# US 2025/0360676 A1 · Additive manufacturing systems and methods for the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0360676 A1
- Document ID: US20250360676A1
- Status: Published application
- Kind: A1
- Application number: 19/236,714
- Filed: 2025-06-12
- Published: 2025-11-27
- Earliest claimed: 2022-12-07
- Assignees: Additive Technologies, LLC dba ADDiTEC
- Applicants: Additive Technologies, LLC dba ADDiTEC
- Inventors: Patrick Y. MAEDA; Daniel BULLARD; Dogan TIMUCIN
- Web page: https://patentgrep.com/patent/US20250360676A1

## CPC

- B22F 10/22: Direct deposition of molten metal
- B29C 64/273: pulsed; frequency modulated
- B22F 10/36: of energy beam parameters
- B22F 10/364: for post-heating, e.g. remelting
- B22F 10/50: Treatment of workpieces or articles during build-up, e.g. treatments applied to fused layers during build-up
- B22F 10/85: for controlling or regulating additive manufacturing processes
- B22F 12/10: Auxiliary heating means
- B22F 12/43: pulsed; frequency modulated
- B22F 12/90: Means for process control, e.g. cameras or sensors
- B23K 26/034: {Observing the temperature of the workpiece}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/362: Laser etching
- B23K 26/40: taking account of the properties of the material involved
- B29C 64/112: using individual droplets, e.g. from jetting heads
- B29C 64/188: involving additional operations performed on the added layers, e.g. smoothing, grinding or thickness control (surface shaping B29C59/00; after-treatment of articles without altering their shape B29C71/00)
- B29C 64/209: Heads; Nozzles
- B29C 64/245: Platforms or substrates (support structures intended to be sacrificed after manufacture B29C64/40)
- B29C 64/295: Heating elements
- B29C 64/393: for controlling or regulating additive manufacturing processes
- B33Y 10/00: Processes of additive manufacturing
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- B33Y 50/02: for controlling or regulating additive manufacturing processes
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An additive manufacturing device includes a stage configured to support a substrate. The device also includes a printhead disposed above the stage. The printhead is configured to heat a build material to a molten build material and to deposit the molten build material on the substrate in the form of droplets to fabricate an article. The device also includes a controlled heating and ablation system disposed proximal the printhead. The controlled heating and ablation system is configured to heat the substrate and ablate oxides on a surface of the substrate.

## Claims

### Claim 1

A method for fabricating an article with an additive manufacturing device, the method comprising:
heating a metal build material in a printhead to produce a molten metal build material;
ejecting the molten metal build material from the printhead towards a substrate, which forms a stack of layers of the metal build material on the substrate; and
ablating metal oxides formed on a top layer of the stack of layers of the metal build material with a controlled heating and ablation system, wherein a laser intensity of the controlled heating and ablation system is higher than an ablation threshold of the metal oxides and lower than a melting threshold of the metal build material.

### Claim 2 (depends on 1)

The method of claim 1, wherein an additional layer of the molten metal build material is deposited immediately following the controlled heating and ablation.

### Claim 3 (depends on 1)

The method of claim 1, wherein the controlled heating and ablation system concurrently heats the top layer and ablates the metal oxides on the top layer.

### Claim 4 (depends on 3)

The method of claim 3, further comprising directing a series of pulsed outputs from the controlled heating and ablation system toward the top layer to concurrently heat the top layer and ablate the metal oxides on the top layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the series of pulsed outputs comprises a first pulsed output and a second pulsed output, wherein an energy of the first pulsed output is substantially equal to an energy of the second pulsed output, and wherein a duration of the first pulsed output is substantially equal to a duration of the second pulsed output.

### Claim 6 (depends on 1)

The method of claim 1, wherein the controlled heating and ablation system heats the top layer and ablates the metal oxides on the top layer by directing a series of pulsed outputs from the controlled heating and ablation system toward the top layer.

### Claim 7 (depends on 5)

The method of claim 5, wherein the series of pulsed outputs comprises a first pulsed output and a second pulsed output, wherein an energy of the first pulsed output is relatively greater than an energy of the second pulsed output, wherein a duration of the first pulsed output is relatively shorter than a duration of the second pulsed output, wherein the first pulsed output ablates the metal oxides on the top layer, and wherein the second pulsed output heats the top layer without ablating the metal oxides.

### Claim 8

A method for fabricating an article with an additive manufacturing device, the method comprising:
heating a metal build material to produce a molten metal build material using a printhead;
depositing the molten metal build material on a substrate in the form of droplets to form a stack of layers of the metal build material; and
heating the layers, which ablates metal oxides on a top layer of the stack of layers, using a controlled heating and ablation system, wherein an intensity of a laser of the controlled heating and ablation system is higher than an ablation threshold of the metal oxides and lower than a melting threshold of the metal build material.

