# US 2025/0323477 A1 · Method of jointing cables

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0323477 A1
- Document ID: US20250323477A1
- Status: Published application
- Kind: A1
- Application number: 19/033,673
- Filed: 2025-01-22
- Published: 2025-10-16
- Earliest claimed: 2024-02-19
- Applicants: Nexans
- Inventors: Robin SANGAR; Karl Magnus BENGTSSON; Matias HALL
- Web page: https://patentgrep.com/patent/US20250323477A1

## CPC

- H02G 1/14: for joining or terminating cables
- B23K 20/028: {Butt welding}
- H01B 7/2825: {using a water impermeable sheath}
- H02G 15/14: specially adapted for submarine cables
- B23K 2101/04: Tubular or hollow articles
- H02G: INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINED OPTICAL AND ELECTRIC CABLES OR LINES
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A method of jointing a first subsea cable to a second subsea cable is provided. A first water barrier layer that surrounds a first cable core. The second subsea cable has a second water barrier layer that surrounds a second cable core. The method includes jointing the first and second water barrier layers. The jointing has the use of a solid-state diffusion process. Optionally, the jointing has bonding an intermediate water barrier to the first and/or second water barrier layers.

## Claims

### Claim 1

A method of jointing a first subsea cable to a second subsea cable, the first subsea cable having a first water barrier layer surrounding a first cable core and the second subsea cable having a second water barrier layer surrounding a second cable core, the method comprising:
jointing the first and second water barrier layers, the jointing comprising the use of a solid-state diffusion process.

### Claim 2 (depends on 1)

The method as defined in claim 1, wherein jointing the first and second water barrier layers comprises: using a solid-state diffusion process to form a first bond between an intermediate water barrier and the first water barrier layer while a portion of the first water barrier is in contact with the intermediate water barrier.

### Claim 3 (depends on 2)

The method as defined in claim 2, wherein jointing the first and second water barrier layers further comprises: using a solid-state diffusion process to form a second bond between the intermediate water barrier and the second water barrier layer while a portion of the second water barrier layer is in contact with the intermediate water barrier.

### Claim 4 (depends on 2)

The method as defined in claim 2, wherein the first and/or second bonds form a continuous seal around first and second water barrier layers, respectively.

### Claim 5 (depends on 2)

The method as defined in claim 2, wherein at least one of the first and second water barrier layers, and/or the intermediate water barrier, comprises a metal.

### Claim 6 (depends on 5)

The method as defined in claim 5, wherein the metal is lead, copper, nickel, tin or titanium.

### Claim 7 (depends on 5)

The method as defined in claim 5, wherein each of the intermediate water barrier and the first and second water barrier layers comprise the metal.

### Claim 8 (depends on 3)

The method as defined in claim 3, wherein the solid-state diffusion process used to form the first bond, or the second bond, comprises applying a pressure that is greater than atmospheric pressure.

### Claim 9 (depends on 8)

The method as defined in claim 8, wherein the pressure is 1 Megapascal or greater.

### Claim 10 (depends on 3)

The method as defined in claim 3, wherein the solid-state diffusion process used to form the first bond, and the second bond, comprises heating at least one of the portions of the respective first or second water barrier layer and the intermediate water barrier that are in contact with one another to a temperature of greater than 50% of the melting point of the intermediate water barrier.

### Claim 11 (depends on 8)

The method as defined in claim 8 wherein the solid-state diffusion process comprises:
applying pressure for at least 1 hour and less than 24 hours.

### Claim 12 (depends on 3)

The method as defined in any one of claim 3, wherein the solid-state diffusion process used to form the first bond, and/or the second bond, comprises cleaning at least the portions of the respective first or second water barrier layers and the intermediate water barrier that contact one another prior to forming the respective bond.

### Claim 13 (depends on 3)

The method as defined in claim 3, wherein the solid-state diffusion process used to form the first bond, and the second bond, comprises replacing a portion of air surrounding the joint with an inert gas such as a noble gas or nitrogen.

### Claim 14 (depends on 1)

The method as defined in claim 1, further comprising jointing the first and second cable cores before jointing the first and second water barrier layers.

### Claim 15 (depends on 1)

The jointed cable comprising a first cable portion jointed to a second cable portion using a method as defined in claim 1 such that a first water barrier layer of the first cable portion is jointed to a second water barrier layer of the second cable portion.

### Claim 16 (depends on 1)

The method as defined in claim 1, wherein at least one of the first and second water barrier layers comprises a metal.

### Claim 17 (depends on 2)

The method as defined in claim 2, wherein the solid-state diffusion process used to form the first bond comprises applying a pressure that is greater than atmospheric pressure.

### Claim 18 (depends on 2)

The method as defined in claim 2, wherein the solid-state diffusion process used to form the first bond comprises heating at least one of the portions of the respective first or second water barrier layer and the intermediate water barrier that are in contact with one another to a temperature of greater than 50% of the melting point of the intermediate water barrier.

### Claim 19 (depends on 10)

A method as defined in claim 10 wherein the solid-state diffusion process comprises: heating for at least 1 hour and less than 24 hours.

### Claim 20 (depends on 2)

A method as defined in claim 2, wherein the solid-state diffusion process used to form the first bond comprises cleaning at least the portions of the respective first or second water barrier layers and the intermediate water barrier that contact one another prior to forming the respective bond.

### Claim 21 (depends on 2)

The method as defined in claim 2, wherein the solid-state diffusion process used to form the first bond comprises replacing a portion of air surrounding the joint with an inert gas such as a noble gas or nitrogen.