# US 2025/0281920 A1 · Methods for reducing small pores of catalyst carriers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0281920 A1
- Document ID: US20250281920A1
- Status: Published application
- Kind: A1
- Application number: 19/072,491
- Filed: 2025-03-06
- Published: 2025-09-11
- Earliest claimed: 2024-03-08
- Assignees: Scientific Design Company, Inc.
- Applicants: Scientific Design Company, Inc.
- Inventors: Mure Te; Li Zhu; Yunxia Chen; Xiankuan Zhang; Lixin Cao; Jorge Ron
- Web page: https://patentgrep.com/patent/US20250281920A1

## CPC

- B01J 35/69: bimodal
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 21/04: Alumina
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/50: Silver
- B01J 23/688: {with manganese, technetium or rhenium}
- B01J 35/612: {less than 10 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 37/0201: {Impregnation}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/16: Reducing
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

Methods are provided in which small pores having a size of less than 0.3 microns are substantially reduced by utilizing a caustic solution. In some embodiments, the reduction of the small sized pores of less than 0.3 microns is achieved by treating a preformed catalyst carrier with a hot caustic solution. In other embodiments, the reduction of small sized pores of less than 0.3 microns is achieved by adding a caustic solution to a carrier composition during the preparation/formation of a catalyst carrier. The caustic solution treated catalyst carrier exhibits a positive/upward shift of the small pore size distribution.

## Claims

### Claim 1

A method of reducing small pore size distribution of a catalyst carrier comprising:
contacting a preformed catalyst carrier having a pore size distribution of less than 0.3 microns with a caustic solution to provide an admixture of the caustic solution and preformed catalyst carrier;
heating the admixture to a temperature of about 70° C. or greater to provide a caustic solution treated preformed catalyst carrier;
cooling the caustic solution treated preformed catalyst carrier to nominal room temperature;
drying the cooled caustic solution treated preformed catalyst carrier;
calcining the dried caustic solution treated preformed catalyst carrier at a temperature of about 1200° C. or greater; and
washing the calcined caustic solution treated preformed catalyst carrier to provide a catalyst carrier having a reduced pore volumes of pores having a pore size of less than 0.3 microns as compared to the preformed catalyst carrier.

### Claim 2 (depends on 1)

The method of claim 1, wherein the caustic solution comprises a base having a pH value of about 13 or greater and water.

### Claim 3 (depends on 2)

The method of claim 2, wherein the caustic solution has a molarity of from about 0.1 M to about 2 M.

### Claim 4 (depends on 3)

The method of claim 3, wherein the caustic solution has a molarity of from about 0.5 M to about 1 M.

### Claim 5 (depends on 1)

The method of claim 1, wherein the contacting includes adding the caustic solution to the preformed catalyst carrier in an amount from about 2 ml to about 20 ml per gram of preformed catalyst carrier employed.

### Claim 6 (depends on 5)

The method of claim 5, wherein the contacting includes adding the caustic solution to the preformed catalyst carrier in an amount from about 5 ml to about 10 ml per gram of preformed catalyst carrier employed.

### Claim 7 (depends on 1)

The method of claim 1, wherein the caustic solution is NaOH.

### Claim 8 (depends on 1)

The method of claim 1, wherein the temperature of heating is from about 50° C. to about 90° C.

### Claim 9 (depends on 1)

The method of claim 1, further comprising adding a catalytically effect amount of silver to the catalyst carrier.

### Claim 10 (depends on 1)

The method of claim 1, further comprising adding a promoting amount of a transition metal or a mixture of two or more transition metals to the catalyst carrier.

### Claim 11

A method of forming a catalyst carrier comprising:
adding a caustic solution to a carrier composition to provide an admixture of the carrier composition and caustic solution;
forming the admixture into a shaped body; and
calcining the shaped body at a temperature of about 1200° C. greater to convert the shaped body into a catalyst carrier.

### Claim 12 (depends on 11)

The method of claim 11, wherein the caustic solution comprises a base having a pH value of about 13 or greater and water.

### Claim 13 (depends on 12)

The method of claim 12, wherein the caustic solution has a molarity of from about 0.1 M to about 2 M.

### Claim 14 (depends on 13)

The method of claim 13, wherein the caustic solution has a molarity of from about 0.5 M to about 1 M.

### Claim 15 (depends on 11)

The method of claim 11, wherein the caustic solution is added in an amount from about 10 wt. % to about 50 wt. % based on a total amount of alumina source present in the carrier composition.

### Claim 16 (depends on 15)

The method of claim 15, wherein the caustic solution is added in an amount from about 20 wt. % to about 30 wt. % based on a total amount of alumina source present in the carrier composition.

### Claim 17 (depends on 11)

The method of claim 11, wherein the caustic solution is NaOH.

### Claim 18 (depends on 11)

The method of claim 11, wherein the forming comprises extruding.

### Claim 19 (depends on 11)

The method of claim 11, further comprising adding a catalytically effective amount of silver to the catalyst carrier.

### Claim 20 (depends on 19)

The method of claim 19, further comprising adding a promoting amount of a transition metal or a mixture of two or more transition metals to the catalyst carrier.