# US 2025/0360494 A1 · Hydrogenation catalyst, and preparation and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0360494 A1
- Document ID: US20250360494A1
- Status: Published application
- Kind: A1
- Application number: 18/993,326
- Filed: 2023-07-11
- Published: 2025-11-27
- Earliest claimed: 2022-07-12
- Assignees: China Petroleum & Chemical Corporation; Sinopec Research Institute of Petroleum Processing Co., Ltd.
- Applicants: China Petroleum & Chemical Corporation; Sinopec Research Institute of Petroleum Processing Co., Ltd.
- Inventors: Wenbin CHEN; Hong NIE; Mingfeng LI; Yubai ZHANG; Qinghe LIU; Dadong LI; Yuanbing XI; Xueyan JU; Shi DING
- Web page: https://patentgrep.com/patent/US20250360494A1

## CPC

- B01J 27/19: Molybdenum
- B01J 21/04: Alumina
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/882: and cobalt
- B01J 23/883: and nickel
- B01J 23/8993: {with chromium, molybdenum or tungsten}
- B01J 27/0515: {with iron group metals or platinum group metals}
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/50: characterised by their shape or configuration
- B01J 35/615: {100-500 m2/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/086: {Decomposition of an organometallic compound, a metal complex or a metal salt of a carboxylic acid}
- B01J 37/20: Sulfiding
- B01J 37/28: Phosphorising
- C10G 45/08: in combination with chromium, molybdenum, or tungsten metals, or compounds thereof
- C10G 65/04: including only refining steps
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- C10G 2400/04: Diesel oil
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A hydrogenation catalyst, and preparation and use thereof are provided. The catalyst has a support and a hydrogenation active metal component, a phosphorus component and an organic complexing component supported on the support. The hydrogenation active metal component has a Group VIII metal and a Group VIB metal, the organic complexing component has an alcohol, a carboxylic acid, and/or an amine. The catalyst has a spectrum obtained by a temperature-programmed oxidation test exhibiting at least two CO2 release peaks, the first release peak being in the range of 200-300° C., the second release peak being in the range of 300-400° C. The ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 0.5-5:1.

## Claims

### Claim 1

A hydrogenation catalyst comprising a support and a hydrogenation active metal component, a phosphorus component and an organic complexing component supported on the support, wherein the hydrogenation active metal component comprises a Group VIII metal and a Group VIB metal, the organic complexing component comprises an alcohol, and further comprises a carboxylic acid and/or an amine, and the catalyst has a spectrum obtained by a temperature-programmed oxidation test exhibiting at least two CO2 release peaks, wherein the temperature corresponding to the first release peak is in the range of 200-300° C., preferably 220-280° C., the temperature corresponding to the second release peak is in the range of 300-400° C., preferably 320-380° C., and the ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 0.5-5:1, preferably 0.7-3.5:1.

### Claim 2 (depends on 1)

The catalyst according to claim 1, wherein, based on the dry weight of the catalyst and calculated as oxides, the catalyst has a content of the Group VIII metal in the range of 1-15 wt %, preferably 2-12 wt %, more preferably 3-8 wt %, a content of the Group VIB metal in the range of 12-50 wt %, preferably 15-45 wt %, more preferably 18-40 wt %, and a content of phosphorus, calculated as P2O5, in the range of 3-10 wt %, preferably 3.5-9 wt %, more preferably 4-8 wt %, and
the molar ratio of the alcohol to the Group VIB metal is in the range of 0.2-4:1, preferably 0.3-3.5:1, and the molar ratio of the total amount of the carboxylic acid and the amine to the Group VIII metal is in the range of 0.1-4:1, preferably 0.2-3.5:1;
preferably, in the catalyst, the atomic ratio of the Group VIII metal to the total amount of the Group VIII metal and the Group VIB metal is in the range of 0.1-0.5:1, more preferably 0.2-0.35:1.

### Claim 3 (depends on 1)

The catalyst according to claim 1, wherein:
the Group VIII metal is selected from iron, cobalt, nickel, ruthenium, rhodium, palladium, osmium, or any combinations thereof,
the metal element of Group VIB is selected from chromium, molybdenum, tungsten, or any combinations thereof,
the alcohol is selected from butanol, isobutanol, pentanol, heptanol, ethylene glycol, glycerol, tetramethylene glycol, polyethylene glycol, polyglycerol, pentaerythritol, xylitol, trimethylolethane, or any combinations thereof, preferably selected from butanol, glycerol, propanol, ethylene glycol, or any combinations thereof;
the carboxylic acid is selected from acetic acid, propionic acid, citric acid, caprylic acid, adipic acid, malonic acid, succinic acid, maleic acid, valeric acid, caproic acid, capric acid, benzoic acid, phenylacetic acid, phthalic acid, terephthalic acid, octadecanoic acid, tartaric acid, or any combinations thereof, preferably selected from citric acid, acetic acid, or any combinations thereof; and/or
the amine is selected from ethylenediamine, ethylenediaminetetraacetic acid, ethanolamine, triethanolamine, cyclohexanediaminetetraacetic acid, or any combinations thereof.

