# US 2025/0270672 A1 · Method for recovering precursor metal for secondary cell cathode material using synergistic solvent extraction applied with extractant degradation preventing technology

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0270672 A1
- Document ID: US20250270672A1
- Status: Published application
- Kind: A1
- Application number: 18/285,840
- Filed: 2023-06-01
- Published: 2025-08-28
- Earliest claimed: 2022-11-14
- Assignees: Cis Chemical Co., Ltd.
- Applicants: Cis Chemical Co., Ltd.
- Inventors: Sung Oh LEE; Chi Jung OH; Jeon Woong AN; Youn Kyu YI
- Web page: https://patentgrep.com/patent/US20250270672A1

## CPC

- C22B 3/30: Oximes
- C22B 7/007: {by acid leaching}
- C01G 3/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- C01G 3/10: Sulfates
- C22B 3/02: Apparatus therefor
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/404: {of organic acids and oximes}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 15/0071: {containing sulfur}
- C22B 15/0089: {by chemical methods}
- C22B 19/22: {with leaching with acids}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- C22B 47/00: Obtaining manganese
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a method for recovering a precursor metal for secondary cell cathode material using synergistic solvent extraction applied with extractant degradation preventing technology including: (a) leaching a low grade MHP and sulfuric acid by high temperature and high pressure oxidation reaction; (b) separating a solution leached by the oxidation reaction and precipitant of an impurity containing iron (Fe); (c) recovering copper as copper sulfate solution by solvent extraction from the leached solution of (b); (d) precipitating and removing some impurities by injecting a neutralizing agent into a raffinate after solvent extraction of cooper in (c); and (e) recovering zinc, cobalt, and nickel from a solution from which some impurities are removed in (d) by means of the synergetic solvent extraction (SSX) to be selectively separated as a raffinate containing manganese, calcium, and magnesium.

## Claims

### Claim 1

A method for recovering a precursor metal for secondary cell cathode material using synergistic solvent extraction applied with an extractant degradation preventing technology, comprising:
(a) a step of leaching a low grade MHP with sulfuric acid by high temperature and high-pressure oxidation reaction;
(b) a step of separating a solution leached by the oxidation reaction and precipitant of an impurity containing iron (Fe);
(c) a step of recovering copper as a copper sulfate solution by solvent extraction from the leached solution of the step (b);
(d) a step of precipitating and removing some impurities by injecting a neutralizing agent into a raffinate after solvent extraction of cooper in the step (c); and
(e) a step of recovering zinc (Zn), cobalt (Co), and nickel (Ni) from a solution from which some impurities are removed in the step (d) by means of the synergetic solvent extraction (SSX) to be selectively separated as a raffinate containing manganese (Mn), calcium (Ca), and magnesium (Mg).

### Claim 2 (depends on 1)

The method according to claim 1, wherein in the step (a), an autoclave is used.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in the solvent extraction in the step (c), a mixture of kerosene which is a diluent and 2-Hydroxy-5-Nonylacetophenone Oxime and 4-Nonylphenol extractants is used.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the neutralizing agent in the step (d) is any one of caustic soda or soda ash and is added to make a pH of the solution 3 to 7.

### Claim 5 (depends on 1)