# US 2025/0277288 A1 · Method for producing a cemented carbide body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0277288 A1
- Document ID: US20250277288A1
- Status: Published application
- Kind: A1
- Application number: 18/286,427
- Filed: 2022-03-18
- Published: 2025-09-04
- Earliest claimed: 2021-05-03
- Assignees: Betek GmbH & Co. KG
- Applicants: Betek GmbH & Co. KG
- Inventors: Heiko Friederichs; Britta Philipp; David Chmelik; Michael Geiger; Ulrich Krämer; Alexander Haller; Tobias Hilgert
- Web page: https://patentgrep.com/patent/US20250277288A1

## CPC

- C22C 1/051: Making hard metals based on borides, carbides, nitrides, oxides or silicides; Preparation of the powder mixture used as the starting material therefor
- B22F 3/1028: {Controlled cooling}
- B22F 3/1035: {Liquid phase sintering}
- B22F 3/16: in successive or repeated steps
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C22C 29/067: {comprising a particular metallic binder}
- C22C 29/08: based on tungsten carbide
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 2003/248: {Thermal after-treatment}
- B22F 2005/001: {Cutting tools, earth boring or grinding tool other than table ware}
- B22F 2009/043: {by ball milling}
- B22F 2301/15: Nickel or cobalt
- B22F 2302/10: Carbide
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

The invention relates to a method for producing a cemented carbide body, wherein in a mixing and/or grinding process, preferably in a wet grinding process, tungsten carbide powder (WC powder) and metallic binder material comprising cobalt powder (Co), nickel (Ni) and aluminum (Al) are mixed to form a powder mixture, wherein a green compact is pressed from at least a portion of the powder mixture and wherein the green compact is sintered in a sintering step under the influence of temperature and pressure in such a way that the cemented carbide body is formed after a cooling step following the sintering step. To create an easily controllable and reliable process for the production of a cemented carbide body, which is characterized by improved wear resistance and, at the same time, a high fracture strength, provision is made in accordance with the invention for nickel aluminide, preferably nickel aluminide powder, in particular Ni3Al powder, to be added to the mixing and/or grinding process as an intermetallic phase material.

## Claims

### Claim at position 1

1-22. (canceled)

### Claim 23

A method for producing a cemented carbide body, comprising:
combining a tungsten carbide powder and a metallic binder material comprising cobalt, nickel, and aluminum to form a powder mixture;
adding nickel aluminide to the powder mixture;
forming a green compact from the powder mixture;
sintering the green compact at a first temperature and a first pressure; and
cooling the compact to form a cemented carbide body comprising a binder phase and an intermetallic phase.

### Claim 24 (depends on 23)

The method of claim 23, wherein the tungsten carbide powder and the metallic binder material are combined in a mixing process or a milling process.

### Claim 25 (depends on 24)

The method of claim 24, wherein the mixing process or the milling process is a multi-stage process comprising at least a first mixing or milling step and a second mixing or milling step, and wherein the nickel aluminide is added before a final mixing or milling step.

### Claim 26 (depends on 24)

The method of claim 24, wherein the tungsten carbide powder and the metallic binder material are combined in a wet milling process.

### Claim 27 (depends on 23)

The method of claim 23, wherein at least a portion of the intermetallic phase comprises (M,Y)3(Al,X), wherein M is Ni, Y comprises Co, and X comprises W.

### Claim 28 (depends on 23)

The method of claim 23, wherein, when cooling the compact, the sintered body is kept at a temperature range between 400° C. and a solvus temperature of the sintered body for a period ranging from 0.25 to 24 hours.

### Claim 29 (depends on 23)

The method of claim 23, wherein the green compact comprises tungsten carbide in an amount ranging from 70 wt % to 95 wt % of the green compact, cobalt in an amount ranging from 1 wt % to 19 wt % of the green compact, and nickel aluminide in an amount ranging from 1 wt % to 28 wt % of the green compact.

