# US 2025/0218992 A1 · Core-shell ball grid array materials for large form factor integrated circuit packages

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0218992 A1
- Document ID: US20250218992A1
- Status: Published application
- Kind: A1
- Application number: 18/399,395
- Filed: 2023-12-28
- Published: 2025-07-03
- Earliest claimed: 2023-12-28
- Assignees: Intel Corporation
- Applicants: Intel Corporation
- Inventors: Rui Zhang; Jiaqi Wu; Brian Franco; Xiao Lu; Mukul Renavikar
- Web page: https://patentgrep.com/patent/US20250218992A1

## CPC

- H10W 72/072: {of bump connectors}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/255: {of outermost layers of multilayered bumps, e.g. material of a coating}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Solder materials, solder balls, and solder features, and microelectronic devices and systems deploying the solders are discussed. A solder ball includes an inner core that is an alloy of tin, silver, and copper, which has a relatively high melting point. Surrounding the inner core is a shell or cladding of a tin-bismuth alloy having a lower melting point. An optional nickel coating is on the inner core and between the inner core and the shell or cladding. During surface mount, the lower melting point the tin-bismuth alloy is used as the reflow temperature.

## Claims

### Claim 1

A solder ball, comprising:
an inner core comprising an alloy of tin, silver, and copper; and
a shell surrounding the inner core, the shell comprising an alloy of tin and bismuth.

### Claim 2 (depends on 1)

The solder ball of claim 1, wherein at least a portion of the shell comprises substantially pure tin-bismuth with not less than 30 wt. % and not more than 57% wt. % bismuth, and a balance of tin.

### Claim 3 (depends on 2)

The solder ball of claim 2, wherein the portion of the shell comprises not more than 1 wt. % silver or antimony.

### Claim 4 (depends on 2)

The solder ball of claim 2, wherein the portion of the shell comprises pure tin-bismuth.

### Claim 5 (depends on 1)

The solder ball of claim 1, wherein the shell is directly on the inner core, the inner core comprising bismuth.

### Claim 6 (depends on 1)

The solder ball of claim 1, further comprising a coating on the inner core and between the inner core and the shell, the coating comprising nickel.

### Claim 7 (depends on 6)

The solder ball of claim 6, wherein the coating has a thickness of not less than 1 micron and not more than 5 microns.

### Claim 8 (depends on 6)

The solder ball of claim 6, wherein the inner core is absent bismuth.

### Claim 9 (depends on 1)

The solder ball of claim 1, wherein the shell has a thickness of not less 0.8 microns and not more than 150 microns.

### Claim 10

An apparatus, comprising:
a first metallization structure of a host component;
a second metallization structure of an integrated circuit (IC) device; and
an interconnect structure coupling the first metallization structure and the second metallization structure, the interconnect structure comprising:
an inner metal core comprising tin, silver, and copper; and
a metal cladding surrounding the inner metal core, the metal cladding comprising tin and bismuth.

### Claim 11 (depends on 10)

The apparatus of claim 10, wherein the metal cladding comprises substantially pure tin-bismuth.

### Claim 12 (depends on 11)

The apparatus of claim 11, wherein the metal cladding comprises not less than 30 wt. % and not more than 57% wt. % bismuth.

### Claim 13 (depends on 10)

The apparatus of claim 10, wherein the metal cladding further comprises silver or antimony.

### Claim 14 (depends on 10)

The apparatus of claim 10, further comprising a coating having a thickness of not less than 1 micron and not more than 5 microns on the inner metal core and between the inner metal core and the metal cladding, the coating comprising nickel.

### Claim 15 (depends on 10)

The apparatus of claim 10, wherein the inner metal core has a cross-sectional dimension of not less than 200 microns and not more than 700 microns and the metal cladding has a thickness of not less than 0.8 microns and not more than 150 microns.

### Claim 16

An apparatus, comprising:
a microelectronics board;
an integrated circuit (IC) package comprising one or more IC devices; and
an interconnect structure electrically coupling the microelectronics board to the IC package, the interconnect structure comprising:
an inner core having a first melting point; and
a cladding surrounding the inner core, the cladding having a second melting point, wherein the first melting point is not less than 40° C. greater than the second melting point.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the inner core comprises an alloy of tin, silver, and copper, and the cladding comprises an alloy of tin and bismuth.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein at least a portion of the inner core comprises about 96.5 wt. % tin, about 3 wt. % silver, and about 0.5 wt. % copper, and at least a portion of the cladding comprises substantially pure tin-bismuth with not less than 30 wt. % and not more than 57% wt. % bismuth, and a balance of tin.

### Claim 19 (depends on 18)

The apparatus of claim 18, wherein the portion of the cladding comprises not more than 1 wt. % silver or antimony.

### Claim 20 (depends on 16)

The apparatus of claim 16, further comprising a coating on the inner core and between the inner core and the cladding, the coating comprising substantially pure nickel and having a thickness of not more than 5 microns.