# US 2025/0219104 A1 · Steel foil for current collector, and all-solid-state secondary cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0219104 A1
- Document ID: US20250219104A1
- Status: Published application
- Kind: A1
- Application number: 18/852,330
- Filed: 2023-01-19
- Published: 2025-07-03
- Earliest claimed: 2022-03-31
- Assignees: Nippon Steel Chemical & Material Co., Ltd.
- Applicants: NIPPON STEEL Chemical & Material Co., Ltd.
- Inventors: Atsushi YASHIRO; Noriaki ISHIKAWA; Hiroto UNNO; Yoshiaki HAGIWARA; Jun NAKATSUKA
- Web page: https://patentgrep.com/patent/US20250219104A1

## CPC

- H01M 4/66: Selection of materials
- H01M 4/669: {Steels}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- H01M 4/75: Wires, rods or strips
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- C21D 9/46: for sheet metals
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The steel foil for a current collector according to the present disclosure includes a ferritic stainless steel foil. In an X-ray diffraction profile with CoKα rays of the ferritic stainless steel foil according to the present disclosure, the half width Fw of the peak for the {110} plane is 0.40 to 0.52°.

## Claims

### Claim 1

A steel foil for a current collector, comprising:
a ferritic stainless steel foil,
wherein:
in an X-ray diffraction profile with CoKα rays, a half width Fw of a peak for a {110} plane of the ferritic stainless steel foil is 0.40 to 0.52°.

### Claim 2 (depends on 1)

The steel foil for a current collector according to claim 1, wherein:
in a surface of the ferritic stainless steel foil,
when an arithmetic average roughness in an arbitrary direction is defined as Ra1 and
an arithmetic average roughness in a direction orthogonal to the arbitrary direction is defined as Ra2,
both the Ra1 and the Ra2 are 0.03 to 0.30 μm.

### Claim 3 (depends on 1)

The steel foil for a current collector according to claim 1, wherein:
a thickness of the ferritic stainless steel foil is 5 to 60 μm.

### Claim 4 (depends on 2)

The steel foil for a current collector according to claim 2, wherein:
a thickness of the ferritic stainless steel foil is 5 to 60 μm.

### Claim 5 (depends on 1)

The steel foil for a current collector according to claim 1, wherein:
a resin coating is formed on a surface of the ferritic stainless steel foil.

### Claim 6 (depends on 2)

The steel foil for a current collector according to claim 2, wherein:
a resin coating is formed on a surface of the ferritic stainless steel foil.

### Claim 7 (depends on 3)

The steel foil for a current collector according to claim 3, wherein:
a resin coating is formed on a surface of the ferritic stainless steel foil.

### Claim 8 (depends on 4)

The steel foil for a current collector according to claim 4, wherein:
a resin coating is formed on a surface of the ferritic stainless steel foil.

### Claim 9 (depends on 1)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 1;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 10 (depends on 2)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 2;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 11 (depends on 3)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 3;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 12 (depends on 4)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 4;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 13 (depends on 5)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 5;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 14 (depends on 6)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 6;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 15 (depends on 7)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 7;
an active material layer;
a solid electrolyte layer; and
a current collector layer.

### Claim 16 (depends on 8)

An all-solid-state secondary cell, comprising:
a steel foil for a current collector according to claim 8;
an active material layer;
a solid electrolyte layer; and
a current collector layer.