# US 2025/0334731 A1 · Composite phosphor ceramic optical fiber with high luminous efficiency and high color rendering index, and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0334731 A1
- Document ID: US20250334731A1
- Status: Published application
- Kind: A1
- Application number: 19/258,868
- Filed: 2025-07-02
- Published: 2025-10-30
- Earliest claimed: 2023-01-06
- Assignees: Jiangsu Normal University; Jiangsu Xiyi Advanced Materials Research Institute Of Industrial Technology Co., LTD; Xuzhou All-To Photoelectric Technology Co., Ltd; Suzhou University of Science and Technology
- Applicants: Jiangsu Normal University; Jiangsu Xiyi Advanced Materials Research Institute Of Industrial Technology Co., LTD; Xuzhou All To Photoelectric Technology Co., LTD; Suzhou University of Science and Technology
- Inventors: Le ZHANG; Mingyuan LIU; Lv ZHU; Cong WEI; Cen SHAO; Jian KANG; Chunming ZHOU; Tianyuan ZHOU; Hao CHEN; Guocan HUANG
- Web page: https://patentgrep.com/patent/US20250334731A1

## CPC

- G02B 6/0003: {the light guides being doped with fluorescent agents}
- C04B 35/62236: {Fibres based on aluminium oxide}
- C04B 35/62272: {based on non-oxide ceramics (carbon nanotubes C01B32/15; carbon fibers D01F9/12)}
- C04B 35/6261: {Milling}
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/62852: {Alumina or aluminates}
- C04B 35/63444: {Nitrogen-containing polymers, e.g. polyacrylamides, polyacrylonitriles, polyvinylpyrrolidone [PVP], polyethylenimine [PEI]}
- C04B 35/638: Removal thereof
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C09K 11/7774: {Aluminates}
- G02B 1/02: made of crystals, e.g. rock-salt, semi-conductors (G02B1/08 takes precedence)
- G02B 6/02: Optical fibres with cladding {with or without a coating}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/63456: {Polyurethanes; Polyisocyanates}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3241: Chromium oxides, chromates, or oxide-forming salts thereof
- C04B 2235/3262: Manganese oxides, manganates, rhenium oxides or oxide-forming salts thereof, e.g. MnO
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/524: Non-oxidic, e.g. borides, carbides, silicides or nitrides
- C04B 2235/526: characterised by the length of the fibers
- C04B 2235/5264: characterised by the diameter of the fibers
- C04B 2235/6022: Injection moulding
- C04B 2235/6023: Gel casting
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/662: Annealing after sintering
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

A composite phosphor ceramic optical fiber with luminous efficiency and color rendering index includes a phosphor ceramic fiber core and a phosphor ceramic cladding, the phosphor ceramic fiber core uses a yellow phosphor ceramic doped with Ce ions, and the phosphor ceramic cladding uses a red phosphor ceramic co-doped with ions. The composite phosphor ceramic fiber is prepared by the gel casting. With this design structure, not only can the energy transfer between Ce ions and other ions cause a red shift in the spectrum to improve the color rendering index, but also the luminous efficiency can be significantly enhanced. In addition, a diameter of the composite phosphor ceramic optical fiber matches a laser spot size very well, effectively solving the “yellow ring effect” problem caused by the mismatch. It can effectively solve the heat dissipation problem during high power LD pumping and is conducive to long term stable lighting.

## Claims

### Claim 1

A composite phosphor ceramic optical fiber, comprising a phosphor ceramic fiber core and a phosphor ceramic cladding; wherein a chemical formula of the phosphor ceramic fiber core is (RE1−xCex)3Al5O12, where 0.00013≤x≤0.005, and RE represents yttrium (Y) or lutetium (Lu); and a chemical formula of the phosphor ceramic cladding is (A1−yCey)3(Al1−zBz)5O12, where 0.001≤y≤0.01, and 0.001≤z≤0.08, A represents Y or Lu, and B represents manganese (Mn) or chromium (Cr); and
wherein a diameter of the composite phosphor ceramic optical fiber is in a range of 0.15 millimeters (mm) to 1 mm, and a diameter of the phosphor ceramic fiber core is in a range of 0.05 mm to 0.2 mm.

