# US 2025/0326698 A1 · Systems and methods for limiting void formation in ceramic matrix composite components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0326698 A1
- Document ID: US20250326698A1
- Status: Published application
- Kind: A1
- Application number: 18/637,706
- Filed: 2024-04-17
- Published: 2025-10-23
- Earliest claimed: 2024-04-17
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Jerome Geoffrey Magnant; Daniel Gene Dunn; Jared Hogg Weaver; Paul Edward Gray; Gregory Allen Willis; Daniel P. Ivkovich
- Web page: https://patentgrep.com/patent/US20250326698A1

## CPC

- C04B 35/573: obtained by reaction sintering {or recrystallisation}
- C04B 41/457: {Non-superficial impregnation or infiltration of the substrate}
- B29C 73/025: {fed under pressure}
- C04B 35/591: obtained by reaction sintering
- C04B 35/62868: {Boron nitride}
- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C04B 37/006: {consisting of metals or metal salts}
- C04B 41/009: {characterised by the material treated}
- C04B 41/4523: {applied from the molten state (vitreous materials C04B41/5022); Thermal spraying, e.g. plasma spraying}
- C04B 41/5006: {Boron compounds}
- C04B 41/5096: {Silicon (C04B35/573 takes precedence)}
- C04B 2111/00982: {as construction elements for space vehicles or aeroplanes}
- C04B 2235/428: Silicon
- C04B 2235/5224: Alumina or aluminates
- C04B 2235/5228: Silica and alumina, including aluminosilicates, e.g. mullite
- C04B 2235/5232: Silica or silicates other than aluminosilicates, e.g. quartz
- C04B 2235/5244: Silicon carbide
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/616: Liquid infiltration of green bodies or pre-forms
- C04B 2237/16: Silicon interlayers
- C04B 2237/38: Fiber or whisker reinforced
- F01D 5/282: {Selecting composite materials, e.g. blades with reinforcing filaments}
- F01D 5/284: {Selection of ceramic materials}
- F05D 2240/11: Shroud seal segments
- F05D 2300/132: Chromium
- F05D 2300/133: Titanium
- F05D 2300/134: Zirconium
- F05D 2300/222: Silicon
- F05D 2300/226: Carbides
- F05D 2300/229: Sulfides
- F05D 2300/6033: Ceramic matrix composites [CMC]
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

A method for limiting void formation in a melt-infiltrated ceramic matrix composite (MI-CMC) component includes arranging one or more infiltrant feedstocks in fluid communication with a targeted area of the MI-CMC component. The one or more infiltrant feedstocks have a nominal melting point at or below a nominal melting point of an alloy within the MI-CMC component. The method includes heating the one or more infiltrant feedstocks to a first temperature at or above the nominal melting point of the one or more infiltrant feedstocks to form a molten phase. The method also includes infiltrating the targeted area of the MI-CMC component with the molten phase. As such, the molten phase reacts with a solid phase in the targeted area of the MI-CMC component. Further, the method includes cooling the MI-CMC component to a second temperature that is below the first temperature to solidify the molten phase.

## Claims

### Claim 1

A method of limiting void formation in a melt-infiltrated ceramic matrix composite (MI-CMC) component, the method comprising:
arranging one or more infiltration sources in fluid communication with a targeted area of the MI-CMC component, the one or more infiltration sources having a nominal melting point at or below a nominal melting point of an alloy within the MI-CMC component;
heating the one or more infiltration sources to a first temperature at or above the nominal melting point of the one or more infiltration sources to form a molten phase;
infiltrating the targeted area of the MI-CMC component with the molten phase, wherein the molten phase reacts with a solid phase in the targeted area of the MI-CMC component; and
cooling the MI-CMC component to a second temperature that is below the first temperature to solidify the molten phase.

### Claim 2 (depends on 1)

The method of claim 1, wherein the one or more infiltration sources comprise one or more infiltrant feedstocks containing a silicon-based material and an infiltrant pre-alloyed material.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
saturating a wick with the molten phase of the one or more infiltrant feedstocks to form a saturated wick;
cooling the wick below a melting point of the alloy to transition the alloy in the molten phase to a solid phase of the alloy; and
arranging the saturated wick in fluid communication with the targeted area of the MI-CMC component.