### Claim 30 (depends on 23)

The method of claim 23, wherein the nickel aluminide is produced in a smelting process or added as a material produced in a melt process.

### Claim 31 (depends on 23)

The method of claim 23, wherein the nickel aluminide has a mean particle size of less than 70 μm.

### Claim 32 (depends on 23)

The method of claim 23, further comprising a preparation step, the preparation step comprising combining the nickel aluminide with a milling liquid and coarse-grained tungsten carbide to form a milling mixture and mixing the milling mixture such that crushed nickel aluminide is formed from the nickel aluminide.

### Claim 33 (depends on 32)

The method of claim 32, wherein the tungsten carbide has a mean particle size of greater than 20 μm.

### Claim 34 (depends on 32)

The method of claim 32, wherein the tungsten carbide is macrocrystalline tungsten carbide, monocrystalline tungsten carbide, or a combination thereof.

### Claim 35 (depends on 32)

The method of claim 32, wherein the preparation step or a subsequent milling step comprises mixing at least the cobalt, at least one alloying constituent, or a combination thereof with the nickel aluminide, the crushed nickel aluminide, or a combination thereof.

### Claim 36 (depends on 32)

The method of claim 32, wherein the milling mixture comprises nickel aluminide in an amount ranging from 8 wt % to 50 wt %

### Claim 37 (depends on 32)

The method of claim 32, further comprising a milling step subsequent to the preparation step, wherein tungsten carbide powder is added to the milling mixture until the milling mixture contains an amount of tungsten carbide ranging from 70 wt % to 95 wt %, and wherein the crushed nickel aluminide is ground into finely-crushed nickel aluminide.

### Claim 38 (depends on 23)

The method of claim 23, wherein the green compact is sintered at a temperature of 1350° C. to 1550° C. using a liquid phase sintering process.

### Claim 39 (depends on 38)

The method of claim 38, wherein the cobalt and the intermetallic phase are at least partially dissolved in each other in a melt during the liquid phase sintering process, wherein, when cooling the compact or during a thermal treatment step subsequent to the sintering process, the intermetallic phase material is formed in the binder phase, and wherein the intermetallic phase material has a structural formula of (M,Y)3(Al,X), wherein M is Ni, Y comprises Co, and X comprises tungsten.

### Claim 40 (depends on 23)

The method of claim 23, wherein at least a portion of the intermetallic phase material has a maximum particle size of 1500 nm and wherein at least a portion of the intermetallic phase material has an L12 crystal structure.

### Claim 41 (depends on 23)

The method of claim 23, wherein the nickel aluminide is present as an intermetallic phase material.

### Claim 42 (depends on 23)

The method of claim 23, further comprising adding Nb, Ti, Ta, Mo, V, Cr, or a combination thereof to the powder mixture, such that the metallic binder material further comprises the Nb, Ti, Ta, Mo, V, Cr or the combination thereof.

### Claim 43 (depends on 42)

The method of claim 42, wherein the Nb, Ti, Ta, Mo, V, Cr or the combination thereof is dissolved in the binder phase.

### Claim 44 (depends on 23)

The method of claim 23, wherein a carbon content of the cemented carbide material is stoichiometric or substoichiometric, and wherein the carbon content in the cemented carbide material ranges from Cstoich (wt %)-0.003*binder content (wt %) to Cstoich (wt %)-0.012*binder content wt %.

### Claim 45 (depends on 23)

The method of claim 23, wherein the binder phase contains 15 at % or less combined Nb, Ti, Ta, Mo, V, and Cr content.

### Claim 46 (depends on 23)

The method of claim 23, wherein the tungsten carbide is present in the cemented carbide material as grains having a mean particle diameter ranging from 1 μm to 15 μm.

### Claim 47 (depends on 23)

The method of claim 23, wherein the binder phase comprises less than 5 wt % Fe.