# US 2025/0296141 A1 · Continuously cast slab and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0296141 A1
- Document ID: US20250296141A1
- Status: Published application
- Kind: A1
- Application number: 18/859,222
- Filed: 2023-03-29
- Published: 2025-09-25
- Earliest claimed: 2022-05-09
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Taiki KAWASAKI; Tomoya ODAGAKI; Kenji TSUZUMI; Kotaro TANAKA; Makoto MURATA
- Web page: https://patentgrep.com/patent/US20250296141A1

## CPC

- B22D 11/22: for cooling cast stock or mould
- B22D 11/225: {for secondary cooling}
- C21D 1/00: General methods or devices for heat treatment, e.g. annealing, hardening, quenching or tempering
- C21D 8/021: involving particular fabrication steps or treatments of ingots or slabs
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/00: Heat treatment, e.g. annealing, hardening, quenching or tempering, adapted for particular articles; Furnaces therefor
- C21D 9/0081: {for slabs; for billets}
- C21D 9/46: for sheet metals
- C21D 11/005: {for cooling}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/009: Pearlite
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A continuously cast slab that can prevent thermal cracking during cooling therefor even if the toughness of the slab is low, and a method for producing the same. Specifically, provided is a continuously cast slab for high-strength steel with features such that the average prior austenite grain size at a position of 10 mm from the surface layer of the continuously cast slab is in the range of 0.5 mm to 2.0 mm; and in the microstructure of the slab, the total area ratio of bainite and ferrite is 90% more, and the area ratio of ferrite is 0%, or 3% or more.

## Claims

### Claim 1

A continuously cast slab for high-strength steel, characterized in that:
an average prior austenite grain size at a position 10 mm from a surface layer of the continuously cast slab is in a range of 0.5 mm to 2.0 mm;
a total of an area ratio of bainite and an area ratio of ferrite in a microstructure of the slab is 90% or more; and
the area ratio of ferrite is 0%, or 3% or more.

### Claim 2 (depends on 1)

The continuously cast slab according to claim 1, comprising, in mass %:
C: in a range of 0.10% to 0.40%,
Si: in a range of 0.10% to 2.50%, and
Mn: in a range of 1.00% to 5.00%.

### Claim 3 (depends on 2)

A method for producing a continuously cast slab for high-strength steel, the continuously cast slab preventing thermal cracking due to cooling, comprising subjecting the continuously cast slab having the ingredient composition according to claim 2 to the following:
a first cooling step of cooling the continuously cast slab under a cooling condition that a retention time while a cooling temperature of a center of a wide face at a position 10 mm from a surface layer of the continuously cast slab is in a range of 1200° C. to 1450° C. is 130 seconds or less;
a second cooling step of cooling the continuously cast slab under a cooling condition that an average cooling rate when a surface temperature at the center of the wide face of the continuously cast slab is in a range of 700° C. to 850° C. is between 25° C./hr and 40° C./hr, or 50° C./hr or more; and
a third cooling step of cooling the continuously cast slab under a cooling condition that an average cooling rate when the surface temperature at the center of the wide face of the continuously cast slab is in a range of 500° C. to 700° C. is 15° C./hr or more.