# US 2025/0289983 A1 · Glitter Glue Stick and Its Preparation Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0289983 A1
- Document ID: US20250289983A1
- Status: Published application
- Kind: A1
- Application number: 18/609,615
- Filed: 2024-03-19
- Published: 2025-09-18
- Earliest claimed: 2024-03-12
- Assignees: Ningbo Pasco United Industry Co., Ltd.
- Applicants: Ningbo Pasco United Industry Co., Ltd.
- Inventors: Xiaohua QIAN
- Web page: https://patentgrep.com/patent/US20250289983A1

## CPC

- C09J 9/005: {Glue sticks}
- C09J 11/00: Features of adhesives not provided for in group C09J9/00, e.g. additives
- C09J 11/04: inorganic
- C09J 11/06: organic
- C09J 11/08: Macromolecular additives
- C09J 139/06: Homopolymers or copolymers of N-vinyl-pyrrolidones
- C08K 5/053: Polyhydroxylic alcohols
- C08L 33/08: Homopolymers or copolymers of acrylic acid esters
- C09J 2400/22: Presence of unspecified polymer
- C09J 2403/00: Presence of starch
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A glitter glue stick and its preparation method. The glitter glue stick comprises the components with the following weight percentage content: 20%˜60% deionized water, 3%˜20% propylene glycol, 10%˜40% glycerin, 15%˜30% adhesive, 0%˜1% defoamer, 1%˜10% excipient, 0.5% ˜2% caustic soda, 0.1%˜0.5% preservative, 0%˜0.3% pigment and 1% ˜10% glitter; the PH value of the glitter glue stick prepared by the present invention is 10.0 to 11.0. After gluing on the paper, the glitter powder can be uniformly and densely distributed on the gluing surface, displaying different colors and glitter effects. The drying time is controllable, and it has a strong adhesive force after completely drying.

## Claims

### Claim 1

The glitter glue stick is characterized in that it comprises the components with the following weight percentage content:
20%˜60% deionized water, 3%˜20% propylene glycol, 10%˜40% glycerin, 15%˜30% adhesive, 0%˜1% defoamer, 1%˜10% excipient, 0.5%˜2% caustic soda, 0.1%˜0.5% preservative, 0%˜0.3% pigment and 1% ˜10% glitter.

### Claim 2 (depends on 1)

The glitter glue stick described in claim 1 is characterized in that the adhesive is selected from at least one of polyvinylpyrrolidone, starch and acrylic resin.

### Claim 3 (depends on 1)

The glitter glue stick described in claim 1 is characterized in that the defoamer is a water-soluble polyether defoamer.

### Claim 4 (depends on 1)

The glitter glue stick described in claim 1 is characterized in that the excipient is a fatty acid with carbon atom number of 12 to 18.

### Claim 5 (depends on 1)

The glitter glue stick described in claim 1 is characterized in that the excipient is a mixed solution of stearic acid, palmitic acid and lauric acid.

### Claim 6 (depends on 1)

The glitter glue stick described in claim 1 is characterized in that the preservative is a BIT-type preservative.

### Claim 7 (depends on 1)

The preparation method of any of the glitter glue stick described in claim 1 is characterized in that the preparation method comprises the following steps:
(a) Immerse the glitter in the silane coupling agent solution and remove and dry it for later use; dissolve the caustic soda in partially deionized water to obtain caustic soda solution for later use;
(b) Add glycerol and propylene glycol to the remaining deionized water and stir well to obtain the first mixed solution;
(c) Under stirring conditions, add the adhesive and part of the defoamer to the first mixed solution and continue stirring for a certain period of time, then heat the mixed solution and continue stirring until the adhesive is completely dissolved. Then add the remaining defoamer and excipient and stir until they are completely dissolved to obtain the second mixed solution;
(d) Add the caustic soda solution to the second mixed solution for saponification reaction. After the end of the reaction, under the condition of heat preservation, then add the preservatives and pigments in turn and stir well, and leave to defoam, to obtain the third mixed solution;
(e) Add the glitter to the third mixed solution and stir well to obtain the said glitter glue stick.

### Claim 8 (depends on 7)

The preparation method described in claim 7 is characterized in that, in step (a), the concentration of the sodium hydroxide solution is 15% to 25%.

### Claim 9 (depends on 7)

The preparation method described in claim 7 is characterized in that the heating temperature is 80 to 90° C. in step (c).

### Claim 10 (depends on 1)

The preparation method described in claim 1 is characterized in that, in step (d), the saponification reaction by adding sodium hydroxide solution to the second mixed solution includes: adding sodium hydroxide solution to the second mixed solution at 80 to 90° C. under stirring conditions and continuing to stir for 30 to 40 min.