# US 2025/0286121 A1 · Sulphide based lithium-ion conducting solid electrolyte and methods for the production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0286121 A1
- Document ID: US20250286121A1
- Status: Published application
- Kind: A1
- Application number: 18/861,901
- Filed: 2023-05-03
- Published: 2025-09-11
- Earliest claimed: 2022-05-04
- Assignees: Umicore AG & Co. KG
- Applicants: Umicore
- Inventors: Antoine BREHAULT; Pol BRIANTAIS; Yann GUIMOND; Tom KREKELS
- Web page: https://patentgrep.com/patent/US20250286121A1

## CPC

- C01B 17/22: Alkali metal sulfides or polysulfides
- H01M 10/0562: Solid materials
- C01B 35/14: Compounds containing boron and nitrogen, phosphorus, sulfur, selenium or tellurium
- C03C 3/14: containing boron
- C03C 3/23: containing halogen and at least one oxide, e.g. oxide of boron
- C03C 4/14: for electro-conductive glass
- C03C 4/18: for ion-sensitive glass
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/431: Inorganic material
- H01M 50/437: Glass
- C01P 2002/02: Amorphous compounds
- C01P 2002/52: containing elements as dopants
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2006/37: Stability against thermal decomposition
- C01P 2006/40: Electric properties
- C03B 32/00: Thermal after-treatment of glass products not provided for in groups {C03B19/00} , C03B25/00 - C03B31/00 {or C03B37/00}, e.g. crystallisation, eliminating gas inclusions or other impurities; {Hot-pressing vitrified, non-porous, shaped glass products}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 2300/0071: Oxides
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to solid materials which are obtainable by melt-quenching mixtures of lithium sulphide, boron sulphide and boron oxide, thereby forming a glassy solid which is suitable for use as a lithium-ion conducting electrolyte. These sulphide based lithium-ion conducting solid electrolytes exhibit a large thermal stability as supported by the large ΔTx, in particular a ΔTx of more than 100° C.

## Claims

### Claim at position 1

1-18. (canceled)

### Claim 19

A solid material having a composition according to general formula (I)
Li2c+dB2a+2bS3a+cO3bXd (I)
wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
a is within the range of 0.03 to 0.1;
b is within the range of 0 to 0.04;
c is within the range of 0.12 to 0.26; and
d is within the range of 0.001 to 0.14.

### Claim 20 (depends on 19)

The solid material according to claim 19, wherein X represents Cl, Br, I, or combinations thereof.

### Claim 21 (depends on 19)

The solid material according to claim 19, wherein
a is within the range of 0.06 to 0.1;
b is within the range of 0.002 to 0.02;
c is within the range of 0.14 to 0.19; and
d is within the range of 0.001 to 0.14.

### Claim 22 (depends on 19)

The solid material according to claim 19, wherein d is within the range of 0.005 to 0.08.

### Claim 23 (depends on 19)

The solid material according to claim 19, wherein the solid material is according to Formula (I)a, (I)b, (I)c or (I)d:
Formula (I)a
Li2c+dB2a+2bS3a+cO3b(BrCl)d
Formula (I)b
Li2c+dB2a+2bS3a+cO3b(BrI)d
Formula (I)c
Li2c+dB2a+2bS3a+cO3b(ClI)d
Formula (I)d
Li2c+dB2a+2bS3a+cO3b(ClBrI)d

### Claim 24 (depends on 19)

The solid material according to claim 19, wherein 5a+5b+3c+2d=1.

### Claim 25

A solid material, which is obtainable by melt-quenching a mixture of A and B,
wherein the molar ratio of A and B in the mixture before quenching is within the range of 60:40 to 99:1; wherein component A is according to general formula (II)
xLi2S-yB2S3-zB2O3 (II)
wherein
x is within the range of 55 to 85;
y is within the range of 15 to 45;
z is within the range of 0 to 15;
x+y+z=100; and
wherein component B is LiX, wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof.

### Claim 26 (depends on 25)

The solid material according to claim 25, wherein X represents Cl, Br, I, or combinations thereof.

### Claim 27 (depends on 25)

The solid material according to claim 25, wherein x is within the range of 62 to 68; y is within the range of 27 to 33; z is within the range of 1 to 8; and x+y+z=100.

### Claim 28 (depends on 25)

The solid material according to claim 25, wherein the molar ratio of A and B in the mixture before quenching is within the range of 70:30 to 96:4.

### Claim 29 (depends on 25)

The solid material according to claim 25, wherein X represents Br, I or a combination thereof.

### Claim 30 (depends on 25)

The solid material according to claim 25, wherein the material is a glassy solid.

### Claim 31 (depends on 25)

The solid material according to claim 25, wherein the material has an ionic conductivity at 25° C. of at least 0.1 mS/cm and a thermal stability ΔTx of more than 100° C., wherein ΔTx=Tx−Tg, wherein Tx is the crystallization onset temperature as determined by DSC and Tg is the glass transition temperature as determined by DSC.

### Claim 32

A method for preparing a solid material, comprising the steps of:
(i) providing the following precursors:
Li2S;
B2S3 and/or both of boron and sulfur;
optionally B2O3; and
LiX wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
(ii) preparing a mixture comprising the precursors provided in step (i) wherein
in said mixture the molar ratio of the elements Li, S, B, O and X matches the general formula (I):
Li2c+dB2a+2bS3a+cO3bXd (I),
wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
a is within the range of 0.03 to 0.1;
b is within the range of 0 to 0.04;
c is within the range of 0.12 to 0.26; and
d is within the range of 0.001 to 0.14; or
in said mixture the molar ratio of A and B in the mixture is within the range of 60:40 to 99:1; wherein component A is according to general formula (II):
xLi2S-yB2S3-zB2O3 (II),
wherein x is within the range of 55 to 85; y is within the range of 15 to 45; z is within the range of 0 to 15; x+y+z=100; and
wherein component B is LiX, wherein X represents F, Cl, Br, I, N3, SCN, CN, OCN, BF4, BH4, or combinations thereof;
(iii) heat-treating the mixture prepared in step (ii) to obtain a melt; and
(iv) quenching the melt obtained in step (iii) to obtain the solid material.

### Claim 33 (depends on 32)

The method according to claim 32, wherein X represents Cl, Br, I, or combinations thereof.

### Claim 34 (depends on 19)

An electrochemical cell comprising the solid material as defined in claim 19.

### Claim 35 (depends on 34)

The electrochemical cell according to claim 34, wherein the electrochemical cell comprises a separator and the separator comprises the solid material.

### Claim 36 (depends on 19)

A solid electrolyte for an electrochemical cell comprising the solid material as defined in claim 19.