# US 2025/0233201 A1 · Sulfide solid electrolyte glass ceramic and manufacturing method for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0233201 A1
- Document ID: US20250233201A1
- Status: Published application
- Kind: A1
- Application number: 18/851,103
- Filed: 2023-03-30
- Published: 2025-07-17
- Earliest claimed: 2022-03-31
- Assignees: Idemitsu Kosan Co., Ltd.
- Applicants: Idemitsu Kosan Co.,Ltd.
- Inventors: Kota TERAI; Yuji OKAMOTO; Kazuaki YANAGI
- Web page: https://patentgrep.com/patent/US20250233201A1

## CPC

- C03C 3/323: {containing halogen, e.g. chalcohalide glasses}
- H01M 10/0562: Solid materials
- C01B 25/14: Sulfur, selenium, or tellurium compounds of phosphorus
- C03C 4/14: for electro-conductive glass
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- C03C 10/16: Halogen containing crystalline phase
- H01B 1/06: mainly consisting of other non-metallic substances
- H01B 1/10: sulfides
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a sulfide solid electrolyte glass ceramic containing a lithium atom, a sulfur atom, a phosphorus atom, and a halogen atom and having peaks at diffraction angles (2θ) of 20.2° and 29.3° in X-ray diffractometry using CuKα line. Due to an intensity ratio (PA/PB) of a peak intensity (PA) of the peak appearing at 2θ=20.2° to a peak intensity (PB) of the peak appearing at 2θ=29.3° made into more than 1.0, the sulfide solid electrolyte glass ceramic has a high ionic conductivity and has an increased water resistance. A method for producing the sulfide solid electrolyte glass ceramic is also provided.

## Claims

### Claim 1

A sulfide solid electrolyte glass ceramic, comprising: a lithium atom, a sulfur atom, a phosphorus atom, and a halogen atom,
wherein the sulfide solid electrolyte glass ceramic has
peaks at diffraction angles (2θ) of 20.2° and 29.3° in X-ray diffractometry using CuKα line, an intensity ratio (PA/PB) of a peak intensity (PA) of a peak appearing at 2θ=20.2° to a peak intensity (PB) of a peak appearing at 2θ=29.3° being more than 1.0, and
a crystallite diameter of 30 nm or more.

### Claim 2 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, wherein an intensity ratio (IA/IB) of a peak area intensity (IA) of the peak appearing at 2θ=20.2° to a peak area intensity (IB) of the peak appearing at 2θ-29.3° is 0.78 or more.

### Claim 3 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, further having a peak at 2θ=23.6°.

### Claim 4 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, comprising an iodine atom as the halogen atom.

### Claim 5 (depends on 4)

The sulfide solid electrolyte glass ceramic according to claim 4, further comprising a bromine atom as the halogen atom.

### Claim 6 (depends on 5)

The sulfide solid electrolyte glass ceramic according to claim 5, wherein a molar content of the bromine atom MBr and a molar content of the iodine atom MI in the sulfide solid electrolyte glass ceramic satisfy a relation of MBr/MI≤1.00.

### Claim 7 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, wherein a P2S64− phosphorous ratio determined by a solid 31P-NMR measurement is 7.5% by mole or less.

### Claim 8 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, wherein (I1Li2S/I1P2S5), which is a ratio of a molar fraction of Li2S to a molar fraction of P2S5 calculated from contents of the elements in raw materials, is 2.60 or more and 3.30 or less.

### Claim 9 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, wherein (I2Li2S/I2P2S5), which is a ratio of a molar fraction of Li2S to a molar fraction of P2S5 measured by using an inductively coupled plasma (ICP) emission spectrophotometer, is 2.60 or more and 3.30 or less.

### Claim 10 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, wherein (lithium atom:phosphorus atom:sulfur atom: halogen atom), which represents a molar ratio of a content of the lithium atom, a content of the phosphorus atom, a content of the sulfur atom, and a content of the halogen atom, is (3.20 to 3.70):(0.70 to 1.30):(3.00 to 5.00):(0.20 to 0.70).

### Claim 11 (depends on 1)

The sulfide solid electrolyte glass ceramic according to claim 1, comprising a thio-LISICON Region II-type crystal structure.

### Claim 12 (depends on 1)

A method for producing the sulfide solid electrolyte glass ceramic according to claim 1, the method comprising:
treating lithium sulfide (Li2S) and phosphorus sulfide (P2S5) by at least one process selected from the group consisting of stirring, mixing, and pulverization to produce a solid electrolyte (A), and
treating the solid electrolyte (A) and a lithium halide by at least one process selected from the group consisting of stirring, mixing, and pulverization to produce a solid electrolyte (B).

### Claim 13 (depends on 12)

The method according to claim 12, further comprising:
heating the solid electrolyte (A).

### Claim 14 (depends on 12)

The method according to claim 12, further comprising:
heating the solid electrolyte (B).

### Claim 15 (depends on 12)

The method according to claim 12, wherein the solid electrolyte (B) has a P2S64− phosphorous ratio determined by a solid 31P-NMR measurement of 15.0% by mole or less.

### Claim 16 (depends on 1)

An electrode mixture material, comprising:
the sulfide solid electrolyte glass ceramic according to claim 1, and
an electrode active material.

### Claim 17 (depends on 1)

A lithium-ion battery, comprising at least one of
the sulfide solid electrolyte glass ceramic according to claim 1 and
an electrode mixture material containing the sulfide solid electrolyte glass ceramic and an electrode active material.