# US 2025/0283249 A1 · Semiconductor wafer made of single-crystal silicon and process for the production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0283249 A1
- Document ID: US20250283249A1
- Status: Published application
- Kind: A1
- Application number: 19/214,282
- Filed: 2025-05-21
- Published: 2025-09-11
- Earliest claimed: 2020-06-25
- Assignees: Siltronic AG
- Applicants: Siltronic AG
- Inventors: Andreas SATTLER; Juergen VETTERHOEFFER
- Web page: https://patentgrep.com/patent/US20250283249A1

## CPC

- C30B 29/06: Silicon
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 15/22: Stabilisation or shape controlling of the molten zone near the pulled crystal; Controlling the section of the crystal
- C30B 25/02: Epitaxial-layer growth
- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor wafer of single-crystal silicon has an oxygen concentration per new ASTM of not less than 5.0×1017 atoms/cm3 and not more than 6.5×1017 atoms/cm3; a nitrogen concentration per new ASTM of not less than 1.0×1013 atoms/cm3 and not more than 1.0×1014 atoms/cm3; a front side having a silicon epitaxial layer wherein the semiconductor wafer has BMDs whose mean size is not more than 10 nm determined by transmission electron microscopy and whose mean density adjacent to the epitaxial layer is not less than 1.0×1011 cm−3, determined by reactive ion etching after having subjected the wafer covered with the epitaxial layer to a heat treatment at a temperature of 780° C. for a period of 3 h and to a heat treatment at a temperature of 600° C. for a period of 10 h.

## Claims

### Claim 1

A process for producing a single-crystal silicon semiconductor wafer, comprising:
pulling a single crystal by the CZ method from a melt containing nitrogen in an atmosphere comprising hydrogen at a partial pressure of not less than 5 Pa and not more than 30 Pa, such that in a section of the single crystal having a uniform diameter the oxygen concentration is not less than 5.0×1017 atoms/cm3 and not more than 6.5×1017 atoms/cm3, the nitrogen concentration is not less than 1.0×1013 atoms/cm3 and not more than 1.0×1014 atoms/cm3;
controlling a pulling velocity V such that the section of the single crystal having a uniform diameter grows in a PV region;
separating the semiconductor wafer from the section of the single crystal having a uniform diameter;
heat treating the semiconductor wafer from a temperature of 600° C. to a target temperature of at least 850° C. but not more than 900° C. at a rate of not less than 0.5° C./min and not more than 2° C./min;
cooling the semiconductor wafer from the target temperature to a temperature of 600° C. at a rate of not less than 0.5° C./min and not more than 2° C./min to form a heat treated semiconductor wafer; and
depositing an epitaxial layer of silicon on a front side of the heat treated semiconductor wafer to form an epitaxial semiconductor wafer.

### Claim 2 (depends on 1)

The process of claim 1, further comprising:
keeping the semiconductor wafer at the target temperature for a period of no longer than 180 min.

### Claim 3 (depends on 1)

The process of claim 1, wherein the rate is 1° C./min.

### Claim 4 (depends on 1)

The process of claim 1, wherein the diameter of the section of the crystal having a uniform diameter is not less than 200 mm.

### Claim 5 (depends on 1)

The process of claim 1, wherein the diameter of the section of the crystal having a uniform diameter is not less than 300 mm.

### Claim 6 (depends on 1)

The process of claim 1, wherein in a region adjacent the epitaxial layer, BMDs have a mean diagonal size of no more than 10 nm and are present in an concentration of not less than 1.0×1011 cm−3.

### Claim 7 (depends on 1)

The process of claim 1, wherein the silicon semiconductor wafer contains dislocation loops and also has a dislocation loop free zone at an interface with the epitaxial layer.

### Claim 8 (depends on 1)

The process of claim 1, wherein the single-crystal silicon wafer has a nickel gettering efficiency of at least 93%.