# US 2025/0320601 A1 · Method and system for forming a silicon oxycarbide layer and structure formed using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0320601 A1
- Document ID: US20250320601A1
- Status: Published application
- Kind: A1
- Application number: 19/234,603
- Filed: 2025-06-11
- Published: 2025-10-16
- Earliest claimed: 2022-01-07
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Takashi Yoshida; Kai Okabe; Zecheng Liu
- Web page: https://patentgrep.com/patent/US20250320601A1

## CPC

- C23C 16/401: {containing silicon}
- C23C 16/45542: {Plasma being used non-continuously during the ALD reactions}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Methods of forming a silicon oxycarbide layer on a surface of a substrate are disclosed. Exemplary methods include providing an oxygen-free reactant to a reaction chamber and performing one or more deposition cycles, wherein each deposition cycle includes providing a silicon precursor to the reaction chamber for a silicon precursor pulse period and providing pulsed plasma power for a plasma power period to form the silicon oxycarbide layer.

## Claims

### Claim 1

A structure comprising:
a substrate; and
a silicon oxycarbide layer overlying the substrate, the silicon oxycarbide layer formed by:
providing the substrate within a reaction chamber of a reactor;
providing an oxygen-free reactant to the reaction chamber; and
performing one or more deposition cycles, wherein each deposition cycle comprises:
providing a silicon precursor to the reaction chamber for a silicon precursor pulse period, the silicon precursor comprising at least one oxygen atom per molecule; and
providing a pulsed plasma power to an electrode for a plasma power period to form a plasma within the reactor during the plasma power period,
wherein a plasma pulse period during the plasma power period is between about 0.01 and 0.2 msec,
wherein providing the pulsed plasma power produces a plasma having a reduced plasma potential, compared to a plasma formed by providing a same plasma power to the electrode without pulsing the plasma power,
wherein a dielectric constant of the silicon oxycarbide layer is less than 4.5, and
wherein a wet etch rate of the silicon oxycarbide layer in 0.5% dilute hydrofluoric acid is less than 1 nm/minute.

### Claim 2 (depends on 1)

The structure of claim 1, further comprising a feature overlying the substrate.

### Claim 3 (depends on 2)

The structure of claim 2, wherein the feature comprises a photoresist feature or a patterned feature.

### Claim 4 (depends on 3)

The structure of claim 3, wherein the patterned feature comprises one of a metallic patterned feature, a semiconductive patterned feature, or a dielectric patterned feature.

### Claim 5 (depends on 2)

The structure of claim 2, wherein the feature comprises one of a recess or a protrusion.

### Claim 6 (depends on 1)

The structure of claim 1, further comprising a spacer.

### Claim 7 (depends on 6)

The structure of claim 6, wherein the spacer is formed using the silicon oxycarbide layer.

### Claim 8 (depends on 6)

The structure of claim 6, wherein the spacer is about a feature.

### Claim 9 (depends on 1)

The structure of claim 1, wherein the dielectric constant of the silicon oxycarbide layer is less than 4.25.

### Claim 10 (depends on 1)

The structure of claim 1, wherein the dielectric constant of the silicon oxycarbide layer is between 3.5 and 4.25.

### Claim 11 (depends on 1)

The structure of claim 1, wherein the wet etch rate of the silicon oxycarbide layer in 0.5% dilute hydrofluoric acid is less than 0.8 nm/minute.

### Claim 12 (depends on 1)

The structure of claim 1, wherein the wet etch rate of the silicon oxycarbide layer in 0.5% dilute hydrofluoric acid is between 0.4 nm/minute and 0.9 nm/minute.

### Claim 13 (depends on 1)

The structure of claim 1, wherein the silicon precursor is represented by the formula:
(Ri)4-xSi(O—Ri)x, where x can be between 1 and 3,
(Ri—O—Ri)4-xSi(O—Ri)x, where x can be between 1 and 3 or,
(Ri3-xSi(O—Ri)x)—Rii—(Ri3-xSi(O—Ri)x), where x can be between 1 and 3.

### Claim 14 (depends on 13)

The structure of claim 13, wherein Ri is an independently selected alkyl group and Rii is an independently selected hydrocarbon.

### Claim 15 (depends on 1)

The structure of claim 1, wherein the silicon precursor comprises one or more of 1,2-bis(triethoxysilyl) ethane (BTESE),), dimethoxymethylvinylsilane (DMOMVS), 1,2-bis(methyldiethoxysilyl) ethane (BMDESE), and (3-methoxypropyl) trimethoxysilane (MPTMS).

### Claim 16 (depends on 1)

The structure of claim 1, wherein a duration of the plasma power period is between 0.01 and 5.0 seconds.

### Claim 17 (depends on 1)

The structure of claim 1, wherein a plasma power on-time duty cycle is greater than 0 and less than 75%.

### Claim 18 (depends on 1)

The structure of claim 1, wherein a plasma power on-time duty cycle is between about 10 and about 50%.

### Claim 19 (depends on 1)

The structure of claim 1, wherein a duration of the silicon precursor pulse period is between about 0.1 and about 2.0 seconds.

### Claim 20 (depends on 1)

The structure of claim 1, wherein the oxygen-free reactant comprises one or more of argon (Ar) and hydrogen (H2).