### Claim 4 (depends on 1)

The catalyst according to claim 1, wherein the support is the phosphorus-containing alumina support, and the phosphorus content in the alumina support, calculated as P2O5, accounts for 10-40 wt %, more preferably 20-30 wt %, of the total phosphorus content in the catalyst.

### Claim 5 (depends on 1)

The catalyst according to claim 1, wherein the catalyst has one or more of the following characteristics:
the pore volume of pores with a pore diameter in the range of 100-300 nm accounts for 5-20%, preferably 8-15% of the total pore volume of the catalyst;
the pore volume of pores with a pore diameter in the range of 2-6 nm accounts for no more than 10%, preferably no more than 8%, of the total pore volume of the catalyst; and
the pore volume of pores with a pore diameter in the range of 2-4 nm accounts for no more than 4%, preferably no more than 2%, of the total pore volume of the catalyst.

### Claim 6 (depends on 1)

The catalyst according to claim 1,
wherein the Group VIII metal is nickel or a combination of nickel with at least one of iron, ruthenium and osmium, and the atomic ratio of nickel to the total amount of the Group VIII metal(s) is in the range of 0.8-1:1, preferably 0.85-1:1;
preferably, in the spectrum obtained by the temperature-programmed oxidation test of the catalyst, the temperature corresponding to the first release peak is in the range of 210-280° C., the temperature corresponding to the second release peak is in the range of 320-380° C., and the ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 0.5-4:1,
further preferably, in the spectrum obtained by the temperature-programmed oxidation test of the catalyst, the temperature corresponding to the first release peak is in the range of 230-260° C., the temperature corresponding to the second release peak is in the range of 320-360° C., and the ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 0.7-3.5:1,
more preferably, in the catalyst, the molar ratio of the alcohol to the Group VIB metal is in the range of 0.2-4:1, preferably 0.5-2.5:1, more preferably 0.6-2.2:1, and the molar ratio of the total amount of the carboxylic acid and the amine to the Group VIII metal is in the range of 0.3-1.5:1, preferably 0.4-1.2:1, more preferably 0.5-1.1:1.

### Claim 7 (depends on 1)

The catalyst according to claim 1, wherein the Group VIII metal is cobalt or a combination of cobalt with one or more other Group VIII metal(s), and the atomic ratio of cobalt to the total amount of Group VIII metal(s) is in the range of 0.8-1:1, preferably 0.85-1:1;
preferably, in the spectrum obtained by the temperature-programmed oxidation test of the catalyst, the ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 1-5:1;
further preferably, in the spectrum obtained by the temperature-programmed oxidation test of the catalyst, the temperature corresponding to the first release peak is in the range of 220-280° C., the temperature corresponding to the second release peak is in the range of 320-380° C., and the ratio of the peak height of the first release peak to the peak height of the second release peak is in the range of 1.5-3:1,
more preferably, in the catalyst, the molar ratio of the alcohol to the Group VIB metal is in the range of 0.2-4:1, preferably 0.3-3.5:1, more preferably 0.8-2.5:1, and the molar ratio of the total amount of the carboxylic acid and the amine to the Group VIII metal is in the range of 0.1-4:1, preferably 0.2-3.5:1, more preferably 0.5-3:1.

### Claim 8 (depends on 1)

A method for preparing the hydrogenation catalyst according to claim 1, comprising steps of:
1) providing a catalyst support; and
2) supporting a Group VIII metal precursor, a Group VIB metal precursor, a phosphorus-containing compound and the organic complexing component on the catalyst support by impregnation, followed by drying to obtain the hydrogenation catalyst,
preferably, the drying is carried out under conditions including: a temperature of 60-200° C. and a time of 2-10 h.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the impregnation in step 2) comprises impregnating the catalyst support with an impregnation solution comprising the Group VIII metal precursor, the Group VIB metal precursor, the phosphorus-containing compound, and the organic complexing component;
preferably, the impregnation solution is obtained by respectively adding the Group VIII metal precursor, the Group VIB metal precursor and the organic complexing component into an aqueous solution of the phosphorus-containing compound.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the catalyst support is the phosphorus-containing alumina support, and the phosphorus content in the alumina support, calculated as P2O5, accounts for 10-40 wt %, more preferably 20-30 wt %, of the total phosphorus content in the obtained hydrogenation catalyst.
preferably, the step 1) further comprises molding and calcining phosphorus-containing pseudo-boehmite powders to obtain the phosphorus-containing alumina support, wherein the phosphorus-containing pseudo-boehmite powders are preferably prepared by introducing phosphoric acid during the preparation of pseudo-boehmite powders;
more preferably, the sodium oxide content in the phosphorus-containing pseudo-boehmite powders is in the range of no more than 0.08 wt %, more preferably no more than 0.05 wt %.

