# US 2025/0276918 A1 · Electrochemical reactor cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0276918 A1
- Document ID: US20250276918A1
- Status: Published application
- Kind: A1
- Application number: 19/210,095
- Filed: 2025-05-16
- Published: 2025-09-04
- Earliest claimed: 2019-03-14
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Chanbasha BASHEER; Hakimu NSUBUGA
- Web page: https://patentgrep.com/patent/US20250276918A1

## CPC

- C02F 1/46109: {Electrodes}
- C02F 1/4672: {by electrooxydation}
- C23C 18/1254: {Sol or sol-gel processing}
- C25B 11/043: Carbon, e.g. diamond or graphene
- C25B 11/057: consisting of a single element or compound
- C25B 11/065: Carbon
- C25B 11/091: consisting of at least one catalytic element and at least one catalytic compound; consisting of two or more catalytic elements or catalytic compounds
- C02F 2001/46142: {Catalytic coating}
- C02F 2001/46147: {Diamond coating}
- C02F 2101/30: Organic compounds
- C02F 2101/305: {Endocrine disruptive agents}
- C02F 2101/308: {Dyes; Colorants; Fluorescent agents}
- C02F 2103/003: {Wastewater from hospitals, laboratories and the like, heavily contaminated by pathogenic microorganisms}
- C02F 2201/4619: Supplying gas to the electrolyte
- C02F 2305/026: Fenton's reagent
- Y02E 60/10: Energy storage using batteries
- Y02W 10/37: using solar energy
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Copper—boron—ferrite (Cu—B—Fe) composites may be prepared and immobilized on graphite electrodes in a silica-based sol-gel, e.g., from rice husks. Different bimetallic loading ratios can produce fast in-situ electrogeneration of reactive oxygen species, H2O2 and ⋅OH, e.g., via droplet flow-assisted heterogeneous electro-Fenton reactor system. Loading ratios of, e.g., 10 to 30 wt. % Fe3+ and 5 to 15% wt. Cu2+, can improve the catalytic activities towards pharmaceutical beta blockers (atenolol and propranolol) degradation in water. Degradation efficiencies of at least 99.9% for both propranolol and atenolol in hospital wastewater were demonstrated. Radicals of ⋅OH in degradation indicate a surface mechanism at inventive cathodes with correlated contributions of iron and copper. Copper and iron can be embedded in porous graphite electrode surface and catalyze the conversion of H2O2 to ⋅OH to enhance the degradation. Inventive cathodes can be stable catalytically after 20 or more cycles under neutral and acidic conditions.

## Claims

### Claim 1 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the cathode is made by a method comprising:
applying a silica-based sol gel composite comprising copper, iron, and boron, onto a sulfonated graphite electrode; and
solidifying the sol gel, to obtain the coating, wherein the coating comprises the iron (III), the copper (II), and the boron immobilized in a silica-based sol-gel.

### Claim at position 2

2-3. (canceled)

### Claim 4 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the silica-based sol gel comprises at least 55 wt. % silica.

### Claim 5 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the sol gel comprises boron in a range of from 0.1 to 10 wt. %, based on total sol gel weight.

### Claim 6 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the silica-based sol gel comprises iron in a range of from 0.1 to 30 wt. %, based on total sol gel weight.

### Claim 7 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the silica-based sol gel comprises copper in a range of from 0.1 to 20 wt. %, based on total sol gel weight.

### Claim 8 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the method of making the cathode further comprises:
preparing the silica-based sol gel by
treating an aqueous silicate solution with iron, copper, and boron; and
gelling the sol.

### Claim 9 (depends on 8)

The electrochemical reactor cell of claim 8, wherein the boron is in the form of boric acid and/or BO33−,
wherein the silicate comprises at least 75 wt. %, based on total silicates, of sodium silicate,
wherein the iron is in the form of an iron (III) salt comprising NO3−, Cl−, Br−, I−, ClO4−, ClO3−, IO3−, SiF62−, and/or SO42−, and/or
wherein the copper is in the form of an copper (II) salt comprising NO3−, Cl−, Br−, I−, ClO4−, ClO3−, IO3−, SiF62−, and/or SO42−.

### Claim 10 (depends on 8)

The electrochemical reactor cell of claim 8, wherein the method of making the cathode, the aqueous silicate solution further comprises a surface directing agent comprising glycerol and cetyltrimethylammonium bromide.

### Claim 11 (depends on 8)

The electrochemical reactor cell of claim 8, wherein the method of making the cathode, the silica-based sol comprises a silica derived from rice husks.

### Claim 12 (depends on 8)

The electrochemical reactor cell of claim 8, wherein the method of making the coated electrode, the copper, iron, and boron are provided in a single solution, and
wherein the single solution comprises 1 to 5 M nitric acid, 5 to 30 wt. % iron, 5 to 15 wt. % copper, and 2.5 to 7.5 wt. % boron.

### Claim 13 (depends on 8)

The electrochemical reactor cell of claim 8, wherein the method of making the coated electrode further comprises:
gelling by adding a mineral acid to the silicate solution during and/or after contacting the silicate solution with the iron, copper, and boron.

### Claim 14

An electrochemical reactor cell, comprising:
a reactor vessel,
a cathode,
an anode, and
a gas supply conduit;
wherein the cathode is a coated electrode, comprising:
a sulfonated graphite slab having a thickness in a range of from 1 to 10 mm;
a coating, directly contacting the slab, comprising a silica-based sol gel, 0.5 to 30 wt. % iron (III), 0.5 to 10 wt. % copper (II), and 0.5 to 5 wt. % boron,
wherein the reactor vessel is configured to contain a liquid, the cathode and anode are disposed in the liquid and the gas conduit is configured to supply an oxygen-containing gas flow to the reactor vessel.

### Claim 15 (depends on 14)

The electrochemical reactor cell of claim 14, wherein the coating comprises at least 5 wt. % iron (III), at least 2.5 wt. % copper (II), and at least 1.5 wt. % boron.

### Claim at position 15

16-20. (canceled)