# US 2025/0233196 A1 · Cell and lithium-ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0233196 A1
- Document ID: US20250233196A1
- Status: Published application
- Kind: A1
- Application number: 19/171,364
- Filed: 2025-04-07
- Published: 2025-07-17
- Earliest claimed: 2023-09-07
- Assignees: Eve Power Co., Ltd.
- Applicants: Eve Power Co., Ltd.
- Inventors: MENG CHEN; HAO WU; JIAXIN ZHU; FANFEN LIU; DINGDING YUAN
- Web page: https://patentgrep.com/patent/US20250233196A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0583: of accumulators with folded construction elements except wound ones, i.e. folded positive or negative electrodes or separators, e.g. with "Z"-shaped electrodes or separators
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A cell includes a jellyroll A and a jellyroll B. The jellyroll A is formed by laminating a first positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially; the jellyroll B comprises a first portion of laminates and a second portion of laminates laminated on the first portion of laminates. The first portion of laminates is formed by laminating a first positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially; the second portion of laminates is formed by laminating a ternary positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially.

## Claims

### Claim 1

A cell, comprising a jellyroll A and a jellyroll B, wherein,
the jellyroll A is formed by laminating a first positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially; the jellyroll B comprises a first portion of laminates and a second portion of laminates laminated on the first portion of laminates;
the first portion of laminates is formed by laminating a first positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially; the second portion of laminates is formed by laminating a ternary positive-electrode sheet, a separator, a negative-electrode sheet, and another separator sequentially;
the first positive-electrode sheet comprises a first active layer, the first active layer comprises a first active material, the first active material is any one of: lithium iron phosphate and lithium manganese iron phosphate.

### Claim 2 (depends on 1)

The cell according to claim 1, wherein, a thickness of the first active layer is in a range of 40 μm to 120 μm.

### Claim 3 (depends on 1)

The cell according to claim 1, wherein a particle size D50 of the first active material is in a range of 0.5 μm to 1 μm.

### Claim 4 (depends on 1)

The cell according to claim 1, wherein the ternary positive-electrode sheet comprises a ternary active layer, and a thickness of the ternary active layer is in a range of 30 μm to 100 μm.

### Claim 5 (depends on 4)

The cell according to claim 4, wherein the ternary active layer comprises a ternary material, and a particle size D50 of the ternary material is in a range of 3 μm to 4 μm.

### Claim 6 (depends on 1)

The cell according to claim 1, wherein in the jellyroll B, a first negative-electrode active layer is arranged on a surface of the negative-electrode sheet near the first positive-electrode sheet, a thickness of the first negative-electrode active layer is in a range of 30 μm to 60 μm; and a second negative-electrode active layer is arranged on a surface of the negative-electrode sheet near the ternary positive-electrode sheet, and a thickness of the second negative-electrode active layer is in a range of 40 μm to 70 μm.

### Claim 7 (depends on 1)

The cell according to claim 1, wherein in the jellyroll B, a ratio of the number of first positive-electrode sheets to the number of ternary positive-electrode sheets is in a range of 1:3 to 2:3.

### Claim 8 (depends on 7)

The cell according to claim 7, wherein in the jellyroll B, the ratio of the number of first positive-electrode sheets to the number of ternary positive-electrode sheets is in a range of 1:2.

### Claim 9 (depends on 1)

The cell according to claim 1, wherein a ratio of the number of first positive-electrode sheets in the jellyroll A to the number of first positive-electrode sheets in the jellyroll B is in a range of 1:3 to 2:3.

### Claim 10 (depends on 1)

A lithium-ion battery, comprising the cell according to claim 1.

### Claim 11

A cell, comprising at least one jellyroll, wherein the at least one jellyroll comprises a plurality of first positive-electrode sheets, a plurality of negative-electrode sheets, a plurality of ternary positive-electrode sheets, and a plurality of separators;
each of the plurality of first positive-electrode sheets is arranged with a first coating formed by a positive-electrode active material; a thickness of the first coating is in a range of 40 μm to 120 μm; the positive-electrode active material is any one of: lithium nickel cobalt manganate and lithium nickel cobalt aluminate;
each of the plurality of ternary positive-electrode sheets is arranged with a ternary coating formed by a ternary active material; a thickness of the ternary coating is in a range of 30 μm to 100 μm.

### Claim 12 (depends on 11)

The cell according to claim 11, wherein one of the at least one jellyroll comprises a plurality of repetitive units that are sequentially laminated; and
one of the plurality of repetitive units comprises a respective one of the plurality of first positive-electrode sheets, a respective one of the plurality of separators, a respective one of the plurality of negative-electrode sheets, another respective one of the plurality of separators, a respective one of the plurality of ternary positive-electrode sheets, another respective one of the plurality of separators, another respective one of the plurality of negative-electrode sheets, and another respective one of the plurality of separators are sequentially laminated.

### Claim 13 (depends on 12)

The cell according to claim 12, wherein the number of the plurality of repetitive units in one of the at least one jellyroll is 2 to 30.

### Claim 14 (depends on 11)

The cell according to claim 11, wherein one of the at least one jellyroll comprises a first repetitive set and a second repetitive set laminated on the first repetitive set;
the first repetitive set is formed by laminating a respective one of the plurality of first positive-electrode sheets, a respective one of the plurality of separators, a respective one of the plurality of negative-electrode sheets, and another respective one of the plurality of separators sequentially; the second repetitive set is formed by laminating a respective one of the plurality of ternary positive-electrode sheets, a respective one of the plurality of separators, a respective one of the plurality of negative-electrode sheets, and another respective one of the plurality of separators sequentially.

### Claim 15 (depends on 14)

The cell according to claim 14, wherein the number of first positive-electrode sheets in the first repetitive set is equal to the number of ternary positive-electrode sheets in the second repetitive set.

### Claim 16 (depends on 11)

The cell according to claim 11, wherein, for each of the plurality of negative-electrode sheets, a first graphite coating is arranged on a surface of the negative-electrode sheet near a respective one of the plurality of first positive-electrode sheets.

### Claim 17 (depends on 16)

The cell according to claim 16, a thickness of the first graphite coating is in a range of 40 μm to 80 μm.

### Claim 18 (depends on 16)

The cell according to claim 16, wherein, for each of the plurality of negative-electrode sheets, a second graphite coating is arranged on a surface of the negative-electrode sheet near a respective one of the plurality of ternary positive-electrode sheets.

### Claim 19 (depends on 18)

The cell according to claim 18, wherein a thickness of the second graphite coating is in a range of 50 μm to 100 μm.

### Claim 20 (depends on 11)

A lithium-ion battery, comprising a battery housing and the cell according to claim 11 arranged inside the battery housing, wherein the number of the at least one jellyroll in the cell is two.