# US 2025/0219065 A1 · Electrode active material, electrode mixture, electrode layer, battery, and method for producing these

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0219065 A1
- Document ID: US20250219065A1
- Status: Published application
- Kind: A1
- Application number: 18/980,155
- Filed: 2024-12-13
- Published: 2025-07-03
- Earliest claimed: 2023-12-28
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Mitsutoshi OTAKI; Masafumi Nose
- Web page: https://patentgrep.com/patent/US20250219065A1

## CPC

- H01M 4/386: {Silicon or alloys based on silicon}
- C01B 33/021: Preparation (chemical coating from the vapour phase C23C16/00)
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/77: by unit-cell parameters, atom positions or structure diagrams
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A main object of the present disclosure is to provide an electrode active material of which volume change due to charge and discharge is small. The present disclosure achieves the object by providing an electrode active material including a silicon clathrate II type crystal phase, wherein a void is included inside a primary particle; and a void amount P1 of a void with a pore diameter of 5 nm or less is 0.015 cc/g or more and 0.05 cc/g or less.

## Claims

### Claim 1

An electrode active material comprising a silicon
clathrate II type crystal phase, wherein
a void is included inside a primary particle; and
a void amount P1 of a void with a pore diameter of 5 nm or less is 0.015 cc/g or more and 0.05 cc/g or less.

### Claim 2 (depends on 1)

The electrode active material according to claim 1, wherein a rate of the void amount P1 with respect to a void amount P2 of a void with a pore diameter of 10 nm or less, which is P1/P2, is 50% or more.

### Claim 3 (depends on 1)

The electrode active material according to claim 1, wherein a void amount P2 of a void with a pore diameter of 10 nm or less is 0.03 cc/g or more and 0.08 cc/g or less.

### Claim 4 (depends on 1)

The electrode active material according to claim 1, wherein a rate of the void amount P1 with respect to a void amount P3 of a void with a pore diameter of 100 nm or less, which is P1/P3, is 6.5% or more.

### Claim 5 (depends on 1)

The electrode active material according to claim 1, wherein a void amount P3 of a void with a pore diameter of 100 nm or less is 0.1 cc/g or more and 0.5 cc/g or less.

### Claim 6 (depends on 1)

The electrode active material according to claim 1, wherein the electrode active material includes the silicon clathrate II type crystal phase as a main phase.

### Claim 7 (depends on 1)

An electrode mixture comprising the electrode active material according to claim 1, and at least one of a conductive material and a binder.

### Claim 8 (depends on 7)

The electrode mixture according to claim 7, further comprising a solid electrolyte.

### Claim 9 (depends on 8)

The electrode mixture according to claim 8, wherein the solid electrolyte included in the electrode mixture is a sulfide solid electrolyte.

### Claim 10

An electrode layer to be used in a battery, the electrode layer comprising:
an electrode active material including a silicon clathrate II type crystal phase and a void inside a primary particle, wherein
a void amount Q1 of a void with a pore diameter of 5 nm or less is 0.008 cc/g or more and 0.04 cc/g or less.

### Claim 11 (depends on 10)

The electrode layer according to claim 10, wherein a rate of the void amount Q1 with respect to a void amount Q2 of a void with a pore diameter of 10 nm or less, which is Q1/Q2, is 50% or more.

### Claim 12 (depends on 10)

The electrode layer according to claim 10, wherein a void amount Q2 of a void with a pore diameter of 10 nm or less is 0.01 cc/g or more and 0.05 cc/g or less.

### Claim 13 (depends on 10)

The electrode layer according to claim 10, wherein a rate of the void amount Q1 with respect to a void amount Q3 of a void with a pore diameter of 100 nm or less, which is Q1/Q3, is 10% or more.

### Claim 14 (depends on 10)

The electrode layer according to claim 10, wherein a void amount Q3 of a void with a pore diameter of 100 nm or less is 0.07 cc/g or more and 0.2 cc/g or less.

### Claim 15 (depends on 10)

A battery comprising a cathode layer, an anode layer, and an electrolyte layer arranged between the cathode layer and the anode layer, wherein
the cathode layer or the anode layer is the electrode layer according to claim 10.

### Claim 16

A method for producing an electrode active material, the method comprising:
an alloying step of obtaining a Na—Si alloy by bringing a Na source and a Si source into reaction;
a burning step of burning the Na—Si alloy to decrease Na amount in the Na—Si alloy and form a precursor active material including a silicon clathrate II type crystal phase; and
a liquid treatment step of performing a liquid treatment to the precursor active material using a hydrofluoric acid, wherein
a concentration of hydrogen fluoride in the hydrofluoric acid is 3 weight % or more; and
a treatment time in the liquid treatment step is 3 hours or more and less than 24 hours.

### Claim 17 (depends on 16)

The method for producing an electrode active material according to claim 16, wherein, in the electrode active material, a void amount P1 of a void with a pore diameter of 5 nm or less is 0.015 cc/g or more and 0.05 cc/g or less.

### Claim 18 (depends on 16)

A method for producing an electrode mixture, the method comprising:
a preparing step of preparing an electrode active material by the method for producing an electrode active material according to claim 16; and
a mixing step of mixing the electrode active material and at least one of a conductive material and a binder to obtain an electrode mixture.

### Claim 19 (depends on 16)

A method for producing an electrode layer, the method comprising:
a preparing step of preparing an electrode active material by the method for producing an electrode active material according to claim 16;
a mixing step of mixing the electrode active material and at least one of a conductive material and a binder to obtain an electrode mixture; and
an electrode layer forming step of forming an electrode layer using the electrode mixture.

### Claim 20 (depends on 16)

A method for producing a battery, the method comprising:
a preparing step of preparing an electrode active material by the method for producing an electrode active material according to claim 16;
a mixing step of mixing the electrode active material and at least one of a conductive material and a binder to obtain an electrode mixture; and
an electrode layer forming step of forming an electrode layer using the electrode mixture.