### Claim 9 (depends on 8)

The method of claim 8, further comprising varying an output power of the laser in a range between about 40 watts (W) to about 1500 W.

### Claim 10 (depends on 8)

The method of claim 8, further comprising varying a pulse width in a range between about 0.5 ns to about 100 ms.

### Claim 11 (depends on 8)

The method of claim 8, further comprising varying a pulse energy of the laser in a range between about 1 microjoule (μJ) to about 50 millijoules (mJ).

### Claim 12 (depends on 8)

The method of claim 8, further comprising adjusting a beam profile of the laser, wherein the beam profile comprises a Gaussian profile, a Top-Hat profile, a multimode donut profile, or a combination thereof.

### Claim 13 (depends on 8)

The method of claim 8, wherein the laser is a pulse laser, a pulse fiber laser, a pulse fiber-coupled laser, or a combination thereof.

### Claim 14 (depends on 8)

The method of claim 8, further comprising:
measuring a temperature of the top layer; and
adjusting the controlled heating and ablation system based on the temperature of the top layer.

### Claim 15 (depends on 8)

The method of claim 8, wherein heating the top layer, which ablates the metal oxides on the top layer, comprises directing a series of pulsed outputs toward the top layer, wherein the series of pulsed outputs comprises a first pulsed output and a second pulsed output, wherein an energy of the first pulsed output is substantially equal to an energy of the second pulsed output, and wherein a duration of the first pulsed output is substantially equal to a duration of the second pulsed output.

### Claim 16 (depends on 8)

The method of claim 8, wherein heating the top layer, which ablates the metal oxides on the top layer, comprises directing a series of pulsed outputs toward the layer, wherein the series of pulsed outputs comprises a first pulsed output and a second pulsed output, wherein an energy of the first pulsed output is relatively greater than an energy of the second pulsed output, and wherein a duration of the first pulsed output is relatively shorter than a duration of the second pulsed output.

### Claim 17 (depends on 8)

The method of claim 8, wherein metal oxides comprise cupric oxide (CuO) and the ablation threshold is about 1.19×107 W/cm2, and the melting threshold of the metal layer is about 6.5×107 W/cm2.

### Claim 18 (depends on 8)

The method of claim 8, wherein the controlled heating and ablation system uses a single pulse to remove the metal oxides from the top layer as completely as possible without damaging the top layer, wherein the single pulse has a wavelength of about 355 nm and a pulse duration of about 50 ns, and wherein the intensity is from about 7.5×107 W/cm2 to about 2×108 W/cm2 in response to a thickness of a layer of the metal oxides being from about 1 μm to about 2.5 μm.

### Claim 19 (depends on 8)

The method of claim 8, wherein the controlled heating and ablation system uses multiple laser pulses having a wavelength of about 355 nm and a pulse duration of about 50 ns, and wherein the laser intensity of the multiple laser pulses is about 1.25×107 W/cm2, which is able to remove the metal oxides from the top layer but does not damage the top layer after the metal oxides are removed.

### Claim 20

A method for fabricating an article with an additive manufacturing device, the method comprising:
heating a metal build material to produce a molten metal build material using a printhead;
depositing the molten metal build material on a substrate in the form of droplets to form a layer of the metal build material; and
heating the layer, which ablates metal oxides on the layer, using a controlled heating and ablation system, wherein an intensity of a laser of the controlled heating and ablation system is higher than an evaporation threshold of cupric oxide (CuO) and lower than a melting threshold of the layer, and wherein
a power of the laser is from about 40 watts (W) to about 1500 W,
an irradiance of the laser is from about 1 W/cm2 to about 10,000 W/cm2,
a wavelength of the laser is from about 355 nm to about 1200 nm,
a fluence (F) of the laser is from about 0.1 J/cm2 to about 50 J/cm2,
a pulse energy of the laser is from about 1 microjoule (μJ) to about 50 millijoules (mJ),
a pulse repetition rate of the laser is from about 5 kHz to about 250 MHZ,
a pulse width of the laser is from about 0.5 ns to about 100 ms, and
a pulse duration of the laser is lower than a thermal relaxation time of the metal layer to minimize a temperature increase of the metal layer, and
an area on the surface that is heated by the laser has a diameter of from about 0.025 mm to about 2.0 mm;
monitoring a temperature of the layer; and
adjusting the power, the irradiance, the wavelength, the fluence, the pulse energy, the pulse repetition rate, the pulse duration, and the area in response to the temperature of the layer.