# US 2025/0367759 A1 · Laser process to enhance the wire bonding process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0367759 A1
- Document ID: US20250367759A1
- Status: Published application
- Kind: A1
- Application number: 19/219,511
- Filed: 2025-05-27
- Published: 2025-12-04
- Earliest claimed: 2024-06-04
- Assignees: Turning Point Lasers Corporation
- Applicants: Turning Point Lasers Corporation.
- Inventors: Szutsun Simon Ou; Hung Sheng Lee; Chi Luen Wang; Han Wei Chang; Chung Cheng Lin
- Web page: https://patentgrep.com/patent/US20250367759A1

## CPC

- B23K 26/21: by welding
- B23K 26/354: by melting
- B23K 26/60: Preliminary treatment
- B23K 2103/12: Copper or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A laser process to enhance the wire bonding process, using before wire bonding, the laser process of the present invention uses a laser processing system to clean the surface oxide where the wire and the substrate are to be joint, then locally heated the substrate, then form a molten pool at the joint position, then uses the wire bonding to join the wire and the substrate. Laser cleaning of the substrate surface can reduce impurities at the bonding interface, and local heating to form the molten pool can make the metal easier to melt, thus reducing the resistance value after bonding and improving

## Claims

### Claim 1

A laser process to enhance the wire bonding process, the process steps comprising:
a). Provide a laser processing system with a laser source;
b). Provide a wire;
c). Before wire bonding, use the laser processing system to clean the surface where the wire and a substrate are to be joined;
d). Use the laser processing system, the laser source uses a blue laser with a laser source wavelength range of 400 nm to 500 nm, to form a molten pool at the joint position, the blue laser includes using 200 to 300 watts (W) of energy to locally heat the substrate for 2 to 3 milliseconds (ms), the molten pool is a circular concave arc with a maximum diameter of 330 μm to 360 μm and a maximum depth of 67 μm to 77 μm; and
e). Finally, wire bonding is used to bond the wire to the substrate, so the wire is fused with the substrate, and after joining, the wire is higher than the substrate to form a ball, so that a joint end of the wire is completely covered in the molten pool.

### Claim 2 (depends on 1)

The laser process to enhance the wire bonding process as claimed in claim 1, wherein the laser source of laser processing system in step a). includes a fiber laser and a free space laser.

### Claim 3 (depends on 1)

The laser process to enhance the wire bonding process as claimed in claim 1, wherein the wire in step b). includes a copper wire.

### Claim 4 (depends on 1)

The laser process to enhance the wire bonding process as claimed in claim 1, wherein the laser source of the laser processing system in step c). used for surface cleaning of the substrate includes a wavelength range 300 nm˜1100 nm.