# US 2025/0369062 A1 · Method for reducing content of mns inclusions in steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0369062 A1
- Document ID: US20250369062A1
- Status: Published application
- Kind: A1
- Application number: 18/976,509
- Filed: 2024-12-11
- Published: 2025-12-04
- Earliest claimed: 2024-06-03
- Assignees: Henglilai New Materials Limited; Tianrun Industry Technology Co., Ltd.
- Applicants: Henglilai New Materials Limited; Tianrun Industry Technology Co., Ltd.
- Inventors: Jianchen CONG; Yufang Wang; Jing Wang; Dong Lin; Yangfan Zhou; Shibo Shao
- Web page: https://patentgrep.com/patent/US20250369062A1

## CPC

- C21C 7/0006: {Adding metallic additives}
- C21C 7/06: Deoxidising, e.g. killing
- C21C 7/064: Dephosphorising; Desulfurising
- C21C 7/0645: {Agents used for dephosphorising or desulfurising}
- C21C 7/072: Treatment with gases (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C21C 7/10: Handling in a vacuum
- Y02P 10/20: Recycling
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention provides a method for reducing content of MnS inclusions in steel, including: (1) placing raw materials of other elements than manganese in a smelting furnace according to components of steel to perform smelting to obtain liquid steel; (2) first adding a first rare earth element and sulfur to the liquid steel, to form rare earth sulphide, then adding a raw material containing manganese to perform smelting, performing tapping after smelting is completed, and performing pouring and cooling to obtain a cast ingot. A rare earth element and sulfur are first added to liquid steel before manganese is added to generate tiny, round rare earth sulphide, and subsequently manganese is added to make it difficult to generate MnS, so that MnS and rare earth/manganese/sulfur composite inclusions are reduced, and content of MnS inclusions at a parting plane of a workpiece is reduced, thereby improving the reliability of the workpiece.

## Claims

### Claim 1

A method for reducing content of MnS inclusions in steel, comprising steps of:
(1) placing raw materials of other elements than manganese in a smelting furnace according to components of steel to perform smelting to obtain liquid steel; and
(2) first adding a first rare earth element and sulfur to the liquid steel, to form rare earth sulphide, then adding a raw material containing manganese to perform smelting, performing tapping after smelting is completed, and performing pouring and cooling to obtain a cast ingot.

### Claim 2 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (1), the smelting furnace is a vacuum smelting furnace, and the smelting is performed in an argon atmosphere.

### Claim 3 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (1), a designation of the steel is 40Cr, 35CrMo, 42CrMo, 40CrNiMo, 50CrMo, 48MnV, C38, C38N2, 38MnVS6 or S38MnSiV.

### Claim 4 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (2), a mass ratio of the first rare earth element to the sulfur added to the liquid steel is 1:0.2 to 1:0.4.

### Claim 5 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (2), the first rare earth element is cerium and/or lanthanum.

### Claim 6 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (2), an addition amount of the sulfur accounts for 0.02 wt % to 0.05 wt % of the steel.

### Claim 7 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (2), before adding a first rare earth element and sulfur to the liquid steel the method further comprises performing drossing treatment on the liquid steel.

### Claim 8 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein in Step (2), a second rare earth element is added to the liquid steel before the tapping, and an addition amount of the second rare earth element accounts for 0.01 wt % to 0.03 wt % of the steel.

### Claim 9 (depends on 8)

The method for reducing content of MnS inclusions in steel according to claim 8, wherein the second rare earth element is cerium and/or lanthanum.

### Claim 10 (depends on 1)

The method for reducing content of MnS inclusions in steel according to claim 1, wherein an amount of the rare earth sulphide particles in the cast ingot accounts for more than 85% of a total quantity of inclusions.