### Claim 2 (depends on 1)

A preparation method of the composite phosphor ceramic optical fiber as claimed in claim 1, comprising:
(1) weighing first oxide raw material powders according to a chemical stoichiometric ratio of each element in the chemical formula (RE1−xCex)3Al5O12, where 0.0001≤x≤0.005, of the phosphor ceramic fiber core, mixing the first oxide raw material powders to obtain first mixed powder, adding sintering aids, a dispersant, grinding balls, and anhydrous ethanol into the first mixed powder to form a first premix solution, and ball-milling the first premix solution to obtain a first mixed slurry; after the ball-milling is completed, drying the first mixed slurry, followed by sieving and removing impurities to obtain fiber core ceramic powder for gel casting;
(2) weighing second oxide raw material powders according to a chemical stoichiometric ratio of each element in the chemical formula (A1−yCey)3(Al1−zBz)5O12, where 0.001≤y≤0.01 and 0.001≤z≤0.08, of the phosphor ceramic cladding, mixing the second oxide raw material powders to obtain second mixed powder, adding the sintering aids, the dispersant, the grinding balls, and the anhydrous ethanol to form a second premix solution, and ball-milling the second premix solution to obtain a second mixed slurry; after the ball-milling is completed, drying the second mixed slurry, followed by sieving and removing impurities to obtain cladding ceramic powder for gel casting;
(3) preparing the fiber core ceramic powder obtained in the step (1) and the cladding ceramic powder obtained in the step (2) into a slurry for preparing the phosphor ceramic fiber core and a slurry for preparing the phosphor ceramic cladding in a gel system, respectively;
vacuum defoaming the slurry for preparing the phosphor ceramic fiber core to obtain a defoamed slurry, injecting the defoamed slurry into a first capillary glass tube, and drying the defoamed slurry injected in the first capillary glass tube to form a phosphor ceramic optical fiber green body, followed by debinding, vacuum-sintering, annealing, and polishing to obtain the phosphor ceramic fiber core; and
(4) placing the phosphor ceramic fiber core obtained in the step (3) in a center of a second capillary glass tube, injecting the slurry for preparing the phosphor ceramic cladding around the phosphor ceramic fiber core, and drying the slurry for preparing the phosphor ceramic cladding injected around the phosphor ceramic fiber core, followed by debinding, vacuum-sintering, annealing, and polishing to obtain the composite phosphor ceramic optical fiber.

### Claim 3 (depends on 2)

The preparation method as claimed in claim 2, wherein, in the step (1) and the step (2), the sintering aids are magnesium oxide (MgO) and tetraethyl orthosilicate (TEOS), and an amount added of the MgO is in a range of 0.2 weight percent (wt %) to 0.7 wt % of a total weight of the first oxide raw material powders or the second oxide raw material powders, and an amount added of the TEOS is in a range of 0.4 wt % to 0.6 wt % of the total weight of the first oxide raw material powders or the second oxide raw material powders; the dispersant is polyethyleneimine (PEI), and an amount added of the PEI is in a range of 0.2 wt % to 0.5 wt % of the total weight of the first oxide raw material powders or the second oxide raw material powders; and a speed of the ball-milling is in a range of 170 revolutions per minute (r/min) to 260 r/min, and a time of the ball-milling is in a range of 24 hours (h) to 36 h.

### Claim 4 (depends on 2)

The preparation method as claimed in claim 2, wherein in the step (1) and the step (2), a temperature of the drying is in a range of 50 Celsius degrees (° C.) to 120° C., a mesh size of the sieving is in a range of 80 mesh to 300 mesh, and a temperature of the removing impurities is in a range of 800° C. to 1100° C.

### Claim 5 (depends on 2)

The preparation method as claimed in claim 2, wherein the gel system in the step (3) is one of an acrylamide system, a methacrylamide system, and a polyfunctional isocyanate bulk gel material (PIBM) system, and a solid content of each of the slurry for preparing the phosphor ceramic fiber core and the slurry for preparing the phosphor ceramic cladding is in a range of 52 volume percentage (vol %) to 56 vol %.

### Claim 6 (depends on 2)

The preparation method as claimed in claim 2, wherein, in the step (3) and the step (4), a temperature of the drying is in a range of 25° C. to 60° C., and a time of the drying is in a range of 12 h to 48 h, and the debinding comprises:
heating from room temperature to 500° C. at a rate of 0.2 Celsius degrees per minute (° C./min) to 5° C./min, then heating to 900° C. at a rate of 5° C./min to 10° C./min, and holding at 900° C. for 5 h to 8 h.

### Claim 7 (depends on 2)

The preparation method as claimed in claim 2, wherein, in the step (3) and the step (4), a temperature of the vacuum-sintering is in a range of 1700° C. to 1800° C., and a holding time of the temperature of the vacuum-sintering is in a range of 8 h to 20 h.

### Claim 8 (depends on 2)

The preparation method as claimed in claim 2, wherein, in the step (3) and the step (4), a temperature of the annealing is in a range of 1400° C. to 1450° C., and a holding time of the temperature of the annealing is in a range of 10 h to 20 h.