### Claim 11 (depends on 6)

A method for grading hydrogenation catalysts, comprising: sequentially loading a first hydrogenation catalyst and a second hydrogenation catalyst along a direction of material flow, wherein the first hydrogenation catalyst is the catalyst according to claim 6, wherein the loading volume ratio of the first hydrogenation catalyst to the second hydrogenation catalyst is from 1:2 to 5:1, preferably from 1:1 to 4:1.

### Claim 12 (depends on 1)

A method for hydrofining distillate oil, comprising a step of contacting the distillate oil with the hydrogenation catalyst according to claim 1 in the presence of hydrogen to carry out a reaction, wherein the hydrogenation catalyst is subjected to sulphurization treatment before use, preferably the hydrofining is selected from hydrodesulphurization, hydrodenitrogenation or a combination thereof, preferably, the sulphurization treatment is carried out by contacting the hydrogenation catalyst with a sulphurizing oil carrying a sulphurizing agent, and the sulphurization treatment is carried out under conditions preferably including: a heating rate of 5-60° C./h, a sulphurization temperature of 280-420° C., a sulphurization time of 8-48 h, a sulphurization pressure of 0.1-15 MPa, a volume space velocity of the sulphurizing oil of 0.5-20 h−1, and a hydrogen-to-oil volume ratio of 100-2000:1.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the hydrofining is hydrodenitrogenation, preferably, the reaction is carried out under conditions including: a temperature of 320-400° C., a pressure of 6-20 MPa, a volume space velocity of 0.5-3 h−1, and a hydrogen-to-oil volume ratio of 300-1500:1;
further preferably, the proportion of secondary processed diesel in the distillate oil is in the range of 20-70 wt %;
more preferably, the distillate oil contains 45-75 wt % of straight-run diesel, 25-55 wt % of catalytic diesel, and 50-2000 ppm of nitrogen.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the hydrofining is hydrodesulphurization,
preferably, the reaction is carried out under conditions including: a temperature of 320-400° C., a pressure of 3-8 MPa, a volume space velocity of 0.5-3 h−1, and a hydrogen-to-oil volume ratio of 100-500:1,
more preferably, the proportion of secondary processed diesel in the distillate oil is in the range of 0-15 wt %.

### Claim 15 (depends on 1)

A method for hydrofining distillate oil, comprising, in the presence of hydrogen, allowing the distillate oil to first pass through a first reaction zone loaded with a first hydrogenation catalyst for a hydrodenitrogenation reaction, and then to pass through a second reaction zone loaded with a second hydrogenation catalyst for a hydrodesulphurization reaction,
wherein the first hydrogenation catalyst and the second hydrogenation catalyst are according to claim 1,
in the first hydrogenation catalyst, the Group VIII metal is nickel or a combination of nickel with at least one of iron, ruthenium and osmium, and the atomic ratio of nickel to the total amount of the Group VIII metal(s) is in the range of 0.8-1:1, and
in the second hydrogenation catalyst, the Group VIII metal is cobalt or a combination of cobalt with one or more other Group VIII metal(s), and the atomic ratio of cobalt to the total amount of Group VIII metal(s) is in the range of 0.8-1:1,
preferably, each of the reactions in the first reaction zone and the second reaction zone is independently carried out under conditions including: a temperature of 300-450° C., a pressure of 3-20 MPa, a volume space velocity of 0.5-3 h−1, and a hydrogen-to-oil volume ratio of 100-2000:1;
further preferably, the proportion of secondary processed diesel in the distillate oil is in the range of 10-30 wt %;
more preferably, the distillate oil contains 75-85 wt % of straight-run diesel, 15-25 wt % of catalytic diesel, 2000-18000 ppm of sulfur, and 15-45 wt % of aromatics.

### Claim 16 (depends on 1)

A hydrogenation catalyst graded system, comprising a first hydrogenation catalyst and a second hydrogenation catalyst, wherein the first hydrogenation catalyst and the second hydrogenation catalyst are according to claim 1,
in the first hydrogenation catalyst, the Group VIII metal is nickel or a combination of nickel with at least one of iron, ruthenium and osmium, and the atomic ratio of nickel to the total amount of the Group VIII metal(s) is in the range of 0.8-1:1,
in the second hydrogenation catalyst, the Group VIII metal is cobalt or a combination of cobalt with one or more other Group VIII metal(s), and the atomic ratio of cobalt to the total amount of Group VIII metal(s) is in the range of 0.8-1:1,
and
the volume ratio of the first hydrogenation catalyst to the second hydrogenation catalyst is from 1:2 to 5:1, preferably from 1:1 to 4:1.