# US 2025/0283192 A1 · Methods of recycling aluminum alloys and purification thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0283192 A1
- Document ID: US20250283192A1
- Status: Published application
- Kind: A1
- Application number: 19/213,470
- Filed: 2025-05-20
- Published: 2025-09-11
- Earliest claimed: 2017-08-16
- Assignees: Alcoa USA Corp.
- Applicants: Alcoa USA Corp.
- Inventors: Xinyan Yan; Francis Caron
- Web page: https://patentgrep.com/patent/US20250283192A1

## CPC

- C22B 21/0092: {Remelting scrap, skimmings or any secondary source aluminium}
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- C22B 21/0069: {from scrap, skimmings or any secondary source aluminium, e.g. recovery of alloy constituents (C22B21/0046, C22B21/0053 and C22B21/0092 take precedence)}
- C22B 21/06: refining {(electrolytic refining C25C; C22B21/0046, C22B21/0061 take precedence)}
- C22B 21/066: {Treatment of circulating aluminium, e.g. by filtration (C22B21/068 takes precedence)}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure relates to methods of producing purified aluminum alloys from aluminum alloy scrap by producing a melt of the aluminum alloy scrap, adding one or more intermetallic former materials, producing iron-bearing intermetallic particles, removing the iron-bearing intermetallic particles, and solidifying the low-iron melt.

## Claims

### Claim 1

A method comprising:
(a) melting aluminum alloy scrap, thereby producing a melt, wherein the aluminum alloy scrap comprises an initial iron content, wherein the initial iron content is at least 0.20 wt. % iron (Fe);
(b) adding an excess of silicon (Si) to the melt, wherein the excess of silicon is an amount of silicon sufficient to produce both (i) iron-bearing intermetallic particles in the melt and (ii) a Si-based aluminum alloy from the melt;
(c) forming iron-bearing intermetallic particles in the melt, wherein a first amount of silicon reacts with iron of the melt to form the iron-bearing intermetallic particles, and wherein a second amount of silicon remains in the melt in unreacted form, the second amount of silicon corresponding to an amount of the excess silicon employed in the adding step (b) required to create the Si-based aluminum alloy from the melt;
(d) removing at least some of the iron-bearing intermetallic particles from the melt, thereby producing a low-iron melt with the second amount of silicon therein;
(e) solidifying the low-iron melt, thereby producing the Si-based aluminum alloy having the second amount of silicon therein, wherein the Si-based aluminum alloy includes a purified iron content, wherein the purified iron content is less than the initial iron content and not greater than 0.5 wt. % Fe, and wherein the Si-based aluminum alloy includes silicon as the predominate alloying ingredient besides aluminum.

### Claim 2 (depends on 1)

The method of claim 1, comprising, during the adding step (b), further adding manganese to the melt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the purified aluminum alloy is one of a 3xx aluminum casting alloy or a 4xxx wrought aluminum alloy.

### Claim 4 (depends on 1)

The method of claim 1, wherein the purified aluminum alloy comprises not greater than 0.35 wt. % iron (Fe).

### Claim 5 (depends on 1)

The method of claim 1, wherein the purified aluminum alloy comprises not greater than 0.20 wt. % iron (Fe).

### Claim 6 (depends on 1)

The method of claim 1, wherein the purified aluminum alloy comprises not greater than 0.15 wt. % iron (Fe).

### Claim 7 (depends on 1)

The method of claim 1, wherein the producing step (c) comprises:
(i) cooling the melt from a first temperature to a second temperature, thereby producing the iron-bearing intermetallic particles.

### Claim 8 (depends on 7)

The method of claim 7, comprising:
at or below the second temperature, completing the removing step (d).

### Claim 9 (depends on 8)

The method of claim 8, wherein the removing step (d) comprises at least one of filtration of the melt and sedimentation of the melt.

### Claim 10 (depends on 9)

The method of claim 9, wherein the removing step (d) comprises filtration using a refractory filter material.

### Claim 11 (depends on 8)

The method of claim 8, wherein the second temperature is at least 10° C. higher than a solidification temperature of fcc aluminum.

### Claim 12 (depends on 11)

The method of claim 11, wherein the solidifying step (e) comprises:
cooling the melt from the second temperature to below a solidus temperature of the low-iron melt.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first temperature is a liquidus temperature, and wherein the liquidus temperature is at least 10° C. higher than the second temperature.

### Claim 14 (depends on 1)

The method of claim 1, comprising:
after the removing step (d) and prior to the solidifying step (e), adding alloying additions to the low-iron melt, wherein the alloying additions are selected from the group consisting of chromium, nickel, zinc, titanium, tin, strontium, copper, magnesium, and combinations thereof;
wherein, after the solidifying step (e), the Si-based aluminum alloy includes the alloying additions.

### Claim 15 (depends on 1)

The method of claim 1, comprising, after the removing step (d) and prior to the solidifying step (e), adding alloying additions to the low-iron melt, wherein the alloying additions include at least one of copper (Cu), and magnesium (Mg);
wherein, after the solidifying step (e), the Si-based aluminum alloy includes the alloying additions.

### Claim 16 (depends on 1)

The method of claim 1, wherein the purified iron content is at least 10% less than the initial iron content.

### Claim 17 (depends on 1)

The method of claim 1, wherein the purified iron content is at least 25% less than the initial iron content.

### Claim 18 (depends on 1)

The method of claim 1, wherein the purified iron content is at least 60% less than the initial iron content.

### Claim 19 (depends on 1)

The method of claim 1, wherein the Si-based aluminum alloy includes from 3.0 to 23.0 wt. % Si.

### Claim 20 (depends on 19)

The method of claim 19, wherein the Si-based aluminum alloy includes at least 4.0 wt. % Si.

### Claim 21 (depends on 19)

The method of claim 19, wherein the Si-based aluminum alloy includes at least 5.0 wt. % Si.

### Claim 22 (depends on 19)

The method of claim 19, wherein the Si-based aluminum alloy includes at least 6.0 wt. % Si.

### Claim 23 (depends on 20)

The method of claim 20, wherein the Si-based aluminum alloy includes at least 7.0 wt. % Si.

### Claim 24 (depends on 21)

The method of claim 21, wherein the Si-based aluminum alloy includes not greater than 20.0 wt. % Si.

### Claim 25 (depends on 22)

The method of claim 22, wherein the Si-based aluminum alloy includes not greater than 15.0 wt. % Si.