# US 2025/0243602 A1 · Process for producing crystals, particularly polycrystals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0243602 A1
- Document ID: US20250243602A1
- Status: Published application
- Kind: A1
- Application number: 19/078,597
- Filed: 2025-03-13
- Published: 2025-07-31
- Earliest claimed: 2024-01-05
- Inventors: Volodymyr TARANYUK; Vadim GAYSHAN
- Web page: https://patentgrep.com/patent/US20250243602A1

## CPC

- C30B 28/04: from liquids
- C30B 11/003: {Heating or cooling of the melt or the crystallised material}
- C30B 29/12: Halides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The invention is a process for producing crystals (polycrystals) that comprises steps of: evacuating, melting a raw material in a container by means of a resistance heater to form a skull layer of 5-10 mm, crystallizing a melt of the raw material, annealing and cooling the crystal, separating the skull layer. The container is coated inside with a metal foil having a thickness of 0.04-0.15 mm; the steps of melting the raw material, crystallizing, annealing and cooling the crystal are performed in a double-layered shell composed of the metal foil and the skull layer; after the crystallization step, the crystal is annealed in a separate annealing furnace. The invention allows to: prevent crystal cracking, produce the crystal without any internal stresses; reduce the raw material mass consumed to form the skull layer; increase the size and the weight of the produced crystal; reduce energy consumption.

## Claims

### Claim 1

A process for producing crystals, the process comprises steps of loading a raw material into a container, placing the container loaded with the raw material into a cooling vacuum chamber that is evacuated to forevacuum, heating and melting the raw material in a skull to form an optimal thickness of a skull layer by means of a resistance heater positioned above the container and in parallel to a melt surface of the raw material, the resistance heater has a working heating surface having an area that is less than an area of an exposed upper part of the container and it has parameters that allow to produce the skull layer along inner surfaces of walls and bottom of the container having a thickness of 5-10 mm, further directional crystallizing the melt of the raw material by reducing a temperature of the resistance heater according to a given program, annealing the produced crystal, cooling the annealed crystal, separating the skull layer, wherein the process comprises, before the step of loading the container with the raw material, coating an inner surface of the container for growing the crystal with a protective metal foil layer having a thickness of 0.04-0.15 mm, and the steps of producing the melt of the raw material, directional crystallizing, annealing and cooling the annealed crystal are performed in a double-layered protective shell that is formed along the inner surfaces of the walls and the bottom of the container by the protective metal foil layer and the skull layer of the raw material, and the step of melting the raw material comprises adjusting a temperature T1 of the resistance heater based on controlling measurement values of a temperature T2 of a side wall of the container and a temperature T3 of the bottom of the container, while correspondingly fixing the temperature T1 of the resistance heater immediately after either one of the temperatures T2 or T3 or both temperatures T2 and T3 simultaneously reached a value that falls within an interval of values that corresponds to a temperature control criterion Ctc that is 0.76-0.8 of a crystal melting temperature value T4 of the crystal being grown, namely, Ctc=(0.76×T4):(0.8×T4), and after the step of directional crystallizing is completed, the step of annealing the crystal is performed in a separate annealing furnace at a temperature T5 having a value of 0.8-0.9 of the crystal melting temperature value T4 of the crystal being grown.

### Claim 2 (depends on 1)

The process according to claim 1, wherein an aluminum foil layer having an aluminum content of at least 98.5% is used as a metal component of the double-layered protective shell.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the step of melting the raw material comprises controlling the temperature measurement value T2 of one of the side walls of the container that is performed in an upper external middle zone of the side wall of the container, while controlling the temperature measurement value T3 of the bottom of the container is performed in a central external zone of the bottom of the container.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the further melting the raw material for formation and maintaining the optimal thickness of the skull layer within 5-10 mm by adjusting the temperature T1 of the resistance heater based on controlling the temperature measurement values T2 and T3 according to the interval of values of the temperature control criterion Ctc=(0.76×T4):(0.8×T4) takes place for 4-8 hours after pre-heating and pre-melting the raw material, and then the produced melt of the raw material having the formed skull layer is maintained for 1-2 hours.

### Claim 5 (depends on 1)

The process according to claim 1, wherein an inner working volume of the separate annealing furnace is heated to the temperature T5 before the container with the crystal is loaded therein, and the crystal is annealed at this temperature for 1-5 hours.

### Claim 6 (depends on 1)

The process according to claim 1, wherein after the steps of annealing and cooling the crystal, the double-layered protective shell is separated from the annealed and cooled crystal successively, namely, firstly, the aluminum foil layer is separated from the skull layer, and then, the skull layer is separated from the crystal.