# US 2025/0338397 A1 · Transparent-freeform wiring with auxetic structure and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0338397 A1
- Document ID: US20250338397A1
- Status: Published application
- Kind: A1
- Application number: 19/094,801
- Filed: 2025-03-28
- Published: 2025-10-30
- Earliest claimed: 2024-04-30
- Assignees: Gwangju Institute of Science and Technology; Seoul National University R&Db Foundation
- Applicants: Gwangju Institute of Science and Technology; Seoul National University R&Db Foundation
- Inventors: Young Chang JOO; Han Wool YEON; Seon Gi LEE; Sung Jae CHOI
- Web page: https://patentgrep.com/patent/US20250338397A1

## CPC

- H05K 1/0283: {Stretchable printed circuits}
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H05K 2201/0108: Transparent
- H05K 2201/0326: Inorganic, non-metallic conductor, e.g. indium-tin oxide [ITO]
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The present inventive concept relates to a transparent-freeform wiring with an auxetic structure and a method for manufacturing the same. Strain of the transparent-freeform wiring may be improved by repeatedly connecting the auxetic structure, which consists of rotating tiles, hinges, and coupling rotating tiles, and excellent electrical conductivity may be achieved by depositing a metal thin film inside the transparent-freeform wiring.

## Claims

### Claim 1

A transparent-freeform wiring with an auxetic structure, the transparent-freeform wiring comprising:
a stretchable substrate; and
a composite transparent conductive thin film with an auxetic structure formed on the stretchable substrate,
wherein the composite transparent conductive thin film has a sandwich structure in which a metal thin film is formed between one or more transparent conductive thin films.

### Claim 2 (depends on 1)

The transparent-freeform wiring of claim 1, wherein
the auxetic structure includes one rotating tile at a center portion thereof, two or more hinges connected to the rotating tile, and coupling rotating tiles respectively formed at ends of the hinges, and
the auxetic structure is repeatedly connected.

### Claim 3 (depends on 2)

The transparent-freeform wiring of claim 2, wherein the rotating tile, the hinges, and the coupling rotating tiles are made of the same material.

### Claim 4 (depends on 2)

The transparent-freeform wiring of claim 2, wherein the coupling rotating tiles serve as connection parts of the auxetic structure, and when two or more coupling rotating tiles are coupled, the two or more coupling rotating tiles function as the rotating tile.

### Claim 5 (depends on 2)

The transparent-freeform wiring of claim 2, wherein
each of the hinges has an “L” shape, and
when a force is applied to the auxetic structure, bent portions of the hinges unfold to change a shape of the transparent-freeform wiring.

### Claim 6 (depends on 5)

The transparent-freeform wiring of claim 5, wherein each of the hinges has an extended portion at a terminal end of the “L” shape, and each of the hinges has a “C” shape.

### Claim 7 (depends on 1)

The transparent-freeform wiring of claim 1, wherein the transparent conductive thin film is indium tin oxide (ITO).

### Claim 8

A method for manufacturing a transparent-freeform wiring with an auxetic structure, comprising:
forming a sacrificial layer on a substrate;
forming a composite transparent conductive thin film by depositing one or more transparent conductive thin films and a metal thin film on the sacrificial layer;
removing the sacrificial layer through an electrochemical reaction to separate the composite transparent conductive thin film from the substrate; and
transferring the composite transparent conductive thin film onto a stretchable substrate,
wherein the composite transparent conductive thin film is formed into the auxetic structure.

### Claim 9 (depends on 8)

The method of claim 8, wherein the forming of the composite transparent conductive thin film by depositing one or more transparent conductive thin films and the metal thin film on the sacrificial layer includes:
forming a first transparent conductive thin film on the sacrificial layer;
forming a metal thin film on the first transparent conductive thin film;
forming a second transparent conductive thin film on the metal thin film to form the composite transparent conductive thin film; and
forming the auxetic structure on the composite transparent conductive thin film.

### Claim 10 (depends on 8)

The method of claim 8, wherein the forming of the composite transparent conductive thin film by depositing one or more transparent conductive thin films and the metal thin film on the sacrificial layer includes:
forming a first transparent conductive thin film on the sacrificial layer;
forming the auxetic structure on the first transparent conductive thin film;
forming a metal thin film on the first transparent conductive thin film;
forming a second transparent conductive thin film on the metal thin film; and
forming the auxetic structure on the second transparent conductive thin film.

### Claim 11 (depends on 8)

The method of claim 8, wherein
the auxetic structure includes one rotating tile at a center portion thereof, two or more hinges connected to the rotating tile, and coupling rotating tiles respectively formed at ends of the hinges, and
the auxetic structure is repeatedly connected.

### Claim 12 (depends on 11)

The method of claim 11, wherein the rotating tile, the hinges, and the coupling rotating tiles are made of the same material.

### Claim 13 (depends on 11)

The method of claim 11, wherein the coupling rotating tiles serve as connection parts of the auxetic structure, and when two or more coupling rotating tiles are coupled, the two or more coupling rotating tiles function as the rotating tile.

### Claim 14 (depends on 11)

The method of claim 11, wherein
each of the hinges has an ‘L’ shape, and
when a force is applied to the auxetic structure, bent portions of the hinges unfold to change a shape of the transparent-freeform wiring.

### Claim 15 (depends on 14)

The method of claim 14, wherein each of the hinges has an extended portion at a terminal end of the “L” shape, and each of the hinges has a “C” shape.

### Claim 16 (depends on 8)

The method of claim 8, wherein the transparent conductive thin film is indium tin oxide (ITO).

### Claim 17 (depends on 8)