### Claim 4 (depends on 3)

The method of claim 3, further comprising delivering the molten phase to the targeted area of the MI-CMC component before the wick can draw molten alloy from the MI-CMC component creating additional porosity.

### Claim 5 (depends on 2)

The method of claim 2, wherein the silicon-based material is an infiltrant powder mixture comprising at least one of silicon or a silicon alloy and an additive material.

### Claim 6 (depends on 5)

The method of claim 5, wherein the additive material comprises a boron-containing additive material.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nominal melting point of the one or more infiltration sources is less than about 1400 degrees Celsius (° C.).

### Claim 8 (depends on 1)

The method of claim 1, wherein the MI-CMC component is a part of a gas turbine engine.

### Claim 9

A system for limiting void formation in a melt-infiltrated ceramic matrix composite (MI-CMC) component, the MI-CMC component having a targeted area needing infiltration, the system comprising:
one or more infiltration sources having a nominal melting point at or below a nominal melting point of an alloy within the MI-CMC component; and
a heat source for heating the one or more infiltration sources to a first temperature to form a molten phase;
wherein, when the one or more infiltration sources is placed in fluid communication with the targeted area, the molten phase infiltrates and reacts with a solid phase within the MI-CMC component at the targeted area, and
wherein the MI-CMC component is cooled to a second temperature that is below the first temperature to solidify the molten phase.

### Claim 10 (depends on 9)

The system of claim 9, wherein the one or more infiltration sources comprise at least one of a wick saturated with the molten phase or one or more infiltrant feedstocks containing a silicon-based material and an infiltrant pre-alloyed material, and wherein the silicon-based material is an infiltrant powder mixture comprising at least one of silicon or a silicon alloy and an additive material.

### Claim 11 (depends on 10)

The system of claim 10, wherein the additive material comprises a boron-containing additive material.

### Claim 12

A method of limiting void formation in a melt-infiltrated ceramic matrix composite (MI-CMC) component, the method comprising:
saturating a wick with a material in a molten phase;
cooling the saturated wick below a melting point of the material to transition the molten phase of the material to a solid phase;
arranging the saturated wick in fluid communication with a targeted area of the MI-CMC component;
heating the saturated wick to a first temperature at or above the melting point of the material to return the solid phase of the material to the molten phase;
infiltrating the targeted area of the MI-CMC component with the molten phase, wherein the molten phase of the material reacts with a solid phase of another material in the targeted area of the MI-CMC component; and
cooling the MI-CMC component to a second temperature that is below the first temperature to solidify the molten phase.

### Claim 13 (depends on 12)

The method of claim 12, further comprising:
providing a first infiltrant feedstock; and
arranging the saturated wick between the first infiltrant feedstock and the targeted area.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first infiltrant feedstock comprises a first silicon-based material having a first nominal melting point, and wherein the saturated wick comprises a second silicon-based material having a second nominal melting point, the first nominal melting point being greater than or equal to the second nominal melting point.

### Claim 15 (depends on 13)

The method of claim 13, wherein the first infiltrant feedstock has a first nominal melting point, the method further comprising:
forming a second infiltrant feedstock having a second nominal melting point.

### Claim 16 (depends on 15)

The method of claim 15, further comprising arranging the second infiltrant feedstock in fluid communication with the first infiltrant feedstock, wherein the second nominal melting point of the second infiltrant feedstock is lower than the first nominal melting point of the first infiltrant feedstock to induce melting of the first infiltrant feedstock before the first infiltrant feedstock is heated to the first nominal melting point.

### Claim 17 (depends on 13)

The method of claim 13, further comprising:
forming the first infiltrant feedstock of an infiltrant powder mixture and an infiltrant pre-alloyed material.

### Claim 18 (depends on 17)

The method of claim 17, wherein the infiltrant powder mixture comprises a silicon-based powder and a boron-containing additive material.

### Claim 19 (depends on 12)

The method of claim 12, further comprising arranging an unsaturated wick adjacent to the saturated wick.

### Claim 20 (depends on 12)

The method of claim 12, wherein the MI-CMC component is part of a gas turbine engine.