# US 2025/0221012 A1 · Method of forming semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0221012 A1
- Document ID: US20250221012A1
- Status: Published application
- Kind: A1
- Application number: 18/398,702
- Filed: 2023-12-28
- Published: 2025-07-03
- Earliest claimed: 2023-12-28
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Shao-Tse HUANG; Jin-Hao JHANG; Wei-De HO; Han-Yu LIN
- Web page: https://patentgrep.com/patent/US20250221012A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/0186: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 84/85: Complementary IGFETs, e.g. CMOS
- H10D 88/00: Three-dimensional [3D] integrated devices
- H10D 88/01: {Manufacture or treatment}
- H10P 95/06: {Planarisation of inorganic insulating materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes a number of operations. A bottom transistor and a top transistor overlapping the bottom transistor are formed. A vertical local interconnect (VLI) structure is formed and electrically connects source/drain regions of the bottom transistor and the top transistor. A hard mask layer is formed over the VLI structure, wherein the hard mask layer includes a bottom nitride layer, a top nitride layer and an amorphous semiconductive layer directly between the bottom nitride layer and the top nitride layer. The hard mask layer is patterned. A trench is formed in the VLI structure. An isolation structure is formed in the trench. A first polishing process is performed to the isolation structure and the hard mask layer, wherein the first polishing process stops the amorphous semiconductive layer. A second polish process is performed to the isolation structure, the bottom nitride layer and the amorphous semiconductive layer.

## Claims

### Claim 1

A method comprising:
forming a bottom transistor and a top transistor overlapping the bottom transistor;
forming a vertical local interconnect (VLI) structure electrically connecting a source/drain region of the bottom transistor and a source/drain region of the top transistor;
forming a hard mask layer over the VLI structure, wherein the hard mask layer comprises a bottom nitride layer, a top nitride layer and an amorphous semiconductive layer directly between the bottom nitride layer and the top nitride layer;
patterning the hard mask layer;
forming a trench in the VLI structure;
forming an isolation structure in the trench;
performing a first polishing process to the isolation structure and the hard mask layer, wherein the first polishing process stops the amorphous semiconductive layer; and
performing a second polish process to the isolation structure, the bottom nitride layer and the amorphous semiconductive layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein before the first polishing process is performed, a thickness of the isolation structure and the top nitride layer higher than the amorphous semiconductive layer is greater than a thickness of the amorphous semiconductive layer and the bottom nitride layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first polishing process polishes the top nitride layer at a first polish rate, and polishes the amorphous semiconductive layer at second polish rate, and the first polish rate is different from the second polish rate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the top nitride layer and the bottom nitride layer comprise silicon nitride.

### Claim 5 (depends on 1)

The method of claim 1, wherein the amorphous semiconductive layer comprises amorphous semiconductive silicon.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming the hard mask layer further comprises forming an oxide layer over the top nitride layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein a thickness of the oxide layer is greater than a thickness of any of the top nitride layer, the amorphous semiconductive layer and the bottom nitride layer after the hard mask layer is formed.

### Claim 8 (depends on 6)

The method of claim 6, wherein the isolation structure is formed and extends from a top surface of the oxide layer into the trench before the first polish process is performed.

### Claim 9 (depends on 1)

The method of claim 1, wherein forming the isolation structure comprises forming a liner through the amorphous semiconductive layer of the hard mask layer and in the trench of the VLI structure.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first polishing process has a first polish selectivity between the top nitride layer and the amorphous semiconductive layer, the second polishing process has a second polish selectivity between the bottom nitride layer and the amorphous semiconductive layer, and the second polish selectivity is less than the first polish selectivity.

### Claim 11

A method, comprising:
forming a first transistor and a second transistor over the first transistor;
forming a first hard mask layer over the second transistor, wherein the first hard mask layer comprises a bottom nitride layer, a top nitride layer and an amorphous semiconductive layer directly between the bottom nitride layer and the top nitride layer;
patterning the first hard mask layer;
forming a first trench extending through gate structures of the first transistor and the second transistor;
forming a vertical local interconnect (VLI) structure in the first trench, the VLI structure electrically connecting a source/drain region of the first transistor to a source/drain region of the second transistor;
performing a first polishing process to the VLI structure and the first hard mask layer, wherein the first polishing process stops at a level of the amorphous semiconductive layer; and
after the first polishing process stops, performing a second polish process to the VLI structure, the bottom nitride layer and the amorphous semiconductive layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein a thickness of the top nitride layer is greater than a thickness of the amorphous semiconductive layer and the bottom nitride layer.

### Claim 13 (depends on 11)

The method of claim 11, wherein the top nitride layer and the bottom nitride layer comprise silicon nitride.

### Claim 14 (depends on 11)

The method of claim 11, wherein the amorphous semiconductive layer comprises amorphous semiconductive silicon.

### Claim 15 (depends on 11)

The method of claim 11, wherein forming the VLI structure comprises forming a nitride liner through the top nitride layer, the amorphous semiconductive layer and the bottom nitride layer of the first hard mask layer.

### Claim 16 (depends on 11)

The method of claim 11, further comprising:
forming a second hard mask layer over the VLI structure, wherein the second hard mask layer comprises a bottom nitride layer, a top nitride layer and an amorphous semiconductive layer directly between the bottom nitride layer and the top nitride layer;
patterning the second hard mask layer;
forming a second trench in the VLI structure;
forming an isolation structure in the second trench; and
performing a third polishing process to the isolation structure and the second hard mask layer.

### Claim 17

A method comprising:
forming a first transistor and a second transistor, wherein the second transistor overlaps the first transistor;
forming a hard mask layer over the second transistor, comprising:
forming a bottom mask layer;
forming an oxygen-free polish stop layer over the bottom mask layer;
forming a protective layer over the oxygen-free polish stop layer; and
forming an oxide layer over the protective layer;
patterning the hard mask layer;
forming a trench in gate structures of the first and second transistors;
forming an oxygen-free liner in the trench;
forming an oxide insulating layer over the oxygen-free liner; and
performing a polishing process to the hard mask, the oxygen-free liner and the oxide insulating layer, wherein the polishing process stops at a level of the oxygen-free polish stop layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the hard mask layer comprises an oxide-free material.

### Claim 19 (depends on 17)

The method of claim 17, wherein the polish process has a first polish rate on the protective layer and a second polish rate on the oxygen-free polish stop layer, the first polish rate is different from the second polish rate.

### Claim 20 (depends on 17)

The method of claim 17, wherein the oxygen-free polish stop layer comprises amorphous silicon.