# US 2025/0230528 A1 · High-strength heat-resistant aluminum-based composite material and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0230528 A1
- Document ID: US20250230528A1
- Status: Published application
- Kind: A1
- Application number: 18/703,207
- Filed: 2021-11-08
- Published: 2025-07-17
- Earliest claimed: 2021-10-29
- Assignees: Hunan Wenchang New Material Technology Co.,Ltd.
- Applicants: Hunan Wenchang New Material Technology Co.,Ltd.
- Inventors: Jun XU; Zhenlin ZHANG; Xianqing LI; Min HE
- Web page: https://patentgrep.com/patent/US20250230528A1

## CPC

- C22C 32/0063: {based on SiC}
- C22C 1/026: {Alloys based on aluminium}
- C22C 1/0416: {Aluminium-based alloys}
- C22C 1/1005: {Pretreatment of the non-metallic additives (pretreatment of non-metallic fibres C22C47/02)}
- C22C 1/1047: {by mixing and casting liquid metal matrix composites}
- C22C 1/1094: {comprising an after-treatment}
- C22C 21/12: with copper as the next major constituent
- C22F 1/04: of aluminium or alloys based thereon
- F16D 65/125: {characterised by the material used for the disc body}
- F16D 2200/003: Light metals, e.g. aluminium
- F16D 2200/006: containing fibres or particles
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES

## Abstract

An aluminum-based composite material and a brake disc made of the composite material are provided. The material includes a base material and a reinforcing phase. The base material includes the following components in mass percentage: 4.0-7.0% of Cu, 0.4-1.2% of Mg, and 0.1-0.8% of Ag, with the balance being Al. The reinforcing phase can be SiC particles having a volume percentage of 10-40%.

## Claims

### Claim 1

An aluminum matrix composite material, comprising:
a matrix material, which comprises following components by mass percentage: 4.0%-7.0% of Cu, 0.4%-1.2% of Mg, 0.1%-0.8% of Ag, and balance being Al; and
a reinforcing phase, which is SiC particles with a volume percentage of 10%-40%.

### Claim 2 (depends on 1)

The aluminum matrix composite material according to claim 1, further comprising 0.05%-0.5% of Mn, 0.05%-0.5% of Ti, and 0.05%-0.5% of Zr by mass percentage.

### Claim 3 (depends on 2)

The aluminum matrix composite material according to claim 2, wherein the content of Mn is 0.05%-0.4%, the content of Ti is 0.05%-0.3%, and the content of Zr is 0.05%-0.2%.

### Claim 4 (depends on 1)

The aluminum matrix composite material according to claim 1, wherein the content of Ag is 0.2%-0.6%, the content of Cu is 4.5%-6.5%, and the content of Mg is 0.6%-1.0%.

### Claim 5 (depends on 1)

The aluminum matrix composite material according to claim 1, wherein a size of the SiC particle is 5 μm-50 μm.

### Claim 6 (depends on 1)

A method for preparing the aluminum matrix composite material according to claim 1, comprising:
melting: mixing pure aluminum and aluminum-copper alloy according to a set mass percentage content of each metal element in the matrix material, heating to melt all the metals, adding pure magnesium and pure silver, and obtaining a first metal melt after all the pure magnesium and pure silver have melted;
refining: slagging-off the first metal melt obtained, adding a refining agent and stirring, and obtaining a second metal melt after dredging the slags;
stirring the second metal melt obtained and controlling the temperature of the second metal melt to be 650° C.-700° C.;
adding SiC particles to the second metal melt at the temperature of 650° C.-700° C. under stirring;
after the addition of SiC particles is completed, lowering the temperature of the second metal melt to make the second metal melt in a semi-solid state, stirring and obtaining an aluminum matrix composite material melt;
after heating the aluminum matrix composite material melt obtained, casting the aluminum matrix composite material melt into a preheated casting mold, and obtaining an aluminum matrix composite material casting; and
performing heat treatment on the aluminum matrix composite material casting obtained.

### Claim 7 (depends on 6)

The method according to claim 6, wherein in the melting step, aluminum manganese alloys, aluminum titanium alloys, aluminum zirconium alloys are mixed with pure aluminum and aluminum copper alloys.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the SiC particles are pre-treated before being used; the pre-treatment comprises ultrasonic cleaning, drying and sieving for the SiC particles, and the SiC particles are preheated to 650° C.-700° C.

### Claim 9 (depends on 6)

The method according to claim 6, wherein in the step of preparing the aluminum matrix composite material melt, the temperature of the second metal melt is lowered to 580° C.-650° C. to make the second metal melt in the semi-solid state; the stirring speed is above 800 rpm, and the stirring time is 15 minutes-30 minutes.

### Claim 10 (depends on 1)

A brake disc, which is prepared from the aluminum matrix composite material according to claim 1.

### Claim 11 (depends on 6)

A brake disc, which is prepared from an aluminum matrix composite material obtained using the method according to claim 6.