# US 2025/0368787 A1 · Polylactide-peroxide masterbatches and branching process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0368787 A1
- Document ID: US20250368787A1
- Status: Published application
- Kind: A1
- Application number: 19/222,482
- Filed: 2025-05-29
- Published: 2025-12-04
- Earliest claimed: 2024-05-31
- Applicants: NatureWorks LLC
- Inventors: Adegbola Adenusi; Marc Flodquist; Nemat Hossieny; Jed Richard Randall
- Web page: https://patentgrep.com/patent/US20250368787A1

## CPC

- C08J 3/22: using masterbatch techniques
- C08J 3/226: {using a polymer as a carrier}
- C08J 3/247: {Heating methods}
- C08K 5/14: Peroxides
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08J 2367/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2367/06 takes precedence)
- C08J 2467/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2467/06 takes precedence)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Solidified polylactide-peroxide masterbatches contain at least 50% of a linear amorphous grade polylactide resin and 1 to 30 parts, per 100 parts by weight of the polylactide, of a peroxide having a half-life of at least 50 seconds at 180° C. The masterbatches are made by combining the polylactide resin and peroxide at a temperature of 80 to 170° C. and then cooling the resulting mixture. The masterbatch is useful for preparing branched and/or crosslinked polylactides.

## Claims

### Claim 1

A solidified polylactide-peroxide masterbatch comprising a thermoplastic resin phase comprising at least 50% by weight of a linear amorphous grade polylactide resin based on the weight of the thermoplastic resin phase and 1 to 30 parts by weight per 100 parts by weight of the thermoplastic resin phase of a peroxide, the peroxide having a half-life of at least 50 seconds at 180° C. dissolved or dispersed in the thermoplastic resin phase.

### Claim 2 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 which is non-porous.

### Claim 3 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 wherein the linear amorphous grade polylactide resin contains 40 to 60 weight percent L-lactic units and correspondingly 60 to 40 weight percent D-lactic units, based on the weight of the lactic units of the solidified linear amorphous grade polylactide resin.

### Claim 4 (depends on 3)

The solidified polylactide-peroxide masterbatch of claim 3 wherein the linear amorphous grade polylactide resin contains 20 to 80 weight percent L-lactic units and correspondingly 80 to 20 weight percent D-lactic units, based on the weight of the lactic units of the solidified linear amorphous grade polylactide resin.

### Claim 5 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 wherein the linear amorphous grade polylactide resin contains greater than 80% and at most 90% L-lactic units and correspondingly less than 20% and at least 10% D-lactic units or greater than 80% and at most 90% D-lactic units and correspondingly less than 20% and at least 10% L-lactic units, based on the weight of lactic units in the random copolymer.

### Claim 6 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 wherein the peroxide is a cyclic peroxide having any of the structures I-III:
wherein each of R1-R6 are independently selected from the group consisting of hydrogen, C1-20 alkyl, C3-20 cycloalkyl, C6-20 aryl, C7-20 aralkyl and C7-20 alkaryl, any of which may optionally be substituted with one or more groups selected from hydroxyl, alkoxy, linear or branched alkyl, aryloxy, ester, carboxy, nitrile and amido.

### Claim 7 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 wherein the peroxide is a cyclic peroxide having the structure:
wherein R7, R8 and R9 are independently hydrogen or hydrocarbyl that may be substituted with one or more groups selected from hydroxyl, alkoxy, linear or branched alkyl, aryloxy, ester, carboxy, nitrile and amido and provided that any two of R7, R8 and R9 may together form a divalent moiety that forms a ring structure with the intervening atoms of the trioxepane ring.

### Claim 8 (depends on 1)

The solidified polylactide-peroxide masterbatch of claim 1 wherein the peroxide includes one or more of di-t-amyl peroxide, 3,6,9-triethyl-3,6,9-trimethyl-1,4,7-triperoxanone, 3,3,5,7,7-pentamethyl-1,2,4-trioxepane and 3-ethyl-3,5,7,7-tetramethyl-1,2,4-trioxepane.

