# US 2025/0219610 A1 · Strained piezoelectric devices for radiofrequency resonators and fabrication methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0219610 A1
- Document ID: US20250219610A1
- Status: Published application
- Kind: A1
- Application number: 18/400,615
- Filed: 2023-12-29
- Published: 2025-07-03
- Earliest claimed: 2023-12-29
- Assignees: Robert Bosch GmbH
- Applicants: Robert Bosch GmbH
- Inventors: Mordechai Kornbluth; Sanjay Gopalan; Christoph Schelling; Simon Schneider
- Web page: https://patentgrep.com/patent/US20250219610A1

## CPC

- H03H 9/02133: {of stress}
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02015: {Characteristics of piezoelectric layers, e.g. cutting angles}
- H03H 9/02031: {consisting of ceramic}
- H03H 9/171: {implemented with thin-film techniques, i.e. of the film bulk acoustic resonator [FBAR] type}
- H03H 9/173: {Air-gaps}
- H03H 9/176: {consisting of ceramic material (H03H9/177, H03H9/178 take precedence)}
- H03H 9/562: {comprising a ceramic piezoelectric layer}
- H03H 9/564: {implemented with thin-film techniques}
- H10N 30/076: by vapour phase deposition
- H10N 30/079: using intermediate layers, e.g. for growth control
- H10N 30/708: {Intermediate layers, e.g. barrier, adhesion or growth control buffer layers}
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Disclosed are methods of fabrication and related piezoelectric devices comprising a piezoelectric layer with an induced compressive strain along a z-axis. The methods include formation of a stress layer on a bottom side of a wafer substrate, after deposition of the piezoelectric layer. Stress layer removal results in an induced compressive strain along the z-axis which increases the electromechanical coupling coefficient, and thereby piezoelectric performance. Related devices are also disclosed, including bulk acoustic wave (BAW) thin film resonators (FBAR), which are fabricated in accordance with the disclosed methods.

## Claims

### Claim 1

A method of inducing compressive strain in a piezoelectric device, comprising:
providing a substrate material;
depositing at least one seed layer on a top surface of the substrate material;
depositing a stress layer on a bottom surface of the substrate material;
depositing a piezoelectric layer on the at least one seed layer;
removing the stress layer;
wherein the deposition and removal of the stress layer induces compressive strain along a z-axis of the piezoelectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the induced compressive strain along the z-axis on the piezoelectric layer is about 0.25-3.0%.

### Claim 3 (depends on 1)

The method of claim 1, wherein the stress layer comprises SiOx wherein 1<x<3, SiNy wherein 0.5<y<2, or Si1-zGez wherein 0<z<1.

### Claim 4 (depends on 1)

The method of claim 1, wherein depositing a stress layer causes bowing of the substrate material and/or the at least one seed layer of about 10-200 microns.

### Claim 5 (depends on 1)

The method of claim 1, wherein the piezoelectric layer comprises Al1-xMxN, where M=at least one of Sc, Y, Yb, Cr, B, wherein 0<x<0.7, or Zn1-xMxO, wherein M is Mg and wherein 0.1<x<0.4.

### Claim 6 (depends on 1)

The method of claim 1, wherein the piezoelectric layer comprises Al1-xScxN, wherein 0<x<0.5.

### Claim 7 (depends on 1)

The method of claim 1, further comprising depositing a capping layer comprising Al1-x(In,Ga)xN wherein 0<x<1 on the piezoelectric layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the capping layer has a greater lattice constant than the piezoelectric layer.

### Claim 9 (depends on 1)

The method of claim 1, further comprising annealing the piezoelectric layer at a temperature greater than about 900° C.

### Claim 10 (depends on 9)

The method of claim 9, wherein during the annealing step, an electric field is applied.

### Claim 11 (depends on 1)

The method of claim 1, further comprising removing the substrate material and/or the at least one seed layer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the piezoelectric device is a membrane film bulk acoustic resonator (FBAR), an air gap FBAR, or a solidly mounted resonator (SMR).

### Claim 13

A film bulk acoustic resonator (FBAR) device, comprising:
a substrate material;
a piezoelectric layer having an induced compressive strain along a z-axis;
a first electrode on a top surface of the piezoelectric layer; and
a second electrode on a bottom surface of the piezoelectric layer,
wherein the induced compressive strain along the z-axis of the piezoelectric layer is provided by a stress layer during the device's deposition process.

### Claim 14 (depends on 12)

The device of claim 12, wherein at least some portion of the piezoelectric layer is not attached to the substrate material.

### Claim 15 (depends on 14)

The device of claim 14, wherein the induced compressive strain along the z-axis in the piezoelectric layer remains after portions of the substrate material are removed.

### Claim 16 (depends on 1)

The method of claim 1, wherein the piezoelectric layer comprises Al1-xMxN, where M=at least one of Sc, Y, Yb, Cr, B, wherein 0<x<0.7, or Zn1-xMxO, wherein M is Mg and wherein 0.1<x<0.4.

### Claim 17 (depends on 16)

The device of claim 16, wherein the piezoelectric layer comprises Al1-xScxN, wherein 0<x<0.5.

### Claim 18 (depends on 12)

The device of claim 12, wherein the piezoelectric layer has an electromechanical coupling constant, kt2, wherein kt2 is about 0.05-0.6.

### Claim 19 (depends on 12)

The device of claim 12, wherein the device is a membrane film bulk acoustic resonator (FBAR), or an air gap FBAR.

### Claim 20

An electrical filter comprising;
a film bulk acoustic resonator (FBAR) device, which comprises:
a substrate material;
a piezoelectric layer having an induced compressive strain along a z-axis of about 0.25-3.0% and an electromechanical coupling constant, kt2 of about 0.05-0.6;
a first electrode on a top surface of the piezoelectric layer; and
a second electrode on a bottom surface of the piezoelectric layer,
wherein the induced compressive strain along the z-axis of the piezoelectric layer is provided by a stress layer during the device's deposition process.