# US 2025/0313486 A1 · Magnesium Silicate Processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0313486 A1
- Document ID: US20250313486A1
- Status: Published application
- Kind: A1
- Application number: 19/228,564
- Filed: 2025-06-04
- Published: 2025-10-09
- Earliest claimed: 2021-08-20
- Assignees: Aspiring Materials Limited
- Applicants: Aspiring Materials Limited
- Inventors: Allan Charles Nye SCOTT; Christopher John-Paul OZE
- Web page: https://patentgrep.com/patent/US20250313486A1

## CPC

- C01F 5/14: Magnesium hydroxide
- B01D 53/62: Carbon oxides
- B01D 53/80: Semi-solid phase processes, i.e. by using slurries
- C04B 9/00: Magnesium cements or similar cements
- C04B 9/20: Manufacture, e.g. preparing the batches (preheating, burning, calcining or cooling lime stone, magnesite or dolomite C04B2/10)
- C04B 14/26: Carbonates
- C04B 20/023: {Chemical treatment}
- C04B 20/0232: {with carbon dioxide}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C25B 1/20: Hydroxides
- B01D 2251/402: of magnesium
- B01D 2253/1124: Metal oxides
- B01D 2257/504: Carbon dioxide
- C04B 28/105: {Magnesium oxide or magnesium carbonate cements}
- C04B 28/32: Magnesium oxychloride cements, e.g. Sorel cement
- C04B 2111/00019: {Carbon dioxide sequestration}
- C25B 11/043: Carbon, e.g. diamond or graphene
- C25B 11/046: Alloys
- C25B 11/047: Ceramics
- C25B 11/063: Valve metal, e.g. titanium
- C25B 11/081: the element being a noble metal
- Y02C 20/40: of CO2
- Y02P 40/18: Carbon capture and storage [CCS]
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods of processing magnesium silicate materials are described to produce a number of products including magnesium hydroxide. Related methods of use of processed magnesium silicate and other reaction products are described for energy production, cement manufacture and carbon sequestration. In one embodiment the method comprises subjecting a magnesium silicate source to an acid digestion; increasing the digested liquid pH to produce a magnesium salt solution; subjecting the magnesium salt solution to electrolysis; and recovering magnesium hydroxide produced from electrolysis. By-products such as silica, iron oxy(oxides) and others are also described along with further reaction products such as magnesium oxide and magnesium carbonate.

## Claims

### Claim 1

A method of carbon sequestration comprising the steps of:
producing magnesium hydroxide by the steps of:
selecting a magnesium silicate source;
subjecting the selected magnesium silicate to acid digestion, to produce a digested solution, acid digestion comprising mixing the magnesium silicate at a temperature of less than 120° C. with acid sufficient to decrease a pH of the acid and the digested solution to −1-6 and, recovering evolved hydrogen gas during acid digestion;
completing a base wash by increasing the digested solution pH by addition of an alkali solution at a temperature of less than 120° C., to produce a magnesium salt solution consisting of magnesium chloride, magnesium sulphate, or both magnesium chloride and magnesium sulphate;
subjecting the magnesium salt solution to electrolysis; and
recovering magnesium hydroxide produced from electrolysis; and
reacting the recovered magnesium hydroxide with carbon dioxide to sequester the carbon dioxide.

### Claim 2 (depends on 1)

The method of claim 1, wherein the magnesium silicate source is selected from: olivine, serpentine, pyroxene, amphiboles, phyllosilicates, clays, or any combination thereof

### Claim 3 (depends on 1)

The method of claim 1, further comprising, prior to acid digestion, subjecting the selected magnesium silicate source to water digestion at a temperature of less than 120° C. and wherein a ratio, by mass, of magnesium silicate source to water in the water digestion is 1 part magnesium silicate to 1 to 20 parts water to form a washed magnesium silicate.

### Claim 4 (depends on 3)

The method as claimed in claim 3 wherein evolved hydrogen gas is recovered during the water digestion.

### Claim 5 (depends on 1)

The method as claimed in claim 1 wherein the acid used during acid digestion is hydrochloric acid or sulfuric acid.

### Claim 6 (depends on 1)

The method as claimed in claim 1 wherein the base wash comprises two pH increasing steps including:
a first increase in digested solution pH by at least 1 to 3 pH greater than the digested solution pH and removing precipitated silica from the magnesium salt solution; and
a subsequent pH increase in digested solution pH to a pH of 6.0 or higher and removing precipitated iron oxide from the magnesium salt solution.

