# US 2025/0367633 A1 · COMPOSITIONS AND METHODS FOR POLYMER-MODIFIED LITHIUM/ALUMINUM LAYERED DOUBLE HYDROXIDE (Li/Al-LDH)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0367633 A1
- Document ID: US20250367633A1
- Status: Published application
- Kind: A1
- Application number: 19/220,546
- Filed: 2025-05-28
- Published: 2025-12-04
- Earliest claimed: 2024-05-31
- Applicants: Virginia Tech Intellectual Properties, Inc.
- Inventors: Wencai Zhang; Yanan Pan
- Web page: https://patentgrep.com/patent/US20250367633A1

## CPC

- B01J 20/08: comprising aluminium oxide or hydroxide; comprising bauxite
- B01J 20/041: {Oxides or hydroxides}
- B01J 20/06: comprising oxides or hydroxides of metals not provided for in group B01J20/04
- B01J 20/261: {obtained by reactions only involving carbon to carbon unsaturated bonds (macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds per se C08F)}
- B01J 20/262: {obtained otherwise than by reactions only involving carbon to carbon unsaturated bonds, e.g. obtained by polycondensation (macromolecular compounds obtained otherwise than by reactions only involving unsaturated carbon-to-carbon bonds per se C08G)}
- B01J 20/3204: {Inorganic carriers, supports or substrates}
- B01J 20/327: {Polymers obtained by reactions involving only carbon to carbon unsaturated bonds}
- B01J 20/3272: {Polymers obtained by reactions otherwise than involving only carbon to carbon unsaturated bonds}
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 26/12: Obtaining lithium
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

The present disclosure pertains to methods for enhancing the properties of conventional Li/Al-LDH by integrating polymers to provide compositions comprising a Li/Al-LDH material and a polymer. The present disclosure further pertains to methods of using such polymer-modified-LDH to improve lithium adsorption and extraction performance. The disclosed methods can comprise incorporating the polymer during the precipitation reaction or by mixing the Li/Al-LDH product with a polymer solution under specific conditions. During the lithium extraction process, the disclosed compositions comprising a Li/Al-LDH material and a polymer can be used as an excellent lithium adsorbent to capture lithium ions from low-concentration lithium resources due to its improved physicochemical properties. The disclosed compositions comprising a Li/Al-LDH material and a polymer provides compositions for lithium extraction from low concentration resources, as well as expands the scope of lithium adsorbent material development.

## Claims

### Claim 1

A composition comprising:
a Li/Al-LDH substrate; and
a polymer attached to the Li/Al-LDH substrate;
wherein the composition has improved affinity for extraction of lithium from a lithium-containing source material.

### Claim 2 (depends on 1)

The composition in claim 1, wherein the polymer is selected from a polyethylene glycol (PEG), a polyacrylic acid (PAA), a polyacrylonitrile (PAN), a polylactic acid (PLA), a polyvinyl chloride (PVC), a polypropylene (PP), a poly (ethylene terephthalate) (PET), a polystyrene (PS), and combinations thereof.

### Claim 3 (depends on 2)

The composition in claim 2, wherein the polymer is selected from polyethylene glycol (PEG), polyacrylic acid (PAA), polyacrylonitrile (PAN), and combinations thereof.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the polymer has a weight average molecular weight (Mw) less than about 10,000 Da.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the polymer is a block copolymer comprising two or more blocks; and wherein each block is independently selected from a polymer block comprising a polyethylene glycol (PEG), a polyacrylic acid (PAA), a polyacrylonitrile (PAN), a polylactic acid (PLA), a polyvinyl chloride (PVC), a polypropylene (PP), a poly (ethylene terephthalate) (PET), a polystyrene (PS), and combinations thereof.

### Claim 6 (depends on 5)

The composition of claim 5, wherein the polymer comprises a first polymer block and a second polymer block.

