- Assignees: Sichuan Huiwei Rongda Technology Co., Ltd
- Applicants: Sichuan Huiwei Rongda Technology Co., Ltd.
- Inventors: Wei ZHANG; Xiaohui LIU
- Web page: https://patentgrep.com/patent/US20250270670A1

## CPC

- C01D 5/14: Preparation of sulfites (C01D5/04 takes precedence)
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C01G 49/14: Sulfates {(C01G49/0018 takes precedence)}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 7/04: Working-up slag
- Y02P 10/20: Recycling
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a method for leaching iron element from a sulfate slag. A sulfur dioxide-containing gas is introduced into a mixed system obtained after mixing the sulfate slag with dilute sulfuric acid, such that ferric sulfate generated by a reaction of the sulfate slag and the dilute sulfuric acid is quickly reduced into ferrous sulfate by sulfur dioxide.

## Claims

### Claim 1

A method for leaching iron element from a sulfate slag, comprising the following steps:
mixing the sulfate slag with dilute sulfuric acid to obtain a mixed system, and introducing a sulfur dioxide-containing gas into the mixed system under stirring at a temperature of 20° C. to 100° C., and conducting reduction leaching;
wherein the dilute sulfuric acid has a mass concentration of 5% to 45%.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a mass content of iron in the sulfate slag is not less than 25%.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a mass ratio of the sulfate slag to the dilute sulfuric acid is in a range of 1:1.5-30.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the stirring is conducted at a speed of 100 r/min to 300 r/min.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the sulfur dioxide-containing gas is introduced in an amount of 1 L/min to 1,000 L/min.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the sulfur dioxide-containing gas comprises one selected from the group consisting of a pure sulfur dioxide gas and a sulfur dioxide-containing tail gas.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the reduction leaching is conducted for 15 min to 180 min.

### Claim 8 (depends on 1)

The method according to claim 1, wherein during the reduction leaching, an unreacted sulfur dioxide-containing gas escapes in a form of a tail gas;
the tail gas is absorbed by a sodium hydroxide solution to form a sodium sulfite solution; and
the sodium sulfite solution is subjected to concentration and crystallization in sequence to obtain sodium sulfite.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising, after the reduction leaching, subjecting a resulting system to filtration to obtain a filter residue and a ferrous sulfate solution as a filtrate; and subjecting the ferrous sulfate solution to concentration and crystallization in sequence to obtain a ferrous sulfate crystal.

### Claim 10 (depends on 2)

The method according to claim 2, wherein a mass ratio of the sulfate slag to the dilute sulfuric acid is in a range of 1:1.5-30.

### Claim 11 (depends on 5)