# US 2025/0320592 A1 · Stainless steel seamless pipe and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0320592 A1
- Document ID: US20250320592A1
- Status: Published application
- Kind: A1
- Application number: 18/865,416
- Filed: 2023-03-08
- Published: 2025-10-16
- Earliest claimed: 2022-07-05
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Yuichi KAMO; Shinsuke IDE; Koki SUGAHARA
- Web page: https://patentgrep.com/patent/US20250320592A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- C22C 38/44: with molybdenum or tungsten
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/004: {containing Cr and Ni}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/085: {Cooling or quenching}
- C21D 9/14: wear-resistant or pressure-resistant pipes
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a stainless steel seamless pipe having high strength and excellent low-temperature toughness and corrosion resistance. The stainless steel seamless pipe comprises: a predetermined chemical composition; 30% or more martensite phase, 50% or less ferrite phase, and 40% or less retained austenite phase in volume fraction; a yield stress of 758 MPa or more; and a Charpy absorbed energy vE−10 at −10° C. of 40 J or more.

## Claims

### Claim 1

A stainless steel seamless pipe comprising:
a chemical composition containing, in mass %,
C: 0.06% or less,
Si: 1.0% or less,
Mn: 0.01% or more and 1.0% or less,
P: 0.05% or less,
S: 0.005% or less,
Cr: 15.2% or more and 18.0% or less,
Mo: 1.5% or more and 4.3% or less,
Cu: 1.2% or more and 3.5% or less,
Ni: 3.5% or more and 5.2% or less,
V: 0.5% or less,
Al: 0.10% or less,
N: 0.10% or less,
O: 0.010% or less,
Sb: 0.001% or more and 1.000% or less,
Co: 0.01% or more and 1.00% or less, and
Ca: 0.001% or more and 0.030% or less,
with a balance consisting of Fe and inevitable impurities;
30% or more martensite phase, 50% or less ferrite phase, and 40% or less retained austenite phase in volume fraction;
a yield stress of 758 MPa or more; and
a Charpy absorbed energy vE−10 at −10° C. of 40 J or more.

### Claim 2 (depends on 1)

The stainless steel seamless pipe according to claim 1, wherein the chemical composition further contains, in mass %, at least one selected from the group consisting of
Nb: 0.07% or less,
Ti: 0.2% or less,
W: 0.9% or less,
B: 0.01% or less,
Ta: 0.3% or less,
Zr: 0.3% or less,
REM: 0.3% or less,
Mg: 0.01% or less, and
Sn: 1.0% or less.

### Claim 3 (depends on 1)

The stainless steel seamless pipe according to claim 1, comprising:
50% or more martensite phase, 50% or less ferrite phase, and 25% or less retained austenite phase in volume fraction; and
a yield stress of 862 MPa or more.

### Claim 4 (depends on 1)

A production method for a stainless steel seamless pipe, the production method comprising:
making a seamless steel pipe from a steel material having the chemical composition according to claim 1;
heating the seamless steel pipe to a quenching temperature of 850° C. to 1150° C.;
cooling the seamless steel pipe after the heating to a cooling stop temperature of 50° C. or less at a cooling rate of 0.01° C./s or more; and
heating the seamless steel pipe after the cooling to a tempering temperature of 500° C. to 650° C., to produce a stainless steel seamless pipe having:
30% or more martensite phase, 50% or less ferrite phase, and 40% or less retained austenite phase in volume fraction; a yield stress of 758 MPa or more; and a Charpy absorbed energy vE−10 at −10° C. of 40 J or more.

### Claim 5 (depends on 4)

The production method for a stainless steel seamless pipe according to claim 4, wherein the stainless steel seamless pipe has: 50% or more martensite phase, 50% or less ferrite phase, and 25% or less retained austenite phase in volume fraction; and a yield stress of 862 MPa or more.

### Claim 6 (depends on 2)

The stainless steel seamless pipe according to claim 2, comprising:
50% or more martensite phase, 50% or less ferrite phase, and 25% or less retained austenite phase in volume fraction; and
a yield stress of 862 MPa or more.

### Claim 7 (depends on 2)

A production method for a stainless steel seamless pipe, the production method comprising:
making a seamless steel pipe from a steel material having the chemical composition according to claim 2;
heating the seamless steel pipe to a quenching temperature of 850° C. to 1150° C.;
cooling the seamless steel pipe after the heating to a cooling stop temperature of 50° C. or less at a cooling rate of 0.01° C./s or more; and
heating the seamless steel pipe after the cooling to a tempering temperature of 500° C. to 650° C., to produce a stainless steel seamless pipe having:
30% or more martensite phase, 50% or less ferrite phase, and 40% or less retained austenite phase in volume fraction; a yield stress of 758 MPa or more; and a Charpy absorbed energy vE−10 at −10° C. of 40 J or more.

### Claim 8 (depends on 7)

The production method for a stainless steel seamless pipe according to claim 7, wherein the stainless steel seamless pipe has: 50% or more martensite phase, 50% or less ferrite phase, and 25% or less retained austenite phase in volume fraction; and a yield stress of 862 MPa or more.