### Claim 7 (depends on 6)

The composition of claim 6, wherein the first polymer block and the second polymer block each comprise different polymer blocks.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the polymer is a gradient copolymer comprising; wherein the gradient on a gradient from a first gradient polymer comprising a polyethylene glycol (PEG), a polyacrylic acid (PAA), a polyacrylonitrile (PAN), a polylactic acid (PLA), a polyvinyl chloride (PVC), a polypropylene (PP), a poly (ethylene terephthalate) (PET), a polystyrene (PS), and combinations thereof, and a second gradient polymer comprising a polyethylene glycol (PEG), a polyacrylic acid (PAA), a polyacrylonitrile (PAN), a polylactic acid (PLA), a polyvinyl chloride (PVC), a polypropylene (PP), a poly (ethylene terephthalate) (PET), a polystyrene (PS), and combinations thereof; and wherein the gradient is a relatively higher concentration of the first gradient polymer at a first terminus of the gradient copolymer to a lower concentration of the first gradient polymer at a second terminus of the gradient polymer distal to the first terminus.

### Claim 9 (depends on 1)

The composition of claim 1, wherein a weight ratio of the polymer to the Li/Al-LDH substrate is about 0.1:1 to about 100:1.

### Claim 10

A method for preparing a composition comprising a Li/Al-LDH substrate and a polymer, the method comprising the steps:
(a) providing a lithium and aluminum salt solution comprising the Li/Al-LDH substrate and a polymer solution comprising a polymer;
(b) pumping the lithium and aluminum salt solution and the polymer solution into an alkali solution within a container, thereby forming a slurry;
(c) allowing the lithium and aluminum salt solution and the polymer solution to be in contact with each other in the slurry at a temperature and for a time suitable for completion of formation of the composition comprising a Li/Al-LDH substrate and a polymer;
(d) washing the slurry with deionized water; and
(e) drying the slurry forming a powder product comprising the composition comprising a Li/Al-LDH substrate and a polymer;
thereby forming the composition comprising a Li/Al-LDH substrate and a polymer,
wherein the composition comprising a Li/Al-LDH substrate and a polymer comprises enhanced adsorption of lithium.

### Claim 11 (depends on 10)

The method of claim 10, wherein the pumping is stopped once the slurry reaches a pH of about 7.0.

### Claim 12 (depends on 10)

The method of claim 10, wherein the pumping speed of the polymer solution is between 2 mL/min and 20 mL/min.

### Claim 13 (depends on 10)

The method of claim 10, wherein the concentration of the polymer solution is between 5 wt/v % and 50 wt/v %.

### Claim 14 (depends on 10)

The method of claim 10, wherein the polymer solution comprises a polymer selected from a polyethylene glycol (PEG), a polyacrylic acid (PAA), a polyacrylonitrile (PAN), a polylactic acid (PLA), a polyvinyl chloride (PVC), a polypropylene (PP), a poly (ethylene terephthalate) (PET), a polystyrene (PS), and combinations thereof.

### Claim 15 (depends on 10)

The method of claim 10, wherein a ratio of the polymer solution to Li/Al-LDH is 10 mL/g to 90 mL/g.

### Claim 16 (depends on 10)

The method of claim 10, wherein about 50% to about 100% of the polymer present initially in the polymer solution is incorporated into the composition comprising a Li/Al-LDH substrate obtained following step (e).

### Claim 17 (depends on 10)

A composition comprising a Li/Al-LDH substrate and a polymer made the method of claim 10.

### Claim 18 (depends on 1)

A method for extraction of lithium, the method comprising:
(a) providing a lithium adsorbent composition; and
(b) contacting the disclosed lithium absorbent composition with a water-byproduct obtained from shale gas production;
wherein the disclosed lithium absorbent composition is the composition of claim 1.

### Claim 19 (depends on 18)

The method of claim 18, wherein the concentration of lithium in the polymer-modified Li/Al-LDH solution is between 100 mg/L and 200 mg/L.

### Claim 20 (depends on 18)

The method of claim 18, wherein the liquid and solid ratio during the adsorption process is between 40 mL/g and 90 mL/g.
