- Inventors: HOU-REN CHEN; MING-ZHOU CHUANG; HSIN-HUNG CHEN
- Web page: https://patentgrep.com/patent/US20250249651A1

## CPC

- B31B 50/64: by applying heat or pressure, e.g. by welding (to unite areas where adhesives are applied B31B50/62)
- B31B 50/14: Cutting, e.g. perforating, punching, slitting or trimming (cutting window openings B31B50/83)
- B31B 50/28: around mandrels, e.g. for forming bottoms
- B31B 50/66: by high-frequency electric heating
- B31B 50/747: {Coating or impregnating blanks or webs}
- B31B 2105/0022: {Making boxes from tubular webs or blanks, e.g. with separate bottoms, including tube or bottom forming operations}
- B31B 2110/10: having a cross section of varying size or shape, e.g. conical or pyramidal
- B31B 2110/20: having a curved cross section, e.g. circular
- B31B 2120/10: provided with covers, e.g. lids
- B31B 2120/40: lined or internally reinforced
- B31B: MAKING CONTAINERS OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUS TO PAPER (making wound articles, e.g. wound tubes, B31C; combined making and filling B65B)

## Abstract

A method for manufacturing a paper container, including following steps: preparing a paper material; applying a covering layer to at least one surface of the paper material to form a base material, wherein a material of the covering layer is selected from a group including acrylic acid; cutting the base material to form a first sheet and a second sheet; bending and connecting the first sheet to form a barrel body; and connecting the second sheet with the barrel body by ultrasonic heating and pressing. The barrel body is circumferentially disposed around the second sheet, and surfaces of the barrel body and the second sheet facing each other respectively have the covering layer applied thereto. The paper container produced by the present invention is easy to recycle and manufacture, and is environmentally friendly and resistant to leakage.

## Claims

### Claim 1

A method for manufacturing a paper container, including:
preparing a paper material;
applying a covering layer to at least one surface of the paper material to form a base material, wherein a material of the covering layer is selected from a group including acrylic acid;
cutting the base material to form a first sheet and a second sheet;
bending and connecting the first sheet to form a barrel body; and
connecting the second sheet with the barrel body by ultrasonic heating and pressing, wherein the barrel body is circumferentially disposed around the second sheet, and surfaces of the barrel body and the second sheet facing each other respectively have the covering layer applied thereto; said covering layers located between the barrel body and the second sheet are at least partially fused together by ultrasonic heating, while the barrel body and the second sheet are being embossed and pressed together.

### Claim 2 (depends on 1)

The method for manufacturing the paper container of claim 1, wherein the material of the covering layer further includes at least one of ethylene propylene copolymer (EPP), ethylene acrylic acid copolymer emulsion (EAA), polypropylene carbonate (PPC), polybutylene adipate terephthalate (PBAT), polybutylene succinate polyester (PBS), polylactic acid (PLA), polyurethane (PU), polyhydroxyalkanoate (PHA), polyethylene terephthalate (PET) and polyethylene terephthalate-1, 4-cyclohexanedimethanol ester (PETG).

### Claim 3 (depends on 1)

The method for manufacturing the paper container of claim 1, wherein the material of the covering layer includes a water-based acrylic acid resin, and the covering layer is distributed on the paper material 1 with a weight of 1 to 20 grams per square meter (GSM).

### Claim 4 (depends on 1)

The method for manufacturing the paper container of claim 1, further including following steps of: bending and folding the second sheet to formed an annular flange, positioning the annular flange on an inner peripheral surface of the barrel body in a predetermined position, and preheating at least one of the barrel body and the annular flange.

### Claim 5 (depends on 4)

The method for manufacturing the paper container of claim 4, wherein a preheating temperature is between 140° C. and 400° C.

### Claim 6 (depends on 1)

The method for manufacturing the paper container of claim 1, wherein the first sheet is cut into a fan shape, and the barrel body and the second sheet are connected to form a cup body.

### Claim 7 (depends on 1)

The method for manufacturing the paper container of claim 1, wherein the first sheet is cut into a rectangular shape, and the barrel body and the second sheet are connected to form a cup lid.

### Claim 8 (depends on 1)

The method for manufacturing the paper container of claim 1, wherein a glass transition temperature (Tg) of the material of the covering layer is higher than or equal to 30° C.

### Claim 9 (depends on 1)