### Claim 9

A method for making a solidified polylactide-peroxide masterbatch, comprising the steps of
i) combining a) one or more thermoplastic resins, the thermoplastic resins comprising at least 50% by weight of a starting linear amorphous grade polylactide resin with b) 1 to 30 parts by weight, per 100 parts by weight of the starting amorphous grade PL(Original) A resin, of a peroxide, the peroxide having a half-life of at least 50 seconds at 180° C. and mixing the starting linear amorphous grade polylactide and the peroxide at a temperature of 80 to 170° C. to produce a solution or dispersion of the one or more peroxides in the thermoplastic resins, and
ii) cooling the solution or dispersion to a temperature of at most 40° C. to produce the solidified polylactide-peroxide masterbatch.

### Claim 10 (depends on 9)

The method of claim 9 where step i) is performed in the absence of a blowing agent to produce a non-porous polylactide-peroxide masterbatch.

### Claim 11 (depends on 9)

The method of claim 9 wherein the temperature is 80 to 160° C.

### Claim 12 (depends on 9)

The method of claim 9 wherein the starting linear amorphous grade polylactide resin contains 20 to 80 weight percent L-lactic units and correspondingly 80 to 20 weight percent D-lactic units, based on the weight of the lactic units of the starting linear amorphous grade polylactide resin and the temperature is 80 to 130° C.

### Claim 13 (depends on 9)

The method of claim 9 wherein the peroxide is a cyclic peroxide having any of the structures I-III:
wherein each of R1-R6 are independently selected from the group consisting of hydrogen, C1-20 alkyl, C3-20 cycloalkyl, C6-20 aryl, C7-20 aralkyl and C7-20 alkaryl, any of which may optionally be substituted with one or more groups selected from hydroxyl, alkoxy, linear or branched alkyl, aryloxy, ester, carboxy, nitrile and amido.

### Claim 14 (depends on 9)

The method of any of claim 9 wherein the peroxide is a cyclic peroxide having the structure:
wherein R7, R8 and R9 are independently hydrogen or hydrocarbyl that may be substituted with one or more groups selected from hydroxyl, alkoxy, linear or branched alkyl, aryloxy, ester, carboxy, nitrile and amido and provided that any two of R7, R8 and R9 may together form a divalent moiety that forms a ring structure with the intervening atoms of the trioxepane ring.

### Claim 15 (depends on 9)

The method of claim 9 wherein the peroxide includes one or more of di-t-amyl peroxide, 3,6,9-triethyl-3,6,9-trimethyl-1,4, 7-triperoxanone, 3,3,5, 7,7-pentamethyl-1,2,4-trioxepane and 3-ethyl-3,5,7,7-tetramethyl-1,2,4-trioxepane.

### Claim 16 (depends on 1)

A method for branching and/or crosslinking polylactide, comprising the steps of
I. combining the solidified polylactide-peroxide masterbatch of claim 1 with additional linear polylactide resin to produce a reactive mixture containing 0.01 to 0.5 weight percent of the peroxide and polylactides comprising the starting linear amorphous grade polylactide resin and the additional linear polylactide resin; and
II. heating the reactive mixture obtained in step I to a temperature of at least 180° C. to heat-soften the polylactides, decompose the peroxide and branch and/or crosslink at least a portion of the polylactides.

### Claim 17 (depends on 16)

The method of claim 16 wherein step II is performed in the presence of 0.05 to 1.5 weight percent, based on the weight of the polylactides, of at least one polyene compound having 2 to 6 vinyl groups and an equivalent weight per vinyl group of up to 500.

### Claim 18 (depends on 16)

The method of claim 16 wherein the additional linear polylactide resin is an amorphous grade.

### Claim 19 (depends on 16)

The method of claim 16 wherein the additional linear polylactide resin is a semi-crystalline grade.