### Claim 7 (depends on 1)

The method as claimed in claim 1 wherein the alkali solution is selected from the group consisting of: magnesium hydroxide, calcium hydroxide, potassium hydroxide, sodium hydroxide, and combinations thereof.

### Claim 8 (depends on 1)

The method as claimed in claim 1 wherein an additional step is completed after recovery of the magnesium hydroxide of:
dehydrating the magnesium hydroxide to produce magnesium oxide (MgO).

### Claim 9 (depends on 1)

The method as claimed in claim 1 wherein the magnesium salt solution is subjected to a further base wash by increasing the digested solution pH by addition of an alkali solution and subsequently, completing base separation and removal of magnesium hydroxide produced during the further base wash.

### Claim 10 (depends on 1)

The method as claimed in claim 1 wherein acid digestion occurs at a temperature of approximately 60° C.

### Claim 11 (depends on 1)

The method as claimed in claim 1 wherein sufficient acid is added during acid digestion to reduce the pH to 2-5.

### Claim 12

A supplementary cementing material (SCM) agent comprising silica produced by a method comprising the steps of:
selecting a magnesium silicate source;
subjecting the selected magnesium silicate to acid digestion, to produce a digested solution, acid digestion comprising mixing the magnesium silicate at a temperature of less than 120° C. with acid sufficient to decrease a pH of the acid and the digested solution to −1-6 and, recovering evolved hydrogen gas during acid digestion;
completing a base wash by increasing the digested solution pH by addition of an alkali solution at a temperature of less than 120° C., to produce a magnesium salt solution consisting of magnesium chloride, magnesium sulphate, or both magnesium chloride and magnesium sulphate; and
recovering silica from the magnesium salt solution.

### Claim 13

A cement comprising 1-50% wt silica as a supplementary cementing material (SCM) agent and at least one cementitious compound, the cement produced by a method comprising the steps of:
selecting a magnesium silicate source;
subjecting the selected magnesium silicate to acid digestion, to produce a digested solution, acid digestion comprising mixing the magnesium silicate at a temperature of less than 120° C. with acid sufficient to decrease a pH of the acid and the digested solution to −1-6 and, recovering evolved hydrogen gas during acid digestion;
completing a base wash by increasing the digested solution pH by addition of an alkali solution at a temperature of less than 120° C., to produce a magnesium salt solution consisting of magnesium chloride, magnesium sulphate, or both magnesium chloride and magnesium sulphate;
recovering silica from the magnesium salt solution; and
mixing the recovered silica with the at least one cementitious material.

### Claim 14

A cement comprising 30-70% wt silica and the balance comprising magnesium oxide, the cement produced by a method comprising the steps of:
producing the silica is produced by a method comprising the steps of:
selecting a magnesium silicate source;
subjecting the selected magnesium silicate to acid digestion, to produce a digested solution, acid digestion comprising mixing the washed magnesium silicate at a temperature of less than 120° C. with acid sufficient to decrease a pH of the acid and the digested solution to −1-6 and, recovering evolved hydrogen gas during acid digestion;
completing a base wash by increasing the digested solution pH by addition of an alkali solution at a temperature of less than 120° C., to produce a magnesium salt solution consisting of magnesium chloride, magnesium sulphate, or both magnesium chloride and magnesium sulphate; and
recovering silica from the magnesium salt solution;
producing the magnesium oxide by:
selecting a magnesium silicate source;
subjecting the selected magnesium silicate to acid digestion, to produce a digested solution, acid digestion comprising mixing the magnesium silicate at a temperature of less than 120° C. with acid sufficient to decrease a pH of the acid and the digested solution to −1-6 and, recovering evolved hydrogen gas during acid digestion;
completing a base wash by increasing the digested solution pH by addition of an alkali solution at a temperature of less than 120° C., to produce a magnesium salt solution consisting of magnesium chloride, magnesium sulphate, or both magnesium chloride and magnesium sulphate;
subjecting the magnesium salt solution to electrolysis;
recovering magnesium hydroxide produced from electrolysis;
dehydrating the magnesium hydroxide to produce magnesium oxide (MgO); and
recovering the dehydrated magnesium oxide; and
combining the recovered silica with the recovered dehydrated magnesium oxide to form the cement.