 10 (depends on 9)

The method according to claim 9, wherein a particle size of the microcrystalline cellulose is 20 μm to 100 μm.

### Claim 11 (depends on 9)

The method according to claim 9, wherein a bulk density of the microcrystalline cellulose is 0.25 to 0.35.

### Claim 12 (depends on 9)

The method according to claim 9, wherein a moisture content of the microcrystalline cellulose is smaller than or equal to 7%.

### Claim 13 (depends on 9)

The method according to claim 9, wherein a degree of polymerization of the microcrystalline cellulose is smaller than or equal to 350.

### Claim 14 (depends on 9)

The method according to claim 9, further comprising a neutralizing step performed on the aqueous solution of acid group-containing monomers before the free radical polymerization step.

### Claim 15 (depends on 9)

The method according to claim 9, further comprising performing a drying step and/or a pulverizing step on the cross-linking core structure before the surface-treating step, so as to obtained a powder of the cross-linking core structure.