# US 2025/0219092 A1 · Positive electrode active material for lithium-ion secondary battery, and production method of positive electrode active material for lithium-ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0219092 A1
- Document ID: US20250219092A1
- Status: Published application
- Kind: A1
- Application number: 18/850,260
- Filed: 2023-03-30
- Published: 2025-07-03
- Earliest claimed: 2022-04-01
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd.
- Inventors: Haruki KANEDA; Yuki KOSHIKA; Takuma NAKAMURA; Yoshitaka SUESHIGE; Yuki KOYAMA; Takuya KAWAZOE
- Web page: https://patentgrep.com/patent/US20250219092A1

## CPC

- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/364: {as mixtures}
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material for a lithium-ion secondary battery includes lithium metal complex oxide particles, and one or more additive particles selected from among aluminum oxide particles, titanium oxide particles, magnesium oxide particles, silicon oxide particles, and zirconium oxide particles. A specific surface area of the positive electrode active material is 0.25 m2/g or more and 4.0 m2/g or less.

## Claims

### Claim 1

A positive electrode active material for a lithium-ion secondary battery, the positive electrode active material comprising:
lithium metal complex oxide particles; and
one or more additive particles selected from among aluminum oxide particles, titanium oxide particles, magnesium oxide particles, silicon oxide particles, and zirconium oxide particles, wherein
a specific surface area of the positive electrode active material is 0.25 m2/g or more and 4.0 m2/g or less.

### Claim 2 (depends on 1)

The positive electrode active material for the lithium-ion secondary battery according to claim 1, wherein
an average particle diameter of the additive particles is 300 nm or less.

### Claim 3 (depends on 1)

The positive electrode active material for the lithium-ion secondary battery according to claim 1, wherein
a percentage of the additive particles relative to the lithium metal complex oxide particles is 0.025% by mass or more and 3.0% by mass or less.

### Claim 4

A production method of a positive electrode active material for a lithium-ion secondary battery, the production method comprises:
mixing lithium metal complex oxide particles, and one or more additive particles selected from among aluminum oxide particles, titanium oxide particles, magnesium oxide particles, silicon oxide particles, and zirconium oxide particles, wherein
in the mixing, the mixing is performed such that a specific surface area of a positive electrode active material obtained after the mixing is 0.25 m2/g or more and 4.0 m2/g or less.

### Claim 5 (depends on 2)

The positive electrode active material for the lithium-ion secondary battery according to claim 2, wherein
a percentage of the additive particles relative to the lithium metal complex oxide particles is 0.025% by mass or more and 3.